钠冷快堆蒸汽发生管自耗现象的实验研究

Ryota Umeda, K. Shimoyama, A. Kurihara
{"title":"钠冷快堆蒸汽发生管自耗现象的实验研究","authors":"Ryota Umeda, K. Shimoyama, A. Kurihara","doi":"10.3327/taesj.j19.012","DOIUrl":null,"url":null,"abstract":"The sodium – water reaction caused by failure of the steam generator tube of sodium-cooled fast re-actors causes the wastage phenomenon, which is erosive and corrosive. Self-wastage takes place in the early stage of the sodium – water reaction event when a very small amount of water / steam penetrates a microcrack. When self-wastage proceeds to the inside wall of the tube, the failed area and water leakage rate will increase, whereby the area affected by the sodium – water reaction will be likely to ex-tend. Thus, it is very important to clarify the self-wastage behavior for a locally affected region and detect water leakage in actual nuclear power plants. In this study, the authors performed self-wastage experiments under a high sodium temperature condition to evaluate the effects of the wastage form / geometry using two types of initial defect, i.e., the microfine pinhole and fatigue crack, and of the water leakage rate on the self-wastage rate. Taking into consideration the influence of crack type, we confirmed that the self-wastage rate did not strongly depend on the initial defect geometry. As a mechanism of the self-plug phenomenon, it is speculated that sodium oxide blocks and inhibits the progress of self-wastage. The dependence of the self-wastage rate on the initial sodium temperature was clearly observed, and a new self-wastage correlation was derived considering the initial sodium temperature.","PeriodicalId":55893,"journal":{"name":"Transactions of the Atomic Energy Society of Japan","volume":"1 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2020-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Experiments of Self-wastage Phenomena Elucidation in Steam Generator Tube of Sodium-cooled Fast Reactor\",\"authors\":\"Ryota Umeda, K. Shimoyama, A. Kurihara\",\"doi\":\"10.3327/taesj.j19.012\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The sodium – water reaction caused by failure of the steam generator tube of sodium-cooled fast re-actors causes the wastage phenomenon, which is erosive and corrosive. Self-wastage takes place in the early stage of the sodium – water reaction event when a very small amount of water / steam penetrates a microcrack. When self-wastage proceeds to the inside wall of the tube, the failed area and water leakage rate will increase, whereby the area affected by the sodium – water reaction will be likely to ex-tend. Thus, it is very important to clarify the self-wastage behavior for a locally affected region and detect water leakage in actual nuclear power plants. In this study, the authors performed self-wastage experiments under a high sodium temperature condition to evaluate the effects of the wastage form / geometry using two types of initial defect, i.e., the microfine pinhole and fatigue crack, and of the water leakage rate on the self-wastage rate. Taking into consideration the influence of crack type, we confirmed that the self-wastage rate did not strongly depend on the initial defect geometry. As a mechanism of the self-plug phenomenon, it is speculated that sodium oxide blocks and inhibits the progress of self-wastage. The dependence of the self-wastage rate on the initial sodium temperature was clearly observed, and a new self-wastage correlation was derived considering the initial sodium temperature.\",\"PeriodicalId\":55893,\"journal\":{\"name\":\"Transactions of the Atomic Energy Society of Japan\",\"volume\":\"1 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2020-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Transactions of the Atomic Energy Society of Japan\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.3327/taesj.j19.012\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q4\",\"JCRName\":\"Engineering\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Transactions of the Atomic Energy Society of Japan","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.3327/taesj.j19.012","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"Engineering","Score":null,"Total":0}
引用次数: 0

摘要

钠冷快堆蒸汽发生管失效引起的钠-水反应,造成侵蚀和腐蚀的损耗现象。当极少量的水/蒸汽穿透微裂纹时,自耗损发生在钠-水反应事件的早期。当自耗损发展到管内壁时,破坏面积和漏水率增加,受钠水反应影响的面积有可能扩大。因此,在实际核电站中,弄清局部受影响区域的自耗损行为和检测漏水是非常重要的。本研究通过高钠温度条件下的自耗损实验,考察了微细针孔和疲劳裂纹两种初始缺陷的耗损形式/几何形状以及漏水率对自耗损率的影响。考虑到裂纹类型的影响,我们证实了自损耗率与初始缺陷几何形状的关系并不强。作为自堵塞现象的一种机制,推测氧化钠阻断和抑制了自损耗的进程。研究了自耗损率与初始钠温度的关系,并推导了考虑初始钠温度的自耗损关系式。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Experiments of Self-wastage Phenomena Elucidation in Steam Generator Tube of Sodium-cooled Fast Reactor
The sodium – water reaction caused by failure of the steam generator tube of sodium-cooled fast re-actors causes the wastage phenomenon, which is erosive and corrosive. Self-wastage takes place in the early stage of the sodium – water reaction event when a very small amount of water / steam penetrates a microcrack. When self-wastage proceeds to the inside wall of the tube, the failed area and water leakage rate will increase, whereby the area affected by the sodium – water reaction will be likely to ex-tend. Thus, it is very important to clarify the self-wastage behavior for a locally affected region and detect water leakage in actual nuclear power plants. In this study, the authors performed self-wastage experiments under a high sodium temperature condition to evaluate the effects of the wastage form / geometry using two types of initial defect, i.e., the microfine pinhole and fatigue crack, and of the water leakage rate on the self-wastage rate. Taking into consideration the influence of crack type, we confirmed that the self-wastage rate did not strongly depend on the initial defect geometry. As a mechanism of the self-plug phenomenon, it is speculated that sodium oxide blocks and inhibits the progress of self-wastage. The dependence of the self-wastage rate on the initial sodium temperature was clearly observed, and a new self-wastage correlation was derived considering the initial sodium temperature.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Transactions of the Atomic Energy Society of Japan
Transactions of the Atomic Energy Society of Japan Energy-Nuclear Energy and Engineering
CiteScore
0.50
自引率
0.00%
发文量
16
期刊最新文献
Promotive Effects of Siltfence on Deposition of Suspended Particles: Evaluations of Diffusion Suppression of Radionuclides in Rectangular Open Channel via Numerical Simulations Circulation of Radioactive Cesium in Deciduous Broad-leaved Forests due to the Fukushima Daiichi Nuclear Power Plant Accident Machine Learning Sintering Density Prediction Model for MOX Fuel Pellet マイナーアクチノイド核変換用窒化物燃料の乾式再処理における崩壊熱の影響 Evaluation of external dose exposure of workers during house demolition and dose reduction work in a difficult-to-return zone
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1