烧结 Ni25Al25Co15Fe15Mn8Ti7Cr5 高熵合金的相形成和力学分析

IF 1.9 Q3 ENGINEERING, MANUFACTURING Manufacturing Letters Pub Date : 2024-10-01 DOI:10.1016/j.mfglet.2024.09.019
Emmanuel Olorundaisi , Bukola J. Babalola , Ufoma S. Anamu , Moipone L. Teffo , Ngeleshi Michel Kibambe , Anthony O. Ogunmefun , Peter Odetola , Peter A. Olubambi
{"title":"烧结 Ni25Al25Co15Fe15Mn8Ti7Cr5 高熵合金的相形成和力学分析","authors":"Emmanuel Olorundaisi ,&nbsp;Bukola J. Babalola ,&nbsp;Ufoma S. Anamu ,&nbsp;Moipone L. Teffo ,&nbsp;Ngeleshi Michel Kibambe ,&nbsp;Anthony O. Ogunmefun ,&nbsp;Peter Odetola ,&nbsp;Peter A. Olubambi","doi":"10.1016/j.mfglet.2024.09.019","DOIUrl":null,"url":null,"abstract":"<div><div>In recent years, the pursuit of cutting-edge materials has intensified, with a focus on affordability, lightweight characteristics, and exceptional performance under high-temperature conditions, to serve as alternatives to Ni-base superalloys and other conventional alloys. Potential materials suitable for high-temperature structural applications with lightweight characteristics are intermetallics such as NiAl, and TiAl, but pose numerous fabrication challenges and poor ductility behaviour at room temperature. In view of this, a novel Ni<sub>25</sub>Al<sub>25</sub>Co<sub>15</sub>Fe<sub>15</sub> Mn<sub>8</sub>Ti<sub>7</sub>Cr<sub>5</sub> high entropy alloy (HEA) was fabricated using spark plasma sintering (SPS). The alloy was developed at a sintering temperature of 850 °C, a heating rate of 90 °C/min, a pressure of 50 MPa, and a dwelling time of 5 min. X-ray diffraction, scanning electron microscopy, and Vickers hardness tester were used to investigate the phase formation, microstructure, and mechanical properties of the HEA, respectively. The microstructure of the sintered HEA shows a homogenous dispersion of the alloying metals. The sintered microstructures showed a mixture of simple and complex phases. The grain size analysis shows that the sintered HEA exhibited a lower grain size of 2.28 µm and a refined crystallite size of 3.159 µm. The microhardness value and relative density of the sintered HEA are 135.8 HV and 99.56 %, respectively.</div></div>","PeriodicalId":38186,"journal":{"name":"Manufacturing Letters","volume":"41 ","pages":"Pages 153-159"},"PeriodicalIF":1.9000,"publicationDate":"2024-10-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Phase formation and mechanical analysis of sintered Ni25Al25Co15Fe15Mn8Ti7Cr5 high entropy alloy\",\"authors\":\"Emmanuel Olorundaisi ,&nbsp;Bukola J. Babalola ,&nbsp;Ufoma S. Anamu ,&nbsp;Moipone L. Teffo ,&nbsp;Ngeleshi Michel Kibambe ,&nbsp;Anthony O. Ogunmefun ,&nbsp;Peter Odetola ,&nbsp;Peter A. Olubambi\",\"doi\":\"10.1016/j.mfglet.2024.09.019\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<div><div>In recent years, the pursuit of cutting-edge materials has intensified, with a focus on affordability, lightweight characteristics, and exceptional performance under high-temperature conditions, to serve as alternatives to Ni-base superalloys and other conventional alloys. Potential materials suitable for high-temperature structural applications with lightweight characteristics are intermetallics such as NiAl, and TiAl, but pose numerous fabrication challenges and poor ductility behaviour at room temperature. In view of this, a novel Ni<sub>25</sub>Al<sub>25</sub>Co<sub>15</sub>Fe<sub>15</sub> Mn<sub>8</sub>Ti<sub>7</sub>Cr<sub>5</sub> high entropy alloy (HEA) was fabricated using spark plasma sintering (SPS). The alloy was developed at a sintering temperature of 850 °C, a heating rate of 90 °C/min, a pressure of 50 MPa, and a dwelling time of 5 min. X-ray diffraction, scanning electron microscopy, and Vickers hardness tester were used to investigate the phase formation, microstructure, and mechanical properties of the HEA, respectively. The microstructure of the sintered HEA shows a homogenous dispersion of the alloying metals. The sintered microstructures showed a mixture of simple and complex phases. The grain size analysis shows that the sintered HEA exhibited a lower grain size of 2.28 µm and a refined crystallite size of 3.159 µm. The microhardness value and relative density of the sintered HEA are 135.8 HV and 99.56 %, respectively.</div></div>\",\"PeriodicalId\":38186,\"journal\":{\"name\":\"Manufacturing Letters\",\"volume\":\"41 \",\"pages\":\"Pages 153-159\"},\"PeriodicalIF\":1.9000,\"publicationDate\":\"2024-10-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Manufacturing Letters\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://www.sciencedirect.com/science/article/pii/S2213846324000762\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q3\",\"JCRName\":\"ENGINEERING, MANUFACTURING\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Manufacturing Letters","FirstCategoryId":"1085","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S2213846324000762","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"ENGINEERING, MANUFACTURING","Score":null,"Total":0}
引用次数: 0

