{"title":"含铅冷却剂循环中结渣机理及氢水混合高温处理预防研究","authors":"M. Koshelev, V. Ulyanov, S. Kharchuk","doi":"10.55176/2414-1038-2021-3-191-205","DOIUrl":null,"url":null,"abstract":"The results of computational and experimental studies of the properties of lead and lead-bismuth coolants and the mechanism of physicochemical processes occurring in their circulation circuits explain the reasons for the formation of slag deposits based on lead oxide. First of all, this is the uncontrolled interaction of lead and lead-bismuth coolants with gaseous oxygen, which, along with nitrogen, is one of the main components of air. Slag deposits are based on lead oxides, but they also contain a significant amount of unoxidized lead (and bismuth in the case of using a lead-bismuth coolant) bound by a lead oxide framework into a single structure, as well as a small amount of components of construction materials (iron , chrome, nickel). The formation of slags in the circulation loop with a lead-containing coolant has a negative effect on its operation: the flow cross-sections are narrowed; heat transfer surfaces are blocked; the normal operation of pipeline fittings is disrupted. To minimize slag accumulation, it is necessary to limit the contact of the coolant with air oxygen, avoid draining the coolant from the circulation circuit, control whether the circulation circuit is in a depressurized state both during research and during non-working periods, when heating and filling the circuits with a coolant, create and maintain a vacuum. The best way to prevent slag accumulation is periodic hydrogen cleaning of the circuit with gas mixtures \"hydrogen - water vapor - inert gas\". The greatest cleaning efficiency is achieved when gas mixtures are introduced directly into the coolant flow using gas injection devices. Mechanical devices with moving parts, ejectors, nozzle nozzles can act as gas injection devices.","PeriodicalId":20426,"journal":{"name":"PROBLEMS OF ATOMIC SCIENCE AND TECHNOLOGY. SERIES: NUCLEAR AND REACTOR CONSTANTS","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2021-09-26","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"INVESTIGATION OF THE SLAGS ACCUMULATION MECHANISM IN LEAD-CONTAINING COOLANTS LOOPS AND ITS PREVENTION BY HIGH-TEMPERATURE TREATMENT WITH HYDROGEN AND WATER STEAM MIXTURES\",\"authors\":\"M. Koshelev, V. Ulyanov, S. Kharchuk\",\"doi\":\"10.55176/2414-1038-2021-3-191-205\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The results of computational and experimental studies of the properties of lead and lead-bismuth coolants and the mechanism of physicochemical processes occurring in their circulation circuits explain the reasons for the formation of slag deposits based on lead oxide. First of all, this is the uncontrolled interaction of lead and lead-bismuth coolants with gaseous oxygen, which, along with nitrogen, is one of the main components of air. Slag deposits are based on lead oxides, but they also contain a significant amount of unoxidized lead (and bismuth in the case of using a lead-bismuth coolant) bound by a lead oxide framework into a single structure, as well as a small amount of components of construction materials (iron , chrome, nickel). The formation of slags in the circulation loop with a lead-containing coolant has a negative effect on its operation: the flow cross-sections are narrowed; heat transfer surfaces are blocked; the normal operation of pipeline fittings is disrupted. To minimize slag accumulation, it is necessary to limit the contact of the coolant with air oxygen, avoid draining the coolant from the circulation circuit, control whether the circulation circuit is in a depressurized state both during research and during non-working periods, when heating and filling the circuits with a coolant, create and maintain a vacuum. The best way to prevent slag accumulation is periodic hydrogen cleaning of the circuit with gas mixtures \\\"hydrogen - water vapor - inert gas\\\". The greatest cleaning efficiency is achieved when gas mixtures are introduced directly into the coolant flow using gas injection devices. Mechanical devices with moving parts, ejectors, nozzle nozzles can act as gas injection devices.