{"title":"不锈钢的凝固开裂敏感性:新的测试和解释","authors":"Kun Liu, P. Yu, S. Kou","doi":"10.29391/2020.99.024","DOIUrl":null,"url":null,"abstract":"The susceptibility of austenitic, ferritic, and duplex stain-less steels to solidification cracking was evaluated by the new Transverse Motion Weldability (TMW) test. The focus was on austenitic stainless steels. 304L and 316L were least susceptible, 321 was significantly more susceptible, and 310 was much more susceptible. However, some 321 welds were even less susceptible than 304L welds. These 321 welds were found to have much finer grains to better resist solidification cracking. Quenching 321 during welding revealed spontaneous grain refining could occur by heterogeneous nucleation. For 304L, 316L, and 310, a new explanation for the susceptibility was proposed based on the continuity of the liquid between columnar dendrites; a discontinuous, isolated liquid allows bonding between dendrites to occur early to better resist cracking. In 304L and 316L, the dendrite-boundary liquid was discontinuous and isolated, as revealed by quenching. The liquid was likely depleted by both fast back diffusion into -dendrites (body-centered cubic) and the L +  + reaction, which consumed L while forming . In 310, however, the dendrites were separated by a continuous liquid that prevented early bonding between them. Back diffusion into -dendrites (face-centered cubic) was much slower, and the L +  + reaction formed little . Quenching also revealed skeletal/lacy formed in 304L and 316L well after solidification ended; thus, skeletal/lacy did not resist solidification cracking, as had been widely believed for decades. The TMW test further demonstrated that both more sulfur and slower welding can increase susceptibility.","PeriodicalId":23681,"journal":{"name":"Welding Journal","volume":null,"pages":null},"PeriodicalIF":2.2000,"publicationDate":"2020-10-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"14","resultStr":"{\"title\":\"Solidification Cracking Susceptibility of Stainless Steels: New Test and Explanation\",\"authors\":\"Kun Liu, P. Yu, S. Kou\",\"doi\":\"10.29391/2020.99.024\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The susceptibility of austenitic, ferritic, and duplex stain-less steels to solidification cracking was evaluated by the new Transverse Motion Weldability (TMW) test. The focus was on austenitic stainless steels. 304L and 316L were least susceptible, 321 was significantly more susceptible, and 310 was much more susceptible. However, some 321 welds were even less susceptible than 304L welds. These 321 welds were found to have much finer grains to better resist solidification cracking. Quenching 321 during welding revealed spontaneous grain refining could occur by heterogeneous nucleation. For 304L, 316L, and 310, a new explanation for the susceptibility was proposed based on the continuity of the liquid between columnar dendrites; a discontinuous, isolated liquid allows bonding between dendrites to occur early to better resist cracking. In 304L and 316L, the dendrite-boundary liquid was discontinuous and isolated, as revealed by quenching. The liquid was likely depleted by both fast back diffusion into -dendrites (body-centered cubic) and the L +  + reaction, which consumed L while forming . In 310, however, the dendrites were separated by a continuous liquid that prevented early bonding between them. Back diffusion into -dendrites (face-centered cubic) was much slower, and the L +  + reaction formed little . Quenching also revealed skeletal/lacy formed in 304L and 316L well after solidification ended; thus, skeletal/lacy did not resist solidification cracking, as had been widely believed for decades. The TMW test further demonstrated that both more sulfur and slower welding can increase susceptibility.\",\"PeriodicalId\":23681,\"journal\":{\"name\":\"Welding Journal\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":2.2000,\"publicationDate\":\"2020-10-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"14\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Welding Journal\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://doi.org/10.29391/2020.99.024\",\"RegionNum\":3,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q2\",\"JCRName\":\"METALLURGY & METALLURGICAL ENGINEERING\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Welding Journal","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.29391/2020.99.024","RegionNum":3,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"METALLURGY & METALLURGICAL ENGINEERING","Score":null,"Total":0}
