On DIC measurements of DeltaKeff to verify if it is the FCG driving force

Julián Andrés Ortiz González, J. Castro, G. Gonzáles, M. Meggiolaro, J. Freire
{"title":"On DIC measurements of DeltaKeff to verify if it is the FCG driving force","authors":"Julián Andrés Ortiz González, J. Castro, G. Gonzáles, M. Meggiolaro, J. Freire","doi":"10.3221/IGF-ESIS.41.31","DOIUrl":null,"url":null,"abstract":"Redundant data obtained under quasi-constant {DeltaK, Kmax} loading conditions is used to verify if the effective stress intensity factor (SIF) range DeltaKeff DeltaKmax DeltaKop is indeed the fatigue crack driving force. The crack opening SIF Kop is measured along the entire crack path on DC(T) low carbon steel specimens by a series of strain gages bonded along the crack paths, by a strain gage bonded on their back faces, and by a digital image correlation technique. All such measurements showed a significant Kop decrease as the crack sizes increased, while the fatigue crack growth rates remained essentially constant both in the thin and thick specimens, a behavior that cannot be explained by DeltaKeff arguments.","PeriodicalId":300868,"journal":{"name":"Fracture and Structural Integrity","volume":"60 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2017-06-28","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"3","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Fracture and Structural Integrity","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.3221/IGF-ESIS.41.31","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 3

Abstract

Redundant data obtained under quasi-constant {DeltaK, Kmax} loading conditions is used to verify if the effective stress intensity factor (SIF) range DeltaKeff DeltaKmax DeltaKop is indeed the fatigue crack driving force. The crack opening SIF Kop is measured along the entire crack path on DC(T) low carbon steel specimens by a series of strain gages bonded along the crack paths, by a strain gage bonded on their back faces, and by a digital image correlation technique. All such measurements showed a significant Kop decrease as the crack sizes increased, while the fatigue crack growth rates remained essentially constant both in the thin and thick specimens, a behavior that cannot be explained by DeltaKeff arguments.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
对DeltaKeff的DIC测量来验证它是否是FCG的驱动力
利用准常数{DeltaK, Kmax}加载条件下获得的冗余数据,验证有效应力强度因子(SIF)范围DeltaKeff DeltaKmax DeltaKop是否为疲劳裂纹驱动力。在DC(T)低碳钢试件上,采用沿裂纹路径粘接应变片、后表面粘接应变片和数字图像相关技术,沿整个裂纹路径测量试件的裂纹张开SIF Kop。所有这些测量都表明,随着裂纹尺寸的增加,Kop显著降低,而疲劳裂纹扩展速率在薄和厚试样中基本保持不变,这种行为无法用DeltaKeff参数来解释。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Fractography and Tensile studies on the effect of different carbon fillers reinforced hybrid nanocomposites Crack identification in plates-type structures using natural frequencies coupled with successful history-based adaptive differential evolution algorithm Fracture Load Estimations for U-Notched and V-Notched 3D Printed PLA and Graphene-Reinforced PLA plates using the ASED Criterion Notch Sensitivity Study in U-notched Polymers Built by Additive Manufacturing (AM) Behavior of a Multi-Story Steel Structure with Eccentric X-Brace
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1