\",\"PeriodicalId\":20426,\"journal\":{\"name\":\"PROBLEMS OF ATOMIC SCIENCE AND TECHNOLOGY. SERIES: NUCLEAR AND REACTOR CONSTANTS\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2021-09-26\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"PROBLEMS OF ATOMIC SCIENCE AND TECHNOLOGY. SERIES: NUCLEAR AND REACTOR CONSTANTS\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.55176/2414-1038-2021-3-191-205\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"PROBLEMS OF ATOMIC SCIENCE AND TECHNOLOGY. SERIES: NUCLEAR AND REACTOR CONSTANTS","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.55176/2414-1038-2021-3-191-205","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

对铅和铅铋冷却剂的性质及其循环回路中发生的物理化学过程机制的计算和实验研究结果解释了氧化铅渣沉积形成的原因。首先,这是铅和铅铋冷却剂与气态氧的不受控制的相互作用,气态氧和氮气是空气的主要成分之一。矿渣沉积物的基础是氧化铅,但它们也含有大量未氧化的铅(在使用铅铋冷却剂的情况下含有铋),这些铅被氧化铅框架结合成一个单一的结构,以及少量的建筑材料成分(铁、铬、镍)。含铅冷却剂在循环回路中形成的结渣对其运行有负面影响:流动截面变窄;传热面被堵塞;管道管件的正常运行受到干扰。为了最大限度地减少积渣,有必要限制冷却剂与空气氧的接触,避免从循环回路中排出冷却剂,控制循环回路在研究和非工作期间是否处于减压状态,在加热和填充冷却剂回路时,创造并保持真空。防止渣堆积的最好方法是用“氢气-水蒸气-惰性气体”混合气体定期对电路进行氢清洗。当使用气体喷射装置将气体混合物直接引入冷却剂流中时,可实现最大的清洁效率。带有活动部件的机械装置、喷射器、喷嘴等可作为气体喷射装置。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
INVESTIGATION OF THE SLAGS ACCUMULATION MECHANISM IN LEAD-CONTAINING COOLANTS LOOPS AND ITS PREVENTION BY HIGH-TEMPERATURE TREATMENT WITH HYDROGEN AND WATER STEAM MIXTURES
The results of computational and experimental studies of the properties of lead and lead-bismuth coolants and the mechanism of physicochemical processes occurring in their circulation circuits explain the reasons for the formation of slag deposits based on lead oxide. First of all, this is the uncontrolled interaction of lead and lead-bismuth coolants with gaseous oxygen, which, along with nitrogen, is one of the main components of air. Slag deposits are based on lead oxides, but they also contain a significant amount of unoxidized lead (and bismuth in the case of using a lead-bismuth coolant) bound by a lead oxide framework into a single structure, as well as a small amount of components of construction materials (iron , chrome, nickel). The formation of slags in the circulation loop with a lead-containing coolant has a negative effect on its operation: the flow cross-sections are narrowed; heat transfer surfaces are blocked; the normal operation of pipeline fittings is disrupted. To minimize slag accumulation, it is necessary to limit the contact of the coolant with air oxygen, avoid draining the coolant from the circulation circuit, control whether the circulation circuit is in a depressurized state both during research and during non-working periods, when heating and filling the circuits with a coolant, create and maintain a vacuum. The best way to prevent slag accumulation is periodic hydrogen cleaning of the circuit with gas mixtures "hydrogen - water vapor - inert gas". The greatest cleaning efficiency is achieved when gas mixtures are introduced directly into the coolant flow using gas injection devices. Mechanical devices with moving parts, ejectors, nozzle nozzles can act as gas injection devices.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
POSSIBILITY OF APPLICATION OF ZrO2-MgO-CaO CRUCIBLES FOR PRODUCING ALLOY U-10 % Zr CALCULATION ESTIMATION OF THE REQUIRED HEAT GENERATION IN TESTING FUEL ELEMENTS TO ACHIEVE SUPERCRITICAL PARAMETERS OF THE COOLANT UNDER IRRADIATION IN THE RESEARCH NUCLEAR REACTOR FEATURES OF THERMAL HYDRAULICS OF ACTIVE ZONES OF FAST LOW-POWER AND HIGH-POWER SODIUM PRODUCTION REACTORS FOR A CLOSED FUEL CYCLE SYSTEM CALCULATION OF THE STRUCTURAL MATERIALS ACTIVATION BY A FUSION NEUTRON FLUX WITH BPSD CODE HEAT PIPES IN NUCLEAR ENGINEERING
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1