{"title":"Effect of Fe on hydrogenation and dehydrogenation of Sm(CobalFexCu0.053Zr0.02)7.84(x=0.2,0.3,0.4,0.5) alloys","authors":"M. Li, Z. Liu, L. Lei, Z. Xue, S. He, R. Chen, D. Lee, X. Liu, A. Yan","doi":"10.1109/INTMAG.2015.7157027","DOIUrl":null,"url":null,"abstract":"Hydrogen decrepitation as a highly efficient and excellent crushing method is widely used in the preparation of NdFeB magnets. However, this method still exist many difficulties in the industrial preparation for 2:17 type SmCo alloys owing to high hydrogen pressure. Our previous work has reported 2:17 type SmCo alloys occur HD at room temperature and hydrogen pressure of 0.3 MPa and has shown that Fe atom improved hydrogenation decrepitation ability of alloys by improving hydrogen-absorbing ability of 1:7 phase. But the mechanism that Fe improve hydrogen-absorbing ability of the 1:7 phase still need further study. In addition, subsequent degassing behaviour of alloys have been studied by using DSC.","PeriodicalId":381832,"journal":{"name":"2015 IEEE Magnetics Conference (INTERMAG)","volume":"19 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2015-05-11","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"2015 IEEE Magnetics Conference (INTERMAG)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/INTMAG.2015.7157027","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1
Abstract
Hydrogen decrepitation as a highly efficient and excellent crushing method is widely used in the preparation of NdFeB magnets. However, this method still exist many difficulties in the industrial preparation for 2:17 type SmCo alloys owing to high hydrogen pressure. Our previous work has reported 2:17 type SmCo alloys occur HD at room temperature and hydrogen pressure of 0.3 MPa and has shown that Fe atom improved hydrogenation decrepitation ability of alloys by improving hydrogen-absorbing ability of 1:7 phase. But the mechanism that Fe improve hydrogen-absorbing ability of the 1:7 phase still need further study. In addition, subsequent degassing behaviour of alloys have been studied by using DSC.