摘要

近年来,人们对尖端材料的追求不断加强,重点关注材料的经济性、轻质特性以及在高温条件下的优异性能,以替代镍基超级合金和其他传统合金。适合高温结构应用且具有轻质特性的潜在材料是镍铝和钛铝等金属间化合物,但它们在制造方面存在诸多挑战,而且在室温下延展性能较差。有鉴于此,一种新型 Ni25Al25Co15Fe15 Mn8Ti7Cr5 高熵合金(HEA)采用火花等离子烧结(SPS)技术制成。该合金的烧结温度为 850 °C,加热速度为 90 °C/分钟,压力为 50 兆帕,停留时间为 5 分钟。利用 X 射线衍射、扫描电子显微镜和维氏硬度计分别研究了 HEA 的相形成、微观结构和机械性能。烧结 HEA 的微观结构显示出合金金属的均匀分散。烧结微结构显示出简单相和复杂相的混合。晶粒度分析表明,烧结 HEA 的晶粒度较低,为 2.28 µm,晶粒度较细,为 3.159 µm。烧结 HEA 的显微硬度值和相对密度分别为 135.8 HV 和 99.56 %。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Phase formation and mechanical analysis of sintered Ni25Al25Co15Fe15Mn8Ti7Cr5 high entropy alloy
In recent years, the pursuit of cutting-edge materials has intensified, with a focus on affordability, lightweight characteristics, and exceptional performance under high-temperature conditions, to serve as alternatives to Ni-base superalloys and other conventional alloys. Potential materials suitable for high-temperature structural applications with lightweight characteristics are intermetallics such as NiAl, and TiAl, but pose numerous fabrication challenges and poor ductility behaviour at room temperature. In view of this, a novel Ni25Al25Co15Fe15 Mn8Ti7Cr5 high entropy alloy (HEA) was fabricated using spark plasma sintering (SPS). The alloy was developed at a sintering temperature of 850 °C, a heating rate of 90 °C/min, a pressure of 50 MPa, and a dwelling time of 5 min. X-ray diffraction, scanning electron microscopy, and Vickers hardness tester were used to investigate the phase formation, microstructure, and mechanical properties of the HEA, respectively. The microstructure of the sintered HEA shows a homogenous dispersion of the alloying metals. The sintered microstructures showed a mixture of simple and complex phases. The grain size analysis shows that the sintered HEA exhibited a lower grain size of 2.28 µm and a refined crystallite size of 3.159 µm. The microhardness value and relative density of the sintered HEA are 135.8 HV and 99.56 %, respectively.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Manufacturing Letters
Manufacturing Letters Engineering-Industrial and Manufacturing Engineering
CiteScore
4.20
自引率
5.10%
发文量
192
审稿时长
60 days
期刊最新文献
Applicability of circularity protocols to extend the lifetime of a thermoplastic pultrusion line: A case study Feasibility study of using friction stir extruded recycled aluminum rods for welding and additive manufacturing Scalable and efficient fabrication of surface microstructures using a small wheeled robot with a vibration-cutting tool Influence of parameter variation and interlayer temperature control in wall angle, curvature and measurement methodology of ER70S-6 parts obtained by WAAM Hard and wear resistant AISI304 stainless steel clad layer deposited on mild steel substrate by TIG cladding
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1