生物陶瓷根管内用药对生物陶瓷根管密封器粘结强度的影响。

IF 2.5 4区 医学 Q2 Dentistry Brazilian Oral Research Pub Date : 2023-01-01 DOI:10.1590/1807-3107bor-2023.vol37.0056
Patrícia Maria Escobar, Alice Corrêa Silva-Sousa, Rafael Verardino de Camargo, Marco Simões-Carvalho, Yara Teresinha Silva-Sousa, Jardel Francisco Mazzi-Chaves, Gustavo DE-Deus, Manoel Damião Sousa-Neto
{"title":"生物陶瓷根管内用药对生物陶瓷根管密封器粘结强度的影响。","authors":"Patrícia Maria Escobar,&nbsp;Alice Corrêa Silva-Sousa,&nbsp;Rafael Verardino de Camargo,&nbsp;Marco Simões-Carvalho,&nbsp;Yara Teresinha Silva-Sousa,&nbsp;Jardel Francisco Mazzi-Chaves,&nbsp;Gustavo DE-Deus,&nbsp;Manoel Damião Sousa-Neto","doi":"10.1590/1807-3107bor-2023.vol37.0056","DOIUrl":null,"url":null,"abstract":"<p><p>To investigate the influence of the remaining volume of a new intracanal medication based on bioceramic compounds on the bond strength (BS) and formation of an adhesive interface between calcium silicate-based and epoxy resin-based root canal sealers. For this purpose, the specimens were distributed according to the intracanal medication (n = 26): Bio-C Temp (BCT) and Ultracal XS (UXS). The roots were scanned in microCT, and after 7 days, the medication was removed. Then a new scan was performed to evaluate the volume of medication remaining. Subsequently, 40 specimens were redistributed into 2 subgroups (n = 10) and filled according to the sealer used: AH Plus (AHP) and Bio-C Sealer (BCS), to assess the bond strength by using the push-out test, and the adhesive interface by confocal laser fluorescence microscopy (CLSM) and scanning electron microscopy (SEM). The t test showed a smaller remainder of BCT (1.77 ± 0.86) compared with UXS (10.47 ± 5.78), irrespective of the root third evaluated. The BS showed that teeth with BCT + BCS had higher bond strength values (3.70 ± 1.22) when compared to the other groups: BCT + AHP (2.15 ± 1.07), UXS + BCS (3.18 ± 1.09) and UXS + AHP (2.11 ± 1.02) (p<0.001). The cervical third had higher BS when compared with the middle and apical thirds (p < 0.001), and higher number of adhesive failures. The adhesive interface in SEM and CLSM images showed better adaptation for the association between BCT + BCS. Intracanal medication and silicate-based endodontic sealer appeared to interact chemically by forming a biomineralizing layer, allowing for an increase in the bond strength and forming an adhesive interface between the materials, with no or less gap formation.</p>","PeriodicalId":48942,"journal":{"name":"Brazilian Oral Research","volume":null,"pages":null},"PeriodicalIF":2.5000,"publicationDate":"2023-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":"{\"title\":\"Influence of bioceramic intracanal medication on the bond strength of bioceramic root canal sealer.\",\"authors\":\"Patrícia Maria Escobar,&nbsp;Alice Corrêa Silva-Sousa,&nbsp;Rafael Verardino de Camargo,&nbsp;Marco Simões-Carvalho,&nbsp;Yara Teresinha Silva-Sousa,&nbsp;Jardel Francisco Mazzi-Chaves,&nbsp;Gustavo DE-Deus,&nbsp;Manoel Damião Sousa-Neto\",\"doi\":\"10.1590/1807-3107bor-2023.vol37.0056\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><p>To investigate the influence of the remaining volume of a new intracanal medication based on bioceramic compounds on the bond strength (BS) and formation of an adhesive interface between calcium silicate-based and epoxy resin-based root canal sealers. For this purpose, the specimens were distributed according to the intracanal medication (n = 26): Bio-C Temp (BCT) and Ultracal XS (UXS). The roots were scanned in microCT, and after 7 days, the medication was removed. Then a new scan was performed to evaluate the volume of medication remaining. Subsequently, 40 specimens were redistributed into 2 subgroups (n = 10) and filled according to the sealer used: AH Plus (AHP) and Bio-C Sealer (BCS), to assess the bond strength by using the push-out test, and the adhesive interface by confocal laser fluorescence microscopy (CLSM) and scanning electron microscopy (SEM). The t test showed a smaller remainder of BCT (1.77 ± 0.86) compared with UXS (10.47 ± 5.78), irrespective of the root third evaluated. The BS showed that teeth with BCT + BCS had higher bond strength values (3.70 ± 1.22) when compared to the other groups: BCT + AHP (2.15 ± 1.07), UXS + BCS (3.18 ± 1.09) and UXS + AHP (2.11 ± 1.02) (p<0.001). The cervical third had higher BS when compared with the middle and apical thirds (p < 0.001), and higher number of adhesive failures. The adhesive interface in SEM and CLSM images showed better adaptation for the association between BCT + BCS. Intracanal medication and silicate-based endodontic sealer appeared to interact chemically by forming a biomineralizing layer, allowing for an increase in the bond strength and forming an adhesive interface between the materials, with no or less gap formation.</p>\",\"PeriodicalId\":48942,\"journal\":{\"name\":\"Brazilian Oral Research\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":2.5000,\"publicationDate\":\"2023-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"1\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Brazilian Oral Research\",\"FirstCategoryId\":\"3\",\"ListUrlMain\":\"https://doi.org/10.1590/1807-3107bor-2023.vol37.0056\",\"RegionNum\":4,\"RegionCategory\":\"医学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q2\",\"JCRName\":\"Dentistry\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Brazilian Oral Research","FirstCategoryId":"3","ListUrlMain":"https://doi.org/10.1590/1807-3107bor-2023.vol37.0056","RegionNum":4,"RegionCategory":"医学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"Dentistry","Score":null,"Total":0}
引用次数: 1

