{"title":"Review of the influence of non-singular higher order terms on the stress field of thin welded lap joints and small inclined cracks in plates","authors":"F. Berto, M. Ayatollahi, S. Vantadori, A. Carpinteri","doi":"10.3221/IGF-ESIS.41.35","DOIUrl":null,"url":null,"abstract":"In stress analysis of cracked plates, alongside the stress intensity factor which quantifies the singular stress component perpendicular to the crack plane, the role played in crack growth by the constant term parallel to the crack plane, called the T-stress, has been widely investigated by many researchers. There are, however, cases of practical interest where the influence on the stress field of the higher order terms in the series expansion for the crack tip stress field, is not negligible. The main aim of the present investigation is to present and apply a set of equations able to describe more accurately the stress components for those cases where the mode I and mode II stress intensity factors used in combination with the T-stress are unable to characterise with sufficient precision the complete stress field ahead the crack tip. The starting point is represented by the Williams’ solution (Williams, 1957) where stresses as expressed in terms of a power series. An example is investigated of a thin-thickness welded lap joint characterized by various joint width to thickness ratios, in the range of d/t ranging from 0.5 to 5. The present paper indicates that the local stresses as well as the strain energy averaged over a control volume which embraces the slip tip, can be evaluated with satisfactory precision only by taking into account a further four terms besides KI, KII and T-stress.","PeriodicalId":300868,"journal":{"name":"Fracture and Structural Integrity","volume":"140 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2017-06-28","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Fracture and Structural Integrity","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.3221/IGF-ESIS.41.35","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1

Abstract

In stress analysis of cracked plates, alongside the stress intensity factor which quantifies the singular stress component perpendicular to the crack plane, the role played in crack growth by the constant term parallel to the crack plane, called the T-stress, has been widely investigated by many researchers. There are, however, cases of practical interest where the influence on the stress field of the higher order terms in the series expansion for the crack tip stress field, is not negligible. The main aim of the present investigation is to present and apply a set of equations able to describe more accurately the stress components for those cases where the mode I and mode II stress intensity factors used in combination with the T-stress are unable to characterise with sufficient precision the complete stress field ahead the crack tip. The starting point is represented by the Williams’ solution (Williams, 1957) where stresses as expressed in terms of a power series. An example is investigated of a thin-thickness welded lap joint characterized by various joint width to thickness ratios, in the range of d/t ranging from 0.5 to 5. The present paper indicates that the local stresses as well as the strain energy averaged over a control volume which embraces the slip tip, can be evaluated with satisfactory precision only by taking into account a further four terms besides KI, KII and T-stress.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
非奇异高阶项对薄焊接搭接接头和板内小斜裂纹应力场影响的综述
在裂纹板的应力分析中,除了量化垂直于裂纹平面的奇异应力分量的应力强度因子外,平行于裂纹平面的常数项t应力在裂纹扩展中的作用也得到了许多研究者的广泛研究。然而,在实际情况下,裂纹尖端应力场级数展开中高阶项对应力场的影响是不可忽略的。本研究的主要目的是提出并应用一组方程,这些方程能够更准确地描述与t应力结合使用的I型和II型应力强度因子无法以足够的精度表征裂纹尖端前面的完整应力场的情况下的应力分量。起点由威廉姆斯解(Williams, 1957)表示,其中应力以幂级数形式表示。研究了一种薄厚焊接搭接接头的实例,该接头具有不同的接头宽度/厚度比,d/t范围为0.5 ~ 5。本文指出,除了KI、KII和t应力外,只有考虑另外四个项,才能以满意的精度计算包含滑移尖端的控制体积上的局部应力和平均应变能。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Fractography and Tensile studies on the effect of different carbon fillers reinforced hybrid nanocomposites Crack identification in plates-type structures using natural frequencies coupled with successful history-based adaptive differential evolution algorithm Fracture Load Estimations for U-Notched and V-Notched 3D Printed PLA and Graphene-Reinforced PLA plates using the ASED Criterion Notch Sensitivity Study in U-notched Polymers Built by Additive Manufacturing (AM) Behavior of a Multi-Story Steel Structure with Eccentric X-Brace
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1