{"title":"PEMANFAATAN LIMBAH KUL IT KAYU (Acacia mangium) SEBAGAI BAHAN BAKU PAPAN PARTIKEL MENGGUNAKAN PEREKAT DAMAR","authors":"Rido Sukmawi","doi":"10.2579/JIIK.V4I1.7338.G6445","DOIUrl":null,"url":null,"abstract":"Acacia Mangium bark waste is an alternative form of raw material that can be used as a raw material in making particle board. Acacia Mangium skin has wood components ranging from 10.5 - 12.1%, while the adhesive used is resin 70% mixed with solar oil 30%. Making particle board with a size of 25 cm x 20 cm x 2 cm with a particle size of 4 mesc with boiling method of raw materials and drying, pressing for 8 hours and conditioning for 20 days. The purpose of this study was to determine the physical and mechanical properties of the particle board, using 3 samples and 3 replications for each test, the data obtained then averaged then the results compared with the characteristics of SNI 03-2105-2006. Based on the results of the research on physical properties, namely density 0.91 gr/cm3, moisture content 11.91%, water absorption 65.12% and development thickness of 16.39% while the mechanical properties are MOE 1.70 104 kgf/cm2 and MOR 27,62 kgf/cm2.","PeriodicalId":270561,"journal":{"name":"JURNAL ILMU-ILMU KEHUTANAN","volume":"95 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2020-03-13","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"JURNAL ILMU-ILMU KEHUTANAN","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.2579/JIIK.V4I1.7338.G6445","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1
Abstract
Acacia Mangium bark waste is an alternative form of raw material that can be used as a raw material in making particle board. Acacia Mangium skin has wood components ranging from 10.5 - 12.1%, while the adhesive used is resin 70% mixed with solar oil 30%. Making particle board with a size of 25 cm x 20 cm x 2 cm with a particle size of 4 mesc with boiling method of raw materials and drying, pressing for 8 hours and conditioning for 20 days. The purpose of this study was to determine the physical and mechanical properties of the particle board, using 3 samples and 3 replications for each test, the data obtained then averaged then the results compared with the characteristics of SNI 03-2105-2006. Based on the results of the research on physical properties, namely density 0.91 gr/cm3, moisture content 11.91%, water absorption 65.12% and development thickness of 16.39% while the mechanical properties are MOE 1.70 104 kgf/cm2 and MOR 27,62 kgf/cm2.