摘要

探讨新型生物陶瓷基根管封闭剂残留量对硅酸钙基根管封闭剂与环氧树脂基根管封闭剂结合强度及界面形成的影响。为此,标本按管内给药方式(n = 26)分发:Bio-C Temp (BCT)和Ultracal XS (UXS)。用微ct扫描牙根,7天后取出药物。然后进行新的扫描以评估剩余的药物量。随后,将40份标本重新分为AH Plus (AHP)和Bio-C sealer (BCS) 2个亚组(n = 10),并根据使用的密封剂进行填充,通过推出试验评估粘接强度,通过共聚焦激光荧光显微镜(CLSM)和扫描电子显微镜(SEM)评估粘接界面。t检验显示,无论评估的根三分之一如何,BCT的剩余量(1.77±0.86)均小于UXS(10.47±5.78)。结果表明,BCT + BCS组牙的结合强度值(3.70±1.22)高于BCT + AHP组(2.15±1.07)、UXS + BCS组(3.18±1.09)、UXS + AHP组(2.11±1.02)
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Influence of bioceramic intracanal medication on the bond strength of bioceramic root canal sealer.

To investigate the influence of the remaining volume of a new intracanal medication based on bioceramic compounds on the bond strength (BS) and formation of an adhesive interface between calcium silicate-based and epoxy resin-based root canal sealers. For this purpose, the specimens were distributed according to the intracanal medication (n = 26): Bio-C Temp (BCT) and Ultracal XS (UXS). The roots were scanned in microCT, and after 7 days, the medication was removed. Then a new scan was performed to evaluate the volume of medication remaining. Subsequently, 40 specimens were redistributed into 2 subgroups (n = 10) and filled according to the sealer used: AH Plus (AHP) and Bio-C Sealer (BCS), to assess the bond strength by using the push-out test, and the adhesive interface by confocal laser fluorescence microscopy (CLSM) and scanning electron microscopy (SEM). The t test showed a smaller remainder of BCT (1.77 ± 0.86) compared with UXS (10.47 ± 5.78), irrespective of the root third evaluated. The BS showed that teeth with BCT + BCS had higher bond strength values (3.70 ± 1.22) when compared to the other groups: BCT + AHP (2.15 ± 1.07), UXS + BCS (3.18 ± 1.09) and UXS + AHP (2.11 ± 1.02) (p<0.001). The cervical third had higher BS when compared with the middle and apical thirds (p < 0.001), and higher number of adhesive failures. The adhesive interface in SEM and CLSM images showed better adaptation for the association between BCT + BCS. Intracanal medication and silicate-based endodontic sealer appeared to interact chemically by forming a biomineralizing layer, allowing for an increase in the bond strength and forming an adhesive interface between the materials, with no or less gap formation.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Brazilian Oral Research
Brazilian Oral Research DENTISTRY, ORAL SURGERY & MEDICINE-
CiteScore
3.70
自引率
4.00%
发文量
107
审稿时长
12 weeks
期刊最新文献
Erratum: Virtual learning object about oral ulcerative lesions: controlled educational intervention study. Braz. Oral Res. 2023:37:e118. Comparative study of sex estimates in adult skulls using direct measurement and tomographic image reconstruction. Braz Oral Res. 2023;37:e064. Association among COVID-19, multisystem inflammatory syndrome in children, and oral health status. Braz Oral Res. 2023;37:e072. Evaluation of peripheral nerve fibers and mast cells in burning mouth syndrome. Erratum: Evaluation of the expression of nerve fiber markers in healthy and inflamed dental pulp. Braz Oral Res. 2023;37:e020.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1