引用次数: 14

摘要

采用新的横向运动可焊性(TMW)试验评价了奥氏体、铁素体和双相不锈钢对凝固开裂的敏感性。重点是奥氏体不锈钢。304L和316L的易感程度最低,321的易感程度显著提高,310的易感程度更高。然而,一些321焊缝甚至比304L焊缝更不容易受到影响。发现这些321焊缝具有更细的晶粒,以更好地抵抗凝固开裂。在焊接过程中淬火321,发现非均相形核可以自发细化晶粒。对于304L、316L和310,基于柱状枝晶间液体的连续性,提出了磁化率的新解释;不连续的、孤立的液体可以使枝晶之间的结合尽早发生,从而更好地抵抗开裂。在304L和316L中,枝晶边界液体不连续且孤立。液体的耗尽可能是由于快速反扩散到以体为中心的状枝晶(体心立方)和L ++ 反应,在形成的同时消耗L。然而,在310年,树突被一种连续的液体分开,阻止了它们之间的早期结合。反向扩散到-枝晶(面心立方)的速度要慢得多,L ++扩散反应形成的扩散较小。淬火后304L和316L凝固结束后也形成了良好的骨状/花边状结构;因此,骨状/蕾丝状胸片并不像几十年来人们普遍认为的那样能抵抗凝固开裂。TMW试验进一步表明,硫含量的增加和焊接速度的减慢都会增加磁化率。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Solidification Cracking Susceptibility of Stainless Steels: New Test and Explanation
The susceptibility of austenitic, ferritic, and duplex stain-less steels to solidification cracking was evaluated by the new Transverse Motion Weldability (TMW) test. The focus was on austenitic stainless steels. 304L and 316L were least susceptible, 321 was significantly more susceptible, and 310 was much more susceptible. However, some 321 welds were even less susceptible than 304L welds. These 321 welds were found to have much finer grains to better resist solidification cracking. Quenching 321 during welding revealed spontaneous grain refining could occur by heterogeneous nucleation. For 304L, 316L, and 310, a new explanation for the susceptibility was proposed based on the continuity of the liquid between columnar dendrites; a discontinuous, isolated liquid allows bonding between dendrites to occur early to better resist cracking. In 304L and 316L, the dendrite-boundary liquid was discontinuous and isolated, as revealed by quenching. The liquid was likely depleted by both fast back diffusion into -dendrites (body-centered cubic) and the L +  + reaction, which consumed L while forming . In 310, however, the dendrites were separated by a continuous liquid that prevented early bonding between them. Back diffusion into -dendrites (face-centered cubic) was much slower, and the L +  + reaction formed little . Quenching also revealed skeletal/lacy formed in 304L and 316L well after solidification ended; thus, skeletal/lacy did not resist solidification cracking, as had been widely believed for decades. The TMW test further demonstrated that both more sulfur and slower welding can increase susceptibility.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Welding Journal
Welding Journal 工程技术-冶金工程
CiteScore
3.00
自引率
0.00%
发文量
23
审稿时长
3 months
期刊介绍: The Welding Journal has been published continually since 1922 — an unmatched link to all issues and advancements concerning metal fabrication and construction. Each month the Welding Journal delivers news of the welding and metal fabricating industry. Stay informed on the latest products, trends, technology and events via in-depth articles, full-color photos and illustrations, and timely, cost-saving advice. Also featured are articles and supplements on related activities, such as testing and inspection, maintenance and repair, design, training, personal safety, and brazing and soldering.
期刊最新文献
SiO2-bearing Fluxes Induced Evolution of γ Columnar Grain Size Prediction of Ultrasonic Welding Parameters for Polymer Joining Effect of Wire Preheat and Feed Rate in X80 Steel Laser Root Welds: Part 1 — Microstructure A State-of-the-Art Review on Direct Welding of Polymer to Metal for Structural Applications: Part 1 — Promising Processes Effect of Wire Preheat and Feed Rate in X80 Steel Laser Root Welds: Part 2 — Mechanical Properties
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1