{"title":"锰岩浸出结果制备二氧化锰-石墨烯复合材料及电性能测试","authors":"Asri Saleh","doi":"10.9734/ajacr/2022/v13i1-2232","DOIUrl":null,"url":null,"abstract":"This study aims to synthesize and test the electrical properties of the MnO2-graphene composite from the leaching of manganese rock. The test method is carried out by testing the electrical properties with the parameters, namely capacitance (C), current (I), voltage (V), resistance (R), and conductometer. Each tested three concentration variations, 0.25: 0.75, 0.5: 0.05, and 0.75: 0.5. Supporting parameters for testing use X-Ray Diffraction (XRD) and Fourier Transform Infrared (FTIR). The results showed that the effect of varying the mass ratio of the MnO2-Graphene composite on the capacitance value was 192.3ꙡF in the variation of 0.25 gr: 0.75, meaning that the higher the concentration of the graphene carbon ratio, the higher the absorption capacity to store charge and electrical energy. For the variation of the voltage obtained by 353 mV at 0.25 gr: 0.75 variations, the current testing variation obtained a value of 13.6 mA at 0.25 gr: 0.75 variations, the variation on resistance obtained the lowest resistance value of 1.6 kΩ in the 0.25 gr variation: 0.75. The X-Ray Diffraction (XRD) test produces α manganese and graphene ranging from 6.8% to 93.2%. The Fourier Transform Infrared (FTIR) test produces Mn-O, CO, and OH bonds. Mn-O with wave numbers 479.44 cm-1, 1.618.35 cm-1, 1.877.47 cm-1, and 992.07 cm-1. CO with wave numbers 1104.27 cm-1, 1190.69 cm-1, and 1384.21 cm-1. OH with wave numbers 1438.44 cm-1 and 1627.70 cm-1 electrical storage medium.","PeriodicalId":8480,"journal":{"name":"Asian Journal of Applied Chemistry Research","volume":"12 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2022-12-31","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Testing of Electrical Properties and Synthesis of MnO2-Graphene Composites from Leaching Results of Manganese Rocks\",\"authors\":\"Asri Saleh\",\"doi\":\"10.9734/ajacr/2022/v13i1-2232\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"This study aims to synthesize and test the electrical properties of the MnO2-graphene composite from the leaching of manganese rock. The test method is carried out by testing the electrical properties with the parameters, namely capacitance (C), current (I), voltage (V), resistance (R), and conductometer. Each tested three concentration variations, 0.25: 0.75, 0.5: 0.05, and 0.75: 0.5. Supporting parameters for testing use X-Ray Diffraction (XRD) and Fourier Transform Infrared (FTIR). The results showed that the effect of varying the mass ratio of the MnO2-Graphene composite on the capacitance value was 192.3ꙡF in the variation of 0.25 gr: 0.75, meaning that the higher the concentration of the graphene carbon ratio, the higher the absorption capacity to store charge and electrical energy. For the variation of the voltage obtained by 353 mV at 0.25 gr: 0.75 variations, the current testing variation obtained a value of 13.6 mA at 0.25 gr: 0.75 variations, the variation on resistance obtained the lowest resistance value of 1.6 kΩ in the 0.25 gr variation: 0.75. The X-Ray Diffraction (XRD) test produces α manganese and graphene ranging from 6.8% to 93.2%. The Fourier Transform Infrared (FTIR) test produces Mn-O, CO, and OH bonds. Mn-O with wave numbers 479.44 cm-1, 1.618.35 cm-1, 1.877.47 cm-1, and 992.07 cm-1. CO with wave numbers 1104.27 cm-1, 1190.69 cm-1, and 1384.21 cm-1. OH with wave numbers 1438.44 cm-1 and 1627.70 cm-1 electrical storage medium.