{"title":"半球形壳谐振器水浴加热辅助小球端磁流变抛光新方法","authors":"Jinchuan TIAN ,&nbsp;Mingjun CHEN ,&nbsp;Jian CHENG ,&nbsp;Henan LIU","doi":"10.1016/j.cja.2023.05.003","DOIUrl":null,"url":null,"abstract":"<div><p>Hemispherical shell resonator (HSR) is the core component of hemispherical resonator gyro. It is a ψ-shaped small-bore complex component with minimum curvature radius less than 3 mm. Thus, traditional polishing methods are difficult to polish it. Small ball-end magnetorheological polishing method can polish the small components with complicated three-dimensional surface and obtain non-destructive surface. Therefore, this method is suitable for polishing HSR. However, the material removal rate of the ordinary small ball-end magnetorheological polishing is low, leading to long polishing time and low output of HSR. To solve this problem, a water bath heating assisted small ball-end magnetorheological polishing method is proposed in this research. The influence rule of processing parameters on the material removal rate is studied experimentally. A set of optimal processing parameters is obtained to maximize the material removal rate. Compared with the ordinary method, the material removal rate of the new method can be improved by 143%. Subsequently, an HSR is polished by the new method. The results show that the polishing time can be reduced by 55%, and the polished surface roughness can reach 7.7 nm. The new method has the great potential to be used in actual production to improve the polishing efficiency of HSR.</p></div>","PeriodicalId":55631,"journal":{"name":"Chinese Journal of Aeronautics","volume":"36 12","pages":"Pages 451-460"},"PeriodicalIF":5.3000,"publicationDate":"2023-12-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://www.sciencedirect.com/science/article/pii/S1000936123001553/pdfft?md5=d1fedbba2e95f90b353a4af06d6a000f&pid=1-s2.0-S1000936123001553-main.pdf","citationCount":"1","resultStr":"{\"title\":\"A novel method of water bath heating assisted small ball-end magnetorheological polishing for hemispherical shell resonators\",\"authors\":\"Jinchuan TIAN ,&nbsp;Mingjun CHEN ,&nbsp;Jian CHENG ,&nbsp;Henan LIU\",\"doi\":\"10.1016/j.cja.2023.05.003\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<div><p>Hemispherical shell resonator (HSR) is the core component of hemispherical resonator gyro. It is a ψ-shaped small-bore complex component with minimum curvature radius less than 3 mm. Thus, traditional polishing methods are difficult to polish it. Small ball-end magnetorheological polishing method can polish the small components with complicated three-dimensional surface and obtain non-destructive surface. Therefore, this method is suitable for polishing HSR. However, the material removal rate of the ordinary small ball-end magnetorheological polishing is low, leading to long polishing time and low output of HSR. To solve this problem, a water bath heating assisted small ball-end magnetorheological polishing method is proposed in this research. The influence rule of processing parameters on the material removal rate is studied experimentally. A set of optimal processing parameters is obtained to maximize the material removal rate. Compared with the ordinary method, the material removal rate of the new method can be improved by 143%. Subsequently, an HSR is polished by the new method. The results show that the polishing time can be reduced by 55%, and the polished surface roughness can reach 7.7 nm. The new method has the great potential to be used in actual production to improve the polishing efficiency of HSR.</p></div>\",\"PeriodicalId\":55631,\"journal\":{\"name\":\"Chinese Journal of Aeronautics\",\"volume\":\"36 12\",\"pages\":\"Pages 451-460\"},\"PeriodicalIF\":5.3000,\"publicationDate\":\"2023-12-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"https://www.sciencedirect.com/science/article/pii/S1000936123001553/pdfft?md5=d1fedbba2e95f90b353a4af06d6a000f&pid=1-s2.0-S1000936123001553-main.pdf\",\"citationCount\":\"1\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Chinese Journal of Aeronautics\",\"FirstCategoryId\":\"1087\",\"ListUrlMain\":\"https://www.sciencedirect.com/science/article/pii/S1000936123001553\",\"RegionNum\":1,\"RegionCategory\":\"工程技术\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q1\",\"JCRName\":\"ENGINEERING, AEROSPACE\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Chinese Journal of Aeronautics","FirstCategoryId":"1087","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S1000936123001553","RegionNum":1,"RegionCategory":"工程技术","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"ENGINEERING, AEROSPACE","Score":null,"Total":0}
引用次数: 1

摘要

半球壳谐振器(HSR)是半球谐振器陀螺仪的核心部件。它是ψ形小孔径复杂元件,最小曲率半径小于 3 毫米。因此,传统的抛光方法很难对其进行抛光。小球端磁流变抛光法可以抛光具有复杂三维表面的小型部件,并获得无损表面。因此,这种方法适用于抛光 HSR。但是,普通小球端磁流变抛光的材料去除率较低,导致抛光时间长,HSR 产量低。为解决这一问题,本研究提出了一种水浴加热辅助小球端磁流变抛光方法。实验研究了加工参数对材料去除率的影响规律。得到了一组最佳加工参数,使材料去除率最大化。与普通方法相比,新方法的材料去除率提高了 143%。随后,用新方法对 HSR 进行了抛光。结果表明,抛光时间可缩短 55%,抛光表面粗糙度可达 7.7 nm。新方法在实际生产中提高 HSR 抛光效率的潜力巨大。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
A novel method of water bath heating assisted small ball-end magnetorheological polishing for hemispherical shell resonators

Hemispherical shell resonator (HSR) is the core component of hemispherical resonator gyro. It is a ψ-shaped small-bore complex component with minimum curvature radius less than 3 mm. Thus, traditional polishing methods are difficult to polish it. Small ball-end magnetorheological polishing method can polish the small components with complicated three-dimensional surface and obtain non-destructive surface. Therefore, this method is suitable for polishing HSR. However, the material removal rate of the ordinary small ball-end magnetorheological polishing is low, leading to long polishing time and low output of HSR. To solve this problem, a water bath heating assisted small ball-end magnetorheological polishing method is proposed in this research. The influence rule of processing parameters on the material removal rate is studied experimentally. A set of optimal processing parameters is obtained to maximize the material removal rate. Compared with the ordinary method, the material removal rate of the new method can be improved by 143%. Subsequently, an HSR is polished by the new method. The results show that the polishing time can be reduced by 55%, and the polished surface roughness can reach 7.7 nm. The new method has the great potential to be used in actual production to improve the polishing efficiency of HSR.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Chinese Journal of Aeronautics
Chinese Journal of Aeronautics 工程技术-工程:宇航
CiteScore
10.00
自引率
17.50%
发文量
3080
审稿时长
55 days
期刊介绍: Chinese Journal of Aeronautics (CJA) is an open access, peer-reviewed international journal covering all aspects of aerospace engineering. The Journal reports the scientific and technological achievements and frontiers in aeronautic engineering and astronautic engineering, in both theory and practice, such as theoretical research articles, experiment ones, research notes, comprehensive reviews, technological briefs and other reports on the latest developments and everything related to the fields of aeronautics and astronautics, as well as those ground equipment concerned.
期刊最新文献
Editorial Board - Inside Front Cover Table of Content Inhibiting plastic tensile instability of non-symmetric thin-walled shell component via increasing regional metal inflow based on heterogeneous pressure-carrying medium Technologies and studies of gas exchange in two-stroke aircraft piston engine: A review Mechanism of capture section affecting an intake for atmosphere-breathing electric propulsion
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1