{"title":"铁在钨中的偏析","authors":"L. Uray, M. Menyhárd","doi":"10.1002/PSSA.2210840108","DOIUrl":null,"url":null,"abstract":"Segregation and solution of iron is followed up on a commercial WFe dilute alloy by measuring electrical resistivity, thermopower and — on the fracture surface — AES. The thermopower measures practically only the solute iron concentration in this alloy. At the same time the excess electrical resistivity is sensitive mostly to the concentration of grain boundaries and the AES measures the iron accumulated on the surface of the grain boundaries. According to these measurements grain boundary segregation occurs at temperatures where the bulk diffusion is negligible yet. So this segregation can be explained only by moving grain boundaries, which “sweep over” the crystallites, accumulating the iron atoms. It turned out that only a part of the iron segregated onto the grain boundaries, the larger part segregated onto the second phases, although their total surface is about ten times less. Supposing a state close to the equilibrium, the heats of segregation is estimated to be 50 and 100 to 120 kJ/mol for segregation to grain boundaries and to second phases, respectively. \n \n \n \nDie Segregation und die Losung von Eisen werden durch die Messung des elektrischen Widerstandes, der Thermokraft und der AES auf der Bruchflache einer diinnen kommerziellen WFe-Legierung untersucht. Die Thermokraft zeigt praktisch nur die Konzentration des gelosten Eisens in dieser Legierung an. Zur gleichen Zeit reagiert der elektrische Zusatzwiderstand hauptsachlich empfindlich auf die Konzentration der Korngrenzen und die AES mist das Eisen, welches sich auf der Flache der Korngrenzen sammelt. Diese Mesergebnisse zeigen, das die Ausscheidung des Eisens an den Korngrenzen bei solchen niedrigen Temperaturen stattfindet, bei denendie volumen-diffusion vernachlassigt werden kann. Diese Ausscheidung des Eisens kann dadurch erklart werden, das die Korngrenzen wahrend ihrer Bewegungen die sich in den Korninneren befindlichen Eisenatome sammeln. Weiterhin zeigen die Mesergebnisse, das nur ein kleiner Teil des Eisens sich an den Korngrenzen ausscheidet, der gros ere Teil mus sich anf den zweiten Phasen aus-scheiden, obwohl ihre Gesamtflaehe ungefahr zehnmal kleiner ist. Ein Zustand in der Nahe des Gleichgewichts vorausgesetzt, betragt die Ausscheidungswarme fur die Ausscheidungen an Korngrenzen bzw. auf zweiten Phasen 50 bzw. 100 bis 120 kJ/mol.","PeriodicalId":17793,"journal":{"name":"July 16","volume":"26 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"1984-07-16","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"10","resultStr":"{\"title\":\"The Segregation of Iron in Tungsten\",\"authors\":\"L. Uray, M. Menyhárd\",\"doi\":\"10.1002/PSSA.2210840108\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Segregation and solution of iron is followed up on a commercial WFe dilute alloy by measuring electrical resistivity, thermopower and — on the fracture surface — AES. The thermopower measures practically only the solute iron concentration in this alloy. At the same time the excess electrical resistivity is sensitive mostly to the concentration of grain boundaries and the AES measures the iron accumulated on the surface of the grain boundaries. According to these measurements grain boundary segregation occurs at temperatures where the bulk diffusion is negligible yet. So this segregation can be explained only by moving grain boundaries, which “sweep over” the crystallites, accumulating the iron atoms. It turned out that only a part of the iron segregated onto the grain boundaries, the larger part segregated onto the second phases, although their total surface is about ten times less. Supposing a state close to the equilibrium, the heats of segregation is estimated to be 50 and 100 to 120 kJ/mol for segregation to grain boundaries and to second phases, respectively. \\n \\n \\n \\nDie Segregation und die Losung von Eisen werden durch die Messung des elektrischen Widerstandes, der Thermokraft und der AES auf der Bruchflache einer diinnen kommerziellen WFe-Legierung untersucht. Die Thermokraft zeigt praktisch nur die Konzentration des gelosten Eisens in dieser Legierung an. Zur gleichen Zeit reagiert der elektrische Zusatzwiderstand hauptsachlich empfindlich auf die Konzentration der Korngrenzen und die AES mist das Eisen, welches sich auf der Flache der Korngrenzen sammelt. Diese Mesergebnisse zeigen, das die Ausscheidung des Eisens an den Korngrenzen bei solchen niedrigen Temperaturen stattfindet, bei denendie volumen-diffusion vernachlassigt werden kann. Diese Ausscheidung des Eisens kann dadurch erklart werden, das die Korngrenzen wahrend ihrer Bewegungen die sich in den Korninneren befindlichen Eisenatome sammeln. Weiterhin zeigen die Mesergebnisse, das nur ein kleiner Teil des Eisens sich an den Korngrenzen ausscheidet, der gros ere Teil mus sich anf den zweiten Phasen aus-scheiden, obwohl ihre Gesamtflaehe ungefahr zehnmal kleiner ist. Ein Zustand in der Nahe des Gleichgewichts vorausgesetzt, betragt die Ausscheidungswarme fur die Ausscheidungen an Korngrenzen bzw. auf zweiten Phasen 50 bzw. 100 bis 120 kJ/mol.