气体爆轰喷涂Fe-Al涂层的摩擦磨损

IF 0.2 Q4 ENGINEERING, GEOLOGICAL Archives for Technical Sciences Pub Date : 2021-11-24 DOI:10.31648/ts.7129
T. Chrostek
{"title":"气体爆轰喷涂Fe-Al涂层的摩擦磨损","authors":"T. Chrostek","doi":"10.31648/ts.7129","DOIUrl":null,"url":null,"abstract":"Comparative tests of gas detonation (GDS) coatings were carried out in order to investigate the influence of spraying parameters on abrasive wear under dry friction conditions. The tests were carried out using the pin-on-disc (PoD) method at room temperature. The microstructure of the coatings was analysed by X-ray diffraction (XRD) and scanning electron microscopy (SEM / EDS) methods. The results showed that with specific GDS process parameters, the main phases in both coatings were FeAl and Fe3Al involving thin oxide films Al2O3. The tribological tests proved that the coatings sprayed with the shorter barrel of the GDS gun showed higher wear resistance. The coefficient of friction was slightly lower in the case of coatings sprayed with the longer barrel of the GDS gun. During dry friction, oxide layers form on the surface, which act as a solid lubricant. The load applied to the samples during the tests causes shear stresses, thus increasing the wear of the coatings. During friction, the surface of the coatings is subjected to alternating tensile and compressive stresses, which lead to delamination and is the main wear mechanism of the coatings.","PeriodicalId":41669,"journal":{"name":"Archives for Technical Sciences","volume":null,"pages":null},"PeriodicalIF":0.2000,"publicationDate":"2021-11-24","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":"{\"title\":\"Tribological wear of Fe-Al coatings applied by gas detonation spraying\",\"authors\":\"T. Chrostek\",\"doi\":\"10.31648/ts.7129\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Comparative tests of gas detonation (GDS) coatings were carried out in order to investigate the influence of spraying parameters on abrasive wear under dry friction conditions. The tests were carried out using the pin-on-disc (PoD) method at room temperature. The microstructure of the coatings was analysed by X-ray diffraction (XRD) and scanning electron microscopy (SEM / EDS) methods. The results showed that with specific GDS process parameters, the main phases in both coatings were FeAl and Fe3Al involving thin oxide films Al2O3. The tribological tests proved that the coatings sprayed with the shorter barrel of the GDS gun showed higher wear resistance. The coefficient of friction was slightly lower in the case of coatings sprayed with the longer barrel of the GDS gun. During dry friction, oxide layers form on the surface, which act as a solid lubricant. The load applied to the samples during the tests causes shear stresses, thus increasing the wear of the coatings. During friction, the surface of the coatings is subjected to alternating tensile and compressive stresses, which lead to delamination and is the main wear mechanism of the coatings.\",\"PeriodicalId\":41669,\"journal\":{\"name\":\"Archives for Technical Sciences\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.2000,\"publicationDate\":\"2021-11-24\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"2\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Archives for Technical Sciences\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.31648/ts.7129\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q4\",\"JCRName\":\"ENGINEERING, GEOLOGICAL\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Archives for Technical Sciences","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.31648/ts.7129","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"ENGINEERING, GEOLOGICAL","Score":null,"Total":0}
引用次数: 2

摘要

为研究干摩擦条件下气体爆轰(GDS)涂层的喷涂参数对磨料磨损的影响,进行了气体爆轰涂层的对比试验。试验采用针盘法(PoD)在室温下进行。采用x射线衍射(XRD)和扫描电镜(SEM / EDS)分析了涂层的微观结构。结果表明:在特定的GDS工艺参数下,两种涂层的主要相均为FeAl和Fe3Al,并伴有氧化膜Al2O3;摩擦学试验表明,采用GDS枪管短段喷涂的涂层具有较高的耐磨性。在GDS炮管较长的情况下,涂层的摩擦系数略低。干摩擦时,表面形成氧化层,起到固体润滑剂的作用。在测试过程中,施加在样品上的载荷会产生剪切应力,从而增加涂层的磨损。在摩擦过程中,涂层表面承受拉压交替应力,导致涂层脱层,这是涂层磨损的主要机制。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Tribological wear of Fe-Al coatings applied by gas detonation spraying
Comparative tests of gas detonation (GDS) coatings were carried out in order to investigate the influence of spraying parameters on abrasive wear under dry friction conditions. The tests were carried out using the pin-on-disc (PoD) method at room temperature. The microstructure of the coatings was analysed by X-ray diffraction (XRD) and scanning electron microscopy (SEM / EDS) methods. The results showed that with specific GDS process parameters, the main phases in both coatings were FeAl and Fe3Al involving thin oxide films Al2O3. The tribological tests proved that the coatings sprayed with the shorter barrel of the GDS gun showed higher wear resistance. The coefficient of friction was slightly lower in the case of coatings sprayed with the longer barrel of the GDS gun. During dry friction, oxide layers form on the surface, which act as a solid lubricant. The load applied to the samples during the tests causes shear stresses, thus increasing the wear of the coatings. During friction, the surface of the coatings is subjected to alternating tensile and compressive stresses, which lead to delamination and is the main wear mechanism of the coatings.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Archives for Technical Sciences
Archives for Technical Sciences ENGINEERING, GEOLOGICAL-
自引率
0.00%
发文量
10
期刊最新文献
EFFECTS OF LANDFILL LEACHES ON GROUND AND SURFACE WATERS: A CASE STUDY OF A WILD LANDFILL IN EASTERN BOSNIA AND HERZEGOVINA ARCHITECTURAL DESIGNING THE NURSING HOMES IN TEHRAN CITY (AS A SAMPLE) ANALYSIS OF OCCUPATIONAL INJURIES IN AN IRON ORE MINE IN BOSNIA AND HERZEGOVINA IN THE PERIOD FROM 2002 TO 2021 LIQUEFACTION-INDUCED DAMAGE IN THE CITIES OF ISKENDERUN AND GOLBASI AFTER THE 2023 TURKEY EARTHQUAKE IDENTIFICATION AND ANALYSIS OF RISKS IN CIVIL ENGINEERING PROJECTS
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1