基于耗散能测量的疲劳裂纹起裂位置估计

A. Akai, K. Inaba, D. Shiozawa, T. Sakagami
{"title":"基于耗散能测量的疲劳裂纹起裂位置估计","authors":"A. Akai, K. Inaba, D. Shiozawa, T. Sakagami","doi":"10.2472/JSMS.64.668","DOIUrl":null,"url":null,"abstract":"The evaluation of fatigue limit is important in designing products. The fatigue limit estimation based on dissipated energy has been getting considerable attentions. In this method, the temperature change due to irreversible energy dissipation is measured by infrared thermography for various levels of stress amplitude. It is known that the dissipated energy increases with increasing stress levels, and a certain stress level, where the change in dissipated energy shows the sharp increase, coincides with the fatigue limit of the material. In this study, the dissipated energy measurement was applied to the estimation of the crack initiation location. The fatigue limit estimation was carried out for the specimen that had multiple notches. The estimated fatigue limit showed similar value at each notch and that gave close agreement with the fatigue limit obtained from conventional fatigue tests. On the other hand, the magnitude and change of dissipated energy at each notch were different. In experiments of fatigue limit estimation, the notch, where the maximum value of dissipated energy was measured, was different from the notch where the maximum sum of principal stress was measured. To investigate the location of the crack initiation, the same specimen was carried out in the constant stress amplitude fatigue test. It was found that the notch where the largest dissipated energy was observed coincided with the crack initiated notch. Therefore, it was considered that the location of crack initiation could be estimated at the early period of fatigue by using the dissipated energy measurement.","PeriodicalId":17366,"journal":{"name":"journal of the Japan Society for Testing Materials","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2015-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"8","resultStr":"{\"title\":\"Estimation of Fatigue Crack Initiation Location Based on Dissipated Energy Measurement\",\"authors\":\"A. Akai, K. Inaba, D. Shiozawa, T. Sakagami\",\"doi\":\"10.2472/JSMS.64.668\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The evaluation of fatigue limit is important in designing products. The fatigue limit estimation based on dissipated energy has been getting considerable attentions. In this method, the temperature change due to irreversible energy dissipation is measured by infrared thermography for various levels of stress amplitude. It is known that the dissipated energy increases with increasing stress levels, and a certain stress level, where the change in dissipated energy shows the sharp increase, coincides with the fatigue limit of the material. In this study, the dissipated energy measurement was applied to the estimation of the crack initiation location. The fatigue limit estimation was carried out for the specimen that had multiple notches. The estimated fatigue limit showed similar value at each notch and that gave close agreement with the fatigue limit obtained from conventional fatigue tests. On the other hand, the magnitude and change of dissipated energy at each notch were different. In experiments of fatigue limit estimation, the notch, where the maximum value of dissipated energy was measured, was different from the notch where the maximum sum of principal stress was measured. To investigate the location of the crack initiation, the same specimen was carried out in the constant stress amplitude fatigue test. It was found that the notch where the largest dissipated energy was observed coincided with the crack initiated notch. Therefore, it was considered that the location of crack initiation could be estimated at the early period of fatigue by using the dissipated energy measurement.\",\"PeriodicalId\":17366,\"journal\":{\"name\":\"journal of the Japan Society for Testing Materials\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2015-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"8\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"journal of the Japan Society for Testing Materials\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.2472/JSMS.64.668\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"journal of the Japan Society for Testing Materials","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.2472/JSMS.64.668","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 8

摘要

疲劳极限评价是产品设计的重要内容。基于耗散能的疲劳极限估计得到了广泛的关注。该方法利用红外热像仪测量不同应力幅值下不可逆能量耗散引起的温度变化。可知,耗散能随应力水平的增加而增大,在某一应力水平上耗散能变化急剧增大,与材料的疲劳极限相吻合。本研究将耗散能测量方法应用于裂纹起裂位置的估计。对具有多个缺口的试样进行了疲劳极限估计。估计的疲劳极限在每个缺口处显示出相似的值,与常规疲劳试验得到的疲劳极限接近。另一方面,各缺口处耗散能的大小和变化是不同的。在疲劳极限估计实验中,测量耗散能最大值的缺口与测量主应力最大值的缺口是不同的。为了研究裂纹萌生的位置,对同一试样进行了恒应力幅疲劳试验。结果表明,耗散能量最大的缺口与裂纹起始缺口重合。因此,认为利用耗散能测量可以在疲劳初期估计裂纹起裂位置。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Estimation of Fatigue Crack Initiation Location Based on Dissipated Energy Measurement
The evaluation of fatigue limit is important in designing products. The fatigue limit estimation based on dissipated energy has been getting considerable attentions. In this method, the temperature change due to irreversible energy dissipation is measured by infrared thermography for various levels of stress amplitude. It is known that the dissipated energy increases with increasing stress levels, and a certain stress level, where the change in dissipated energy shows the sharp increase, coincides with the fatigue limit of the material. In this study, the dissipated energy measurement was applied to the estimation of the crack initiation location. The fatigue limit estimation was carried out for the specimen that had multiple notches. The estimated fatigue limit showed similar value at each notch and that gave close agreement with the fatigue limit obtained from conventional fatigue tests. On the other hand, the magnitude and change of dissipated energy at each notch were different. In experiments of fatigue limit estimation, the notch, where the maximum value of dissipated energy was measured, was different from the notch where the maximum sum of principal stress was measured. To investigate the location of the crack initiation, the same specimen was carried out in the constant stress amplitude fatigue test. It was found that the notch where the largest dissipated energy was observed coincided with the crack initiated notch. Therefore, it was considered that the location of crack initiation could be estimated at the early period of fatigue by using the dissipated energy measurement.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Development of In-Situ Iron Powder Mixing Treatment with Air Bubbles Using Deep Mixing Method Revised Design Models for Geogrid Reinforced Soil Walls and LRFD Calibration Quantitative Characterization of the Changes in Surface Topography of Austenitic Stainless Steel under Low Cycle Fatigue Loading Service Life Prediction of an Aged Bridge Based on Carbonation Tests of Cross-Section Cutting-Off Girders 静的強度特性値による機械構造用炭素鋼のS-N 曲線に関する統計的推定
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1