{"title":"缺陷工程硅的压阻","authors":"H. Li, A. Thayil, C. Lew, M. Filoche, B. C. Johnson, J. McCallum, S. Arscott, A. Rowe","doi":"10.1103/PHYSREVAPPLIED.15.014046","DOIUrl":null,"url":null,"abstract":"The steady-state, space-charge-limited piezoresistance (PZR) of defect-engineered, silicon-on-insulator device layers containing silicon divacancy defects changes sign as a function of applied bias. Above a punch-through voltage ($V_t$) corresponding to the onset of a space-charge-limited hole current, the longitudinal $\\langle 110 \\rangle$ PZR $\\pi$-coefficient is $\\pi \\approx 65 \\times 10^{-11}$~Pa$^{-1}$, similar to the value obtained in charge-neutral, p-type silicon. Below $V_t$, the mechanical stress dependence of the Shockley-Read-Hall (SRH) recombination parameters, specifically the divacancy trap energy $E_T$ which is estimated to vary by $\\approx 30$~$\\mu$V/MPa, yields $\\pi \\approx -25 \\times 10^{-11}$~Pa$^{-1}$. The combination of space-charge-limited transport and defect engineering which significantly reduces SRH recombination lifetimes makes this work directly relevant to discussions of giant or anomalous PZR at small strains in nano-silicon whose characteristic dimension is larger than a few nanometers. In this limit the reduced electrostatic dimensionality lowers $V_t$ and amplifies space-charge-limited currents and efficient SRH recombination occurs via surface defects. The results reinforce the growing evidence that in steady state, electro-mechanically active defects can result in anomalous, but not giant, PZR.","PeriodicalId":8423,"journal":{"name":"arXiv: Applied Physics","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2020-08-11","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Piezoresistance in Defect-Engineered Silicon\",\"authors\":\"H. Li, A. Thayil, C. Lew, M. Filoche, B. C. Johnson, J. McCallum, S. Arscott, A. Rowe\",\"doi\":\"10.1103/PHYSREVAPPLIED.15.014046\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The steady-state, space-charge-limited piezoresistance (PZR) of defect-engineered, silicon-on-insulator device layers containing silicon divacancy defects changes sign as a function of applied bias. Above a punch-through voltage ($V_t$) corresponding to the onset of a space-charge-limited hole current, the longitudinal $\\\\langle 110 \\\\rangle$ PZR $\\\\pi$-coefficient is $\\\\pi \\\\approx 65 \\\\times 10^{-11}$~Pa$^{-1}$, similar to the value obtained in charge-neutral, p-type silicon. Below $V_t$, the mechanical stress dependence of the Shockley-Read-Hall (SRH) recombination parameters, specifically the divacancy trap energy $E_T$ which is estimated to vary by $\\\\approx 30$~$\\\\mu$V/MPa, yields $\\\\pi \\\\approx -25 \\\\times 10^{-11}$~Pa$^{-1}$. The combination of space-charge-limited transport and defect engineering which significantly reduces SRH recombination lifetimes makes this work directly relevant to discussions of giant or anomalous PZR at small strains in nano-silicon whose characteristic dimension is larger than a few nanometers. In this limit the reduced electrostatic dimensionality lowers $V_t$ and amplifies space-charge-limited currents and efficient SRH recombination occurs via surface defects. The results reinforce the growing evidence that in steady state, electro-mechanically active defects can result in anomalous, but not giant, PZR.\",\"PeriodicalId\":8423,\"journal\":{\"name\":\"arXiv: Applied Physics\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2020-08-11\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"arXiv: Applied Physics\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1103/PHYSREVAPPLIED.15.014046\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"arXiv: Applied Physics","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1103/PHYSREVAPPLIED.15.014046","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

含有硅间隙缺陷的绝缘体上硅器件层的稳态、空间电荷限制压阻(PZR)随施加偏置的函数而变化。在对应于空间电荷限制空穴电流起始的穿孔电压($V_t$)以上,纵向$\langle 110 \rangle$ PZR $\pi$ -系数为$\pi \approx 65 \times 10^{-11}$ Pa $^{-1}$,类似于在电荷中性的p型硅中获得的值。在$V_t$下面,Shockley-Read-Hall (SRH)复合参数的机械应力依赖关系,特别是距离陷阱能量$E_T$,估计变化为$\approx 30$$\mu$ V/MPa,得到$\pi \approx -25 \times 10^{-11}$ Pa $^{-1}$。空间电荷限制输运和缺陷工程的结合显著降低了SRH重组寿命,这使得这项工作与纳米硅中特征尺寸大于几纳米的小应变下的巨大或异常PZR的讨论直接相关。在这个极限下,降低的静电维数降低$V_t$并放大空间电荷限制电流,通过表面缺陷发生有效的SRH重组。结果强化了越来越多的证据,即在稳态下,机电活性缺陷可以导致异常的PZR,但不会导致巨大的PZR。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Piezoresistance in Defect-Engineered Silicon
The steady-state, space-charge-limited piezoresistance (PZR) of defect-engineered, silicon-on-insulator device layers containing silicon divacancy defects changes sign as a function of applied bias. Above a punch-through voltage ($V_t$) corresponding to the onset of a space-charge-limited hole current, the longitudinal $\langle 110 \rangle$ PZR $\pi$-coefficient is $\pi \approx 65 \times 10^{-11}$~Pa$^{-1}$, similar to the value obtained in charge-neutral, p-type silicon. Below $V_t$, the mechanical stress dependence of the Shockley-Read-Hall (SRH) recombination parameters, specifically the divacancy trap energy $E_T$ which is estimated to vary by $\approx 30$~$\mu$V/MPa, yields $\pi \approx -25 \times 10^{-11}$~Pa$^{-1}$. The combination of space-charge-limited transport and defect engineering which significantly reduces SRH recombination lifetimes makes this work directly relevant to discussions of giant or anomalous PZR at small strains in nano-silicon whose characteristic dimension is larger than a few nanometers. In this limit the reduced electrostatic dimensionality lowers $V_t$ and amplifies space-charge-limited currents and efficient SRH recombination occurs via surface defects. The results reinforce the growing evidence that in steady state, electro-mechanically active defects can result in anomalous, but not giant, PZR.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
High performance photonic microwave filters based on a 50GHz FSR optical soliton crystal Kerr micro-comb Ultra-high bandwidth fiber-optic data transmission with a single chip source High order pulse-echo (HOPE) ultrasound Data-driven modelling of scalable spinodoid structures for energy absorption Radioplasmonics: design of plasmonic milli-particles in air and absorbing media for antenna communication and human-body in-vivo applications.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1