{"title":"热固化义齿基托丙烯酸树脂的抗断裂性能试验","authors":"Aleksandra Maletin, Jovana Bastajić, I. Ristić, Branislava Petronijević Šarčev, Isidora Nešković, Tanja Veljović, D. Marković","doi":"10.7251/comen1802130m","DOIUrl":null,"url":null,"abstract":"For many years, poly-methyl methacrylate has been used as a material of choice for making the denture base, thanks to its good and desirable performances, such as: simplicity in work, possibility of reparation, aesthetics and affordable price. Considering to its insufficient hardness and fracture resistance, there is a tendency to improve the mechanical properties of the material, by changing its basic composition. The aim of the research was to determine the fracture resistance of the heat-curing denture base acrylic resin materials. Materials and methods: For the research ,20 samples of the 2 heat-curing acrylics had been prepared, standard ones and reinforced acrylic resin material. After the storage in the saline for 15 days, measurements of the fracture resistance were performed by using the universal testing device. The data were statistically processed using the Student’s t-test for independent samples. Results: By measuring the flexural strength and deflection at breakage, it has been proven that there was, statistically, a significant difference of the flexural strength between reinforced (179.91-248.72MPa) and standard heat-curing acrylics (183.25- 200.74MPa). The deflection at breakage showed approximately the same values for both materials (1,0-1,4mm; 1.0-1.5mm). Conclusion: By enhancing the polymer, the mechanical properties of the denture base acrylic resin materials will be improved, primarily, higher fracture resistance, that means that these technologies need to be improved.","PeriodicalId":10617,"journal":{"name":"Contemporary Materials","volume":"17 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2018-10-10","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":"{\"title\":\"TESTING OF THE FRACTURE RESISTANCE OF THE HEAT-CURING DENTURE BASE ACRYLIC RESIN\",\"authors\":\"Aleksandra Maletin, Jovana Bastajić, I. Ristić, Branislava Petronijević Šarčev, Isidora Nešković, Tanja Veljović, D. Marković\",\"doi\":\"10.7251/comen1802130m\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"For many years, poly-methyl methacrylate has been used as a material of choice for making the denture base, thanks to its good and desirable performances, such as: simplicity in work, possibility of reparation, aesthetics and affordable price. Considering to its insufficient hardness and fracture resistance, there is a tendency to improve the mechanical properties of the material, by changing its basic composition. The aim of the research was to determine the fracture resistance of the heat-curing denture base acrylic resin materials. Materials and methods: For the research ,20 samples of the 2 heat-curing acrylics had been prepared, standard ones and reinforced acrylic resin material. After the storage in the saline for 15 days, measurements of the fracture resistance were performed by using the universal testing device. The data were statistically processed using the Student’s t-test for independent samples. Results: By measuring the flexural strength and deflection at breakage, it has been proven that there was, statistically, a significant difference of the flexural strength between reinforced (179.91-248.72MPa) and standard heat-curing acrylics (183.25- 200.74MPa). The deflection at breakage showed approximately the same values for both materials (1,0-1,4mm; 1.0-1.5mm). Conclusion: By enhancing the polymer, the mechanical properties of the denture base acrylic resin materials will be improved, primarily, higher fracture resistance, that means that these technologies need to be improved.\",\"PeriodicalId\":10617,\"journal\":{\"name\":\"Contemporary Materials\",\"volume\":\"17 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2018-10-10\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"1\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Contemporary Materials\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.7251/comen1802130m\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Contemporary Materials","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.7251/comen1802130m","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1

摘要

多年来,聚甲基丙烯酸甲酯一直被用作制作义齿基托的首选材料,因为它具有工作简单、易于修复、美观、价格实惠等优良性能。考虑到材料的硬度和抗断裂能力不足,人们倾向于通过改变材料的基本成分来改善材料的力学性能。研究热固化义齿基托丙烯酸树脂材料的抗断裂性能。材料与方法:本研究共制备了2种热固化丙烯酸树脂、标准丙烯酸树脂和增强丙烯酸树脂材料各20个样品。在盐水中保存15天后,使用通用测试装置进行抗骨折性测试。使用独立样本的学生t检验对数据进行统计处理。结果:通过测定抗折强度和断裂挠度,证明增强材料抗折强度(179.91 ~ 248.72 mpa)与标准热固化丙烯酸材料抗折强度(183.25 ~ 200.74MPa)有统计学差异。断裂时的挠度在两种材料中显示出大致相同的值(0,0 -1,4mm;1.0 - -1.5毫米)。结论:通过增强聚合物,可以改善义齿基托丙烯酸树脂材料的力学性能,主要是提高抗断裂性能,这意味着这些技术需要改进。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
TESTING OF THE FRACTURE RESISTANCE OF THE HEAT-CURING DENTURE BASE ACRYLIC RESIN
For many years, poly-methyl methacrylate has been used as a material of choice for making the denture base, thanks to its good and desirable performances, such as: simplicity in work, possibility of reparation, aesthetics and affordable price. Considering to its insufficient hardness and fracture resistance, there is a tendency to improve the mechanical properties of the material, by changing its basic composition. The aim of the research was to determine the fracture resistance of the heat-curing denture base acrylic resin materials. Materials and methods: For the research ,20 samples of the 2 heat-curing acrylics had been prepared, standard ones and reinforced acrylic resin material. After the storage in the saline for 15 days, measurements of the fracture resistance were performed by using the universal testing device. The data were statistically processed using the Student’s t-test for independent samples. Results: By measuring the flexural strength and deflection at breakage, it has been proven that there was, statistically, a significant difference of the flexural strength between reinforced (179.91-248.72MPa) and standard heat-curing acrylics (183.25- 200.74MPa). The deflection at breakage showed approximately the same values for both materials (1,0-1,4mm; 1.0-1.5mm). Conclusion: By enhancing the polymer, the mechanical properties of the denture base acrylic resin materials will be improved, primarily, higher fracture resistance, that means that these technologies need to be improved.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
LABORATORY TESTING OF UNSTIMULATED AND STIMULATED SALIVA BUFFERING CAPACITY IN PATIENT AND CONTROL GROUPS AFTER TITRATION WITH HCl AND NaOH NEURAL NETWORKS FOR SOLVING HUXLEY’S EQUATION USE OF 3D-BIOPRINTING IN TISSUE ENGINEERING SCAFFOLD PRODUCTION DETERMINATION OF IRON CONTENT IN NATURAL MINERAL WATER: COMPARISON OF ICP-OES AND SPECTROPHOTOMETRIC METHOD INFLUENCE OF GEOLOGICAL PARAMETERS ON THE INDOOR RADON CONCENTRATION IN THE CITY OF TREBINJE
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1