应变控制载荷下耐热镍基合金EP741NP和EI698VD的循环行为

A. Khudiakova, A. N. Servetnik, M. Volkov, S. B. Polianskii
{"title":"应变控制载荷下耐热镍基合金EP741NP和EI698VD的循环行为","authors":"A. Khudiakova, A. N. Servetnik, M. Volkov, S. B. Polianskii","doi":"10.26896/1028-6861-2023-89-4-50-62","DOIUrl":null,"url":null,"abstract":"Low cycle fatigue behavior of nickel-base alloys EP741NP and EI698VD under strain-control loading with zero strain ratio was studied for a wide range of strain amplitudes and temperatures. Dependences of the stress amplitude, mean stress and plastic strain range on the number of cycles were analyzed. Three stages of the cyclic behavior were marked out: the first stage of non-steady behavior with hardening, or softening, or transition from hardening to softening; the second stage of steady hardening, softening or stability; and the third stage associated with a crack development. Qualitative and quantitative parameters are proposed that make it possible to determine a share of the first stage of cyclic instability in the total cyclic durability and the nature of the material behavior in the first and second stages proceeding from the analysis of the dependence of the range of plastic deformations on the cycle number. The absence of cyclic stability was demonstrated for both alloys almost in the whole range of testing. It was shown, that the contribution of the first stage to the fatigue life (total durability) can be up to 30% and the greater the strain range, the greater the contribution. The temperature dependence of the character of cyclic behavior of materials is revealed. Alloy EP741NP is softened at the first and second stages at room temperature and is liable to hardening at elevated temperatures 300, 450, and 600°C, whereas alloy EI698VD is hardened at the first stage at 20 and 400°C, but inclines to softening at 650°C. At the second stage alloy EI698VD inclines to softening at 20 and 650°C and is liable to hardening at 400°C. With strain ranges 0.6 and 0.7%, both alloys can be considered cyclic stable at the second stage over the entire temperature range","PeriodicalId":13559,"journal":{"name":"Industrial laboratory. Diagnostics of materials","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2023-04-22","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Cyclic behavior of heat resistant nickel-base alloys EP741NP and EI698VD under strain-control loading\",\"authors\":\"A. Khudiakova, A. N. Servetnik, M. Volkov, S. B. Polianskii\",\"doi\":\"10.26896/1028-6861-2023-89-4-50-62\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Low cycle fatigue behavior of nickel-base alloys EP741NP and EI698VD under strain-control loading with zero strain ratio was studied for a wide range of strain amplitudes and temperatures. Dependences of the stress amplitude, mean stress and plastic strain range on the number of cycles were analyzed. Three stages of the cyclic behavior were marked out: the first stage of non-steady behavior with hardening, or softening, or transition from hardening to softening; the second stage of steady hardening, softening or stability; and the third stage associated with a crack development. Qualitative and quantitative parameters are proposed that make it possible to determine a share of the first stage of cyclic instability in the total cyclic durability and the nature of the material behavior in the first and second stages proceeding from the analysis of the dependence of the range of plastic deformations on the cycle number. The absence of cyclic stability was demonstrated for both alloys almost in the whole range of testing. It was shown, that the contribution of the first stage to the fatigue life (total durability) can be up to 30% and the greater the strain range, the greater the contribution. The temperature dependence of the character of cyclic behavior of materials is revealed. Alloy EP741NP is softened at the first and second stages at room temperature and is liable to hardening at elevated temperatures 300, 450, and 600°C, whereas alloy EI698VD is hardened at the first stage at 20 and 400°C, but inclines to softening at 650°C. At the second stage alloy EI698VD inclines to softening at 20 and 650°C and is liable to hardening at 400°C. With strain ranges 0.6 and 0.7%, both alloys can be considered cyclic stable at the second stage over the entire temperature range\",\"PeriodicalId\":13559,\"journal\":{\"name\":\"Industrial laboratory. Diagnostics of materials\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2023-04-22\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Industrial laboratory. Diagnostics of materials\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.26896/1028-6861-2023-89-4-50-62\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Industrial laboratory. Diagnostics of materials","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.26896/1028-6861-2023-89-4-50-62","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

研究了零应变比应变控制载荷下EP741NP和EI698VD镍基合金在宽应变幅值和温度范围内的低周疲劳行为。分析了应力幅值、平均应力和塑性应变范围与循环次数的关系。循环行为分为三个阶段:第一阶段为非稳态行为,伴硬化或软化,或由硬化向软化过渡;稳定硬化、软化或稳定的第二阶段;第三阶段与裂缝发育有关。通过分析塑性变形范围对循环次数的依赖关系,提出了定性和定量参数,可以确定第一阶段循环不稳定在总循环耐久性中的份额,以及材料在第一和第二阶段的行为性质。几乎在整个测试范围内,两种合金都没有循环稳定性。结果表明,第一阶段对疲劳寿命(总耐久性)的贡献可达30%,且应变范围越大,贡献越大。揭示了材料循环特性的温度依赖性。EP741NP合金在室温下处于第一和第二阶段软化,在300、450和600℃的高温下容易硬化,而EI698VD合金在20和400℃时处于第一阶段硬化,但在650℃时倾向软化。在第二阶段,合金EI698VD在20°C和650°C时倾向于软化,在400°C时容易硬化。当应变范围为0.6和0.7%时,两种合金在整个温度范围内的第二阶段都可以认为是循环稳定的
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Cyclic behavior of heat resistant nickel-base alloys EP741NP and EI698VD under strain-control loading
Low cycle fatigue behavior of nickel-base alloys EP741NP and EI698VD under strain-control loading with zero strain ratio was studied for a wide range of strain amplitudes and temperatures. Dependences of the stress amplitude, mean stress and plastic strain range on the number of cycles were analyzed. Three stages of the cyclic behavior were marked out: the first stage of non-steady behavior with hardening, or softening, or transition from hardening to softening; the second stage of steady hardening, softening or stability; and the third stage associated with a crack development. Qualitative and quantitative parameters are proposed that make it possible to determine a share of the first stage of cyclic instability in the total cyclic durability and the nature of the material behavior in the first and second stages proceeding from the analysis of the dependence of the range of plastic deformations on the cycle number. The absence of cyclic stability was demonstrated for both alloys almost in the whole range of testing. It was shown, that the contribution of the first stage to the fatigue life (total durability) can be up to 30% and the greater the strain range, the greater the contribution. The temperature dependence of the character of cyclic behavior of materials is revealed. Alloy EP741NP is softened at the first and second stages at room temperature and is liable to hardening at elevated temperatures 300, 450, and 600°C, whereas alloy EI698VD is hardened at the first stage at 20 and 400°C, but inclines to softening at 650°C. At the second stage alloy EI698VD inclines to softening at 20 and 650°C and is liable to hardening at 400°C. With strain ranges 0.6 and 0.7%, both alloys can be considered cyclic stable at the second stage over the entire temperature range
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
CiteScore
0.60
自引率
0.00%
发文量
0
期刊最新文献
Evaluation of the use of polyvinyl alcohol in the manufacture of pressed samples for X-ray fluorescence analysis Determination of the criterion for the morphological classification of etching pits formed in InSb single crystals grown by the Czochralski method in the crystallographic direction [111] and doped with tellurium The paradigm shift in mathematical methods of research Low cycle fracture resistance of the superalloy at single- and two-frequency modes of loading Fatigue fracture of 316L steel manufactured by selective laser melting method
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1