经处理和未经处理的菠萝叶纤维增强水泥稳定土砖的抗压和抗弯强度

Nounagnon A. Vodounon, C. Kanali, J. Mwero
{"title":"经处理和未经处理的菠萝叶纤维增强水泥稳定土砖的抗压和抗弯强度","authors":"Nounagnon A. Vodounon, C. Kanali, J. Mwero","doi":"10.4236/OJCM.2018.84012","DOIUrl":null,"url":null,"abstract":"This study compares the effect of treated pineapple leaves fibres (T-PALF) with sodium hydroxide solution and untreated fibres (N-PALF) on the compressive and flexural strength of earth bricks stabilized with 3% and 5% cement. The fibre content ranged from 0% to 5% in steps of 1% by weight. The compressive strength tests were made at 7, 14, 21 and 28 days of curing; the flexural strength test were conducted at 28th day only. The results show that the T-PALF had a higher compressive strength when comparing to the N-PALF. The highest compressive strength of the bricks was obtained at 28 days of curing. The compressive strength at 28 days of stabilized brick at 3% and 5% of cement reinforced with T-PALF were 4.01 and 4.81 MPa, respectively, while the one reinforced with N-PALF was 3.19 and 4.63 MPa, respectively. The results further show that the highest flexural strength of both stabilized bricks at 3% and 5% of cement reinforced with T-PALF and N-PALF was obtained with the bricks stabilized with 5% of cement reinforced with T-PALF. This results show that bricks stabilized with 5% cement and reinforced with 3% of treated fibres content are good for construction of load bearing walls. It was observed; a significant improvement of the reinforced blocks under flexure than under compression.","PeriodicalId":57868,"journal":{"name":"复合材料期刊(英文)","volume":"08 1","pages":"145-160"},"PeriodicalIF":0.0000,"publicationDate":"2018-10-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"14","resultStr":"{\"title\":\"Compressive and Flexural Strengths of Cement Stabilized Earth Bricks Reinforced with Treated and Untreated Pineapple Leaves Fibres\",\"authors\":\"Nounagnon A. Vodounon, C. Kanali, J. Mwero\",\"doi\":\"10.4236/OJCM.2018.84012\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"This study compares the effect of treated pineapple leaves fibres (T-PALF) with sodium hydroxide solution and untreated fibres (N-PALF) on the compressive and flexural strength of earth bricks stabilized with 3% and 5% cement. The fibre content ranged from 0% to 5% in steps of 1% by weight. The compressive strength tests were made at 7, 14, 21 and 28 days of curing; the flexural strength test were conducted at 28th day only. The results show that the T-PALF had a higher compressive strength when comparing to the N-PALF. The highest compressive strength of the bricks was obtained at 28 days of curing. The compressive strength at 28 days of stabilized brick at 3% and 5% of cement reinforced with T-PALF were 4.01 and 4.81 MPa, respectively, while the one reinforced with N-PALF was 3.19 and 4.63 MPa, respectively. The results further show that the highest flexural strength of both stabilized bricks at 3% and 5% of cement reinforced with T-PALF and N-PALF was obtained with the bricks stabilized with 5% of cement reinforced with T-PALF. This results show that bricks stabilized with 5% cement and reinforced with 3% of treated fibres content are good for construction of load bearing walls. It was observed; a significant improvement of the reinforced blocks under flexure than under compression.\",\"PeriodicalId\":57868,\"journal\":{\"name\":\"复合材料期刊(英文)\",\"volume\":\"08 1\",\"pages\":\"145-160\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2018-10-30\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"14\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"复合材料期刊(英文)\",\"FirstCategoryId\":\"1087\",\"ListUrlMain\":\"https://doi.org/10.4236/OJCM.2018.84012\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"复合材料期刊(英文)","FirstCategoryId":"1087","ListUrlMain":"https://doi.org/10.4236/OJCM.2018.84012","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 14

摘要

本研究比较了经氢氧化钠溶液处理的菠萝叶纤维(T-PALF)和未经处理的纤维(N-PALF)对用3%和5%水泥稳定的土砖抗压和抗弯强度的影响。纤维含量在0%至5%的范围内,以1重量%为步长。抗压强度测试在固化的第7、14、21和28天进行;仅在第28天进行弯曲强度试验。结果表明,与N-PALF相比,T-PALF具有更高的抗压强度。砖的最高抗压强度是在固化28天时获得的。T-PALF加固的稳定砖在水泥用量为3%和5%时28天的抗压强度分别为4.01和4.81MPa,而N-PALF加固时的抗压强度则分别为3.19和4.63MPa。结果进一步表明,用T-PALF和N-PALF加固的3%和5%水泥的稳定砖的抗弯强度最高,而用T-PAFF加固的5%水泥稳定砖的弯曲强度最高。结果表明,用5%水泥稳定并用3%处理过的纤维加固的砖有利于承重墙的施工。观察到;弯曲下的增强块比压缩下的显著改善。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Compressive and Flexural Strengths of Cement Stabilized Earth Bricks Reinforced with Treated and Untreated Pineapple Leaves Fibres
This study compares the effect of treated pineapple leaves fibres (T-PALF) with sodium hydroxide solution and untreated fibres (N-PALF) on the compressive and flexural strength of earth bricks stabilized with 3% and 5% cement. The fibre content ranged from 0% to 5% in steps of 1% by weight. The compressive strength tests were made at 7, 14, 21 and 28 days of curing; the flexural strength test were conducted at 28th day only. The results show that the T-PALF had a higher compressive strength when comparing to the N-PALF. The highest compressive strength of the bricks was obtained at 28 days of curing. The compressive strength at 28 days of stabilized brick at 3% and 5% of cement reinforced with T-PALF were 4.01 and 4.81 MPa, respectively, while the one reinforced with N-PALF was 3.19 and 4.63 MPa, respectively. The results further show that the highest flexural strength of both stabilized bricks at 3% and 5% of cement reinforced with T-PALF and N-PALF was obtained with the bricks stabilized with 5% of cement reinforced with T-PALF. This results show that bricks stabilized with 5% cement and reinforced with 3% of treated fibres content are good for construction of load bearing walls. It was observed; a significant improvement of the reinforced blocks under flexure than under compression.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
127
期刊最新文献
A Decisive Study on Dielectric Response of Bi2O3/Polystyrene & Bi2O3/PVDF Composite as Flexible Electrodes for Energy Storage Influence of Plastic and Coconut Shell (Cocos nucifera L.) on the Physico-Mechanical Properties of the 8/6 Composite Rafter The Equilibrium Moisture Content of Five Lesser Utilized Species of Ghana Contrasted with Three European Species Development and Evaluation of the Mechanical Properties of Coconut Fibre Reinforced Low Density Polyethylene Composite Influence of the Age of Bamboo Culm and Its Vertical Position on the Technological Properties of Bamboo Fibers: A Case of Bambusa vulgaris Species from Cameroonian Culture
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1