\",\"PeriodicalId\":8480,\"journal\":{\"name\":\"Asian Journal of Applied Chemistry Research\",\"volume\":\"12 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2022-12-31\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Asian Journal of Applied Chemistry Research\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.9734/ajacr/2022/v13i1-2232\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Asian Journal of Applied Chemistry Research","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.9734/ajacr/2022/v13i1-2232","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

本研究旨在合成并测试锰岩浸出的二氧化锰-石墨烯复合材料的电学性能。测试方法是通过测试电性能的参数,即电容(C),电流(I),电压(V),电阻(R)和电导来完成的。每个测试三种浓度变化,0.25:0.75,0.5:0.05和0.75:0.5。辅助测试参数采用x射线衍射(XRD)和傅里叶变换红外(FTIR)。结果表明,在0.25 gr: 0.75的变化范围内,mno2 -石墨烯复合材料的质量比对电容值的影响为192.3ꙡF,这意味着石墨烯碳比浓度越高,其存储电荷和电能的吸收能力越高。对于353 mV在0.25 gr: 0.75变化时得到的电压变化,在0.25 gr: 0.75变化时得到的电流测试变化值为13.6 mA,在0.25 gr: 0.75变化时得到的电阻值最低为1.6 kΩ。x射线衍射(XRD)测试得到α锰和石墨烯含量为6.8% ~ 93.2%。傅里叶变换红外(FTIR)测试产生Mn-O, CO和OH键。Mn-O的波数分别为479.44 cm-1、1.618.35 cm-1、1.877.47 cm-1和992.07 cm-1。CO波数分别为1104.27 cm-1、1190.69 cm-1和1384.21 cm-1。OH具有波数1438.44 cm-1和1627.70 cm-1的电存储介质。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Testing of Electrical Properties and Synthesis of MnO2-Graphene Composites from Leaching Results of Manganese Rocks
This study aims to synthesize and test the electrical properties of the MnO2-graphene composite from the leaching of manganese rock. The test method is carried out by testing the electrical properties with the parameters, namely capacitance (C), current (I), voltage (V), resistance (R), and conductometer. Each tested three concentration variations, 0.25: 0.75, 0.5: 0.05, and 0.75: 0.5. Supporting parameters for testing use X-Ray Diffraction (XRD) and Fourier Transform Infrared (FTIR). The results showed that the effect of varying the mass ratio of the MnO2-Graphene composite on the capacitance value was 192.3ꙡF in the variation of 0.25 gr: 0.75, meaning that the higher the concentration of the graphene carbon ratio, the higher the absorption capacity to store charge and electrical energy. For the variation of the voltage obtained by 353 mV at 0.25 gr: 0.75 variations, the current testing variation obtained a value of 13.6 mA at 0.25 gr: 0.75 variations, the variation on resistance obtained the lowest resistance value of 1.6 kΩ in the 0.25 gr variation: 0.75. The X-Ray Diffraction (XRD) test produces α manganese and graphene ranging from 6.8% to 93.2%. The Fourier Transform Infrared (FTIR) test produces Mn-O, CO, and OH bonds. Mn-O with wave numbers 479.44 cm-1, 1.618.35 cm-1, 1.877.47 cm-1, and 992.07 cm-1. CO with wave numbers 1104.27 cm-1, 1190.69 cm-1, and 1384.21 cm-1. OH with wave numbers 1438.44 cm-1 and 1627.70 cm-1 electrical storage medium.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Synthesis of Novel Perovskite-organic Hybrid Materials for High-efficiency Photovoltaic Devices Study on Micro Structural Properties of Alkali - Doped SiO2 Melt Using Molecular Dynamics Simulation Exploration of Antioxidant, Antibacterial, and Alpha-glucosidase Inhibition Potential of Cirsium verutum (D. Don) Spreng Extracts: In vitro and in silico Approach Biodegradation of Spent Oil in Soil Using Citrullus Colocynthis Peels and Other Plant Wastes Biodegradable Nypa fruticans (Nipa) Starch-PVA Biocomposite Films for Food Packaging
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1