羊绒用阴阳离子水性聚氨酯和石墨烯纤维素纳米晶抗静电剂的制备及应用

Mingxing Yang, K. Ismoilov, S. Chauhan, Q. Heng, Z. Islamova
{"title":"羊绒用阴阳离子水性聚氨酯和石墨烯纤维素纳米晶抗静电剂的制备及应用","authors":"Mingxing Yang, K. Ismoilov, S. Chauhan, Q. Heng, Z. Islamova","doi":"10.4236/graphene.2019.82002","DOIUrl":null,"url":null,"abstract":"The main purpose of this research work is to improve anti-static properties of Cashmere fabric by introducing application comprising anti-static agent by foaming which was made with cationic waterborne polyurethane and graphene-CNC. Cashmere fabric was cut into 10 pieces of sample cloth of 5 cm * 5 cm size, washed with acetone solution, and then dried in an oven at 60℃. Three forms of waterborne polyurethanes such as two forms of Cationic waterborne polyurethane (CWPU) and a form of Anionic waterborne polyurethane (AWPU) were synthesized. Cellulose nanocrystalline (CNC)/graphite powder solution with the ratio of 0.5/1, 1/1, 2/1 was prepared by ultrasonic probe stripping method, and the concentration of graphite powder was ensured to be 1 mg/ml. The fabric was treated with anionic and cationic WPUs foaming solution until the weight gain reached 2.5 - 3.5 wt%. After drying, the elastic cloth was foamed with graphene solution until the graphite content of the cloth was close to 10%, 20%, 40%, 60% respectively, and then dried for reserving. Characterization properties of pure graphite powder, pure CNC and graphene solution with different proportions of three components were tested by Fourier transform infrared spectrometer (FTIR), X-ray diffraction (XRD), Thermalgravitimetric analysis (TGA) and scanning electron microscopy (SEM). Take the original cloth, only WPU treated cloth and four clothes with different graphite content for the fabric performance test.","PeriodicalId":63892,"journal":{"name":"石墨烯(英文)","volume":" ","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2019-09-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":"{\"title\":\"Preparation and Application of Anionic and Cationic Waterborne Polyurethanes and Graphene-Cellulose Nanocrystal as an Antistatic Agent for Cashmere\",\"authors\":\"Mingxing Yang, K. Ismoilov, S. Chauhan, Q. Heng, Z. Islamova\",\"doi\":\"10.4236/graphene.2019.82002\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The main purpose of this research work is to improve anti-static properties of Cashmere fabric by introducing application comprising anti-static agent by foaming which was made with cationic waterborne polyurethane and graphene-CNC. Cashmere fabric was cut into 10 pieces of sample cloth of 5 cm * 5 cm size, washed with acetone solution, and then dried in an oven at 60℃. Three forms of waterborne polyurethanes such as two forms of Cationic waterborne polyurethane (CWPU) and a form of Anionic waterborne polyurethane (AWPU) were synthesized. Cellulose nanocrystalline (CNC)/graphite powder solution with the ratio of 0.5/1, 1/1, 2/1 was prepared by ultrasonic probe stripping method, and the concentration of graphite powder was ensured to be 1 mg/ml. The fabric was treated with anionic and cationic WPUs foaming solution until the weight gain reached 2.5 - 3.5 wt%. After drying, the elastic cloth was foamed with graphene solution until the graphite content of the cloth was close to 10%, 20%, 40%, 60% respectively, and then dried for reserving. Characterization properties of pure graphite powder, pure CNC and graphene solution with different proportions of three components were tested by Fourier transform infrared spectrometer (FTIR), X-ray diffraction (XRD), Thermalgravitimetric analysis (TGA) and scanning electron microscopy (SEM). Take the original cloth, only WPU treated cloth and four clothes with different graphite content for the fabric performance test.\",\"PeriodicalId\":63892,\"journal\":{\"name\":\"石墨烯(英文)\",\"volume\":\" \",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2019-09-30\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"2\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"石墨烯(英文)\",\"FirstCategoryId\":\"1089\",\"ListUrlMain\":\"https://doi.org/10.4236/graphene.2019.82002\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"石墨烯(英文)","FirstCategoryId":"1089","ListUrlMain":"https://doi.org/10.4236/graphene.2019.82002","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2

摘要

本研究的主要目的是通过引入阳离子水性聚氨酯和石墨烯CNC发泡防静电剂的应用,提高羊绒织物的防静电性能。将羊绒织物切成10块5cm×5cm大小的样品布,用丙酮溶液洗涤,然后在60℃的烘箱中干燥。合成了三种形式的水性聚氨酯,如两种形式的阳离子水性聚氨酯(CWPU)和一种形式的阴离子水性聚氨酯。采用超声波探针剥离法制备了比例为0.5/1、1/1、2/1的纤维素纳米晶(CNC)/石墨粉溶液,并保证石墨粉的浓度为1mg/ml。用阴离子和阳离子WPU发泡溶液处理织物,直到重量增加达到2.5-3.5wt%。干燥后,用石墨烯溶液对弹性布进行发泡,直到布的石墨含量分别接近10%、20%、40%、60%,然后干燥保存。采用傅立叶变换红外光谱(FTIR)、X射线衍射(XRD)、热重分析(TGA)和扫描电子显微镜(SEM)测试了纯石墨粉末、纯CNC和不同比例三组分的石墨烯溶液的表征性能。以原布为例,仅用WPU处理过的布和四件石墨含量不同的衣服进行织物性能测试。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Preparation and Application of Anionic and Cationic Waterborne Polyurethanes and Graphene-Cellulose Nanocrystal as an Antistatic Agent for Cashmere
The main purpose of this research work is to improve anti-static properties of Cashmere fabric by introducing application comprising anti-static agent by foaming which was made with cationic waterborne polyurethane and graphene-CNC. Cashmere fabric was cut into 10 pieces of sample cloth of 5 cm * 5 cm size, washed with acetone solution, and then dried in an oven at 60℃. Three forms of waterborne polyurethanes such as two forms of Cationic waterborne polyurethane (CWPU) and a form of Anionic waterborne polyurethane (AWPU) were synthesized. Cellulose nanocrystalline (CNC)/graphite powder solution with the ratio of 0.5/1, 1/1, 2/1 was prepared by ultrasonic probe stripping method, and the concentration of graphite powder was ensured to be 1 mg/ml. The fabric was treated with anionic and cationic WPUs foaming solution until the weight gain reached 2.5 - 3.5 wt%. After drying, the elastic cloth was foamed with graphene solution until the graphite content of the cloth was close to 10%, 20%, 40%, 60% respectively, and then dried for reserving. Characterization properties of pure graphite powder, pure CNC and graphene solution with different proportions of three components were tested by Fourier transform infrared spectrometer (FTIR), X-ray diffraction (XRD), Thermalgravitimetric analysis (TGA) and scanning electron microscopy (SEM). Take the original cloth, only WPU treated cloth and four clothes with different graphite content for the fabric performance test.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
9
期刊最新文献
Graphene: Fabrication, Properties and Applications Introduction Future Histories: Graphene Innovation after Covid-19 Creating an Icon: The Making of a Global Brand Graphene City and Beyond: Building an Innovation Ecosystem
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1