{"title":"Development of sintered composites of CaSO4 doped with Dy and Nd","authors":"M. A. P. Chagas, L. Parente, D. Souza","doi":"10.1504/AFP.2010.031016","DOIUrl":null,"url":null,"abstract":"The main purpose of this work is the development of sintered composites in order to allow their use as thermoluminescence (TL) dosimeters using a simple route to preparation and employing high temperature. The composites were prepared with CaSO4.2H2O doped with Dy2O3 and NdO3. Initially, CaSO4.2H2O was dehydrated in an oven at 100°C for 1 h. After addition of dopants and homogenisation, Polyvinyl Alcohol (PVA) was incorporated into the compounds to make their compaction easier. The pellets, 6 mm in diameter and 1 mm thick, were sintered at 900°C and 1000°C for 6 h. The TL emission curves showed two peaks when the samples were irradiated with a beta source (90Sr + 90Y). During calibration, TL responses were found to be proportional to the absorbed dose. The results showed that this material can potentially be used in dosimetry.","PeriodicalId":130250,"journal":{"name":"Atoms for Peace: An International Journal","volume":"33 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2010-01-19","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Atoms for Peace: An International Journal","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1504/AFP.2010.031016","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1
Abstract
The main purpose of this work is the development of sintered composites in order to allow their use as thermoluminescence (TL) dosimeters using a simple route to preparation and employing high temperature. The composites were prepared with CaSO4.2H2O doped with Dy2O3 and NdO3. Initially, CaSO4.2H2O was dehydrated in an oven at 100°C for 1 h. After addition of dopants and homogenisation, Polyvinyl Alcohol (PVA) was incorporated into the compounds to make their compaction easier. The pellets, 6 mm in diameter and 1 mm thick, were sintered at 900°C and 1000°C for 6 h. The TL emission curves showed two peaks when the samples were irradiated with a beta source (90Sr + 90Y). During calibration, TL responses were found to be proportional to the absorbed dose. The results showed that this material can potentially be used in dosimetry.