\",\"PeriodicalId\":17793,\"journal\":{\"name\":\"July 16\",\"volume\":\"26 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1984-07-16\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"10\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"July 16\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1002/PSSA.2210840108\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"July 16","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1002/PSSA.2210840108","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 10
摘要
通过电阻率、热功率和断口表面AES的测量,对一种WFe稀合金进行了铁的偏析和溶解。热电仪实际上只测量合金中溶质铁的浓度。同时,过量电阻率主要对晶界浓度敏感,原子发射光谱测量的是晶界表面铁的积累。根据这些测量,晶界偏析发生在体扩散还可以忽略不计的温度下。所以这种分离只能通过移动晶界来解释,它“横扫”了晶体,积聚了铁原子。结果表明,只有一部分铁偏析到晶界上,大部分铁偏析到第二相上,尽管它们的总表面大约是前者的十分之一。假设接近平衡状态,估计晶界偏析热为50 kJ/mol,第二相偏析热为100 ~ 120 kJ/mol。模具分离、模具失效、模具失效、模具失效、模具失效、模具失效、模具失效、模具失效、模具失效。热转印工艺的研究与应用。Zur gleichen Zeit reagert der elektrische Zusatzwiderstand hauptsachlich empfinlich auf die konzation der konngrenzen和die AES mist as Eisen, welches der Flache der konngrenzen sammelt。Diese Mesergebnisse zeigen, das die Ausscheidung des Eisens和den Korngrenzen bei solchen niedrien温度统计,bei denendie体积扩散理论分类。在德国,当我们在德国,当我们在德国,当我们在德国,当我们在德国,当我们在德国,当我们在德国,当我们在德国,当我们在德国,当我们在德国,当我们在德国。weiterin zeigen die Mesergebnisse, das nur ein kleiner Teil des Eisens sich and den Korngrenzen ausschidet, der gros是Teil mus sich和den zweiten Phasen ausschiden,即Gesamtflaehe ungefahr zehnmal kleiner ist。在此基础上,提出了一种新的研究方法,即建立一个新的研究模型,建立一个新的研究模型。auf zweiten相位50 bzw。100比120 kJ/mol。
Segregation and solution of iron is followed up on a commercial WFe dilute alloy by measuring electrical resistivity, thermopower and — on the fracture surface — AES. The thermopower measures practically only the solute iron concentration in this alloy. At the same time the excess electrical resistivity is sensitive mostly to the concentration of grain boundaries and the AES measures the iron accumulated on the surface of the grain boundaries. According to these measurements grain boundary segregation occurs at temperatures where the bulk diffusion is negligible yet. So this segregation can be explained only by moving grain boundaries, which “sweep over” the crystallites, accumulating the iron atoms. It turned out that only a part of the iron segregated onto the grain boundaries, the larger part segregated onto the second phases, although their total surface is about ten times less. Supposing a state close to the equilibrium, the heats of segregation is estimated to be 50 and 100 to 120 kJ/mol for segregation to grain boundaries and to second phases, respectively.
Die Segregation und die Losung von Eisen werden durch die Messung des elektrischen Widerstandes, der Thermokraft und der AES auf der Bruchflache einer diinnen kommerziellen WFe-Legierung untersucht. Die Thermokraft zeigt praktisch nur die Konzentration des gelosten Eisens in dieser Legierung an. Zur gleichen Zeit reagiert der elektrische Zusatzwiderstand hauptsachlich empfindlich auf die Konzentration der Korngrenzen und die AES mist das Eisen, welches sich auf der Flache der Korngrenzen sammelt. Diese Mesergebnisse zeigen, das die Ausscheidung des Eisens an den Korngrenzen bei solchen niedrigen Temperaturen stattfindet, bei denendie volumen-diffusion vernachlassigt werden kann. Diese Ausscheidung des Eisens kann dadurch erklart werden, das die Korngrenzen wahrend ihrer Bewegungen die sich in den Korninneren befindlichen Eisenatome sammeln. Weiterhin zeigen die Mesergebnisse, das nur ein kleiner Teil des Eisens sich an den Korngrenzen ausscheidet, der gros ere Teil mus sich anf den zweiten Phasen aus-scheiden, obwohl ihre Gesamtflaehe ungefahr zehnmal kleiner ist. Ein Zustand in der Nahe des Gleichgewichts vorausgesetzt, betragt die Ausscheidungswarme fur die Ausscheidungen an Korngrenzen bzw. auf zweiten Phasen 50 bzw. 100 bis 120 kJ/mol.