{"title":"ANALISA PENGARUH SUHU PERLAKUAN PANAS TERHADAP PROPERTI MEKANIK KOMPOSIT AL-TIC 3% DENGAN METODE COOLING SLOPE SUDUT KEMIRINGAN 45°","authors":"Farida Ariani, Diky Setiawan Hutabarat","doi":"10.21776/jrm.v14i2.1206","DOIUrl":null,"url":null,"abstract":"On the industrial side, the selection of materials for a product produced by a company must be following the function and purpose of the product. There are many types of materials used by various companies in the manufacture of a product, one of which is aluminium. This study aims to determine the effect of temperature variations of 3% Al-TiC Composite Heat Treatment 350°C, 450°C, 550°C on the mechanical properties and microstructure with the cooling slope method. The casting process is carried out using A356 aluminium material and the addition of 3% titanium carbide (TiC). The casting results are poured into a permanent mould through a cooling slope with a pouring angle of 45°. And finally carried out by heat treatment on the test object with temperature variations of 350°C, 450°C, 550°C with oil cooling media SAE 40. The highest hardness was obtained at a heat treatment temperature of 550°C with a value of 64.25 BHN, at a temperature of 450°C with a value of 60.02 BHN, and 350°C with a value of 56.59 BHN. The highest tensile strength was obtained at a heat treatment temperature of 550°C of 219,862 MPa, a temperature of 450°C of 183,273 MPa, and 350°C of 164,328 MPa. The obtained microstructure shows hypo-eutectic silicon dispersed among the aluminium. The microstructure shows that the homogenization of silicon and TiC at a heat treatment temperature of 550°C is very good, as evidenced by the uniformly dispersed density of the alloy filling the aluminium matrix.","PeriodicalId":167086,"journal":{"name":"Jurnal Rekayasa Mesin","volume":"8 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2023-08-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Jurnal Rekayasa Mesin","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.21776/jrm.v14i2.1206","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
On the industrial side, the selection of materials for a product produced by a company must be following the function and purpose of the product. There are many types of materials used by various companies in the manufacture of a product, one of which is aluminium. This study aims to determine the effect of temperature variations of 3% Al-TiC Composite Heat Treatment 350°C, 450°C, 550°C on the mechanical properties and microstructure with the cooling slope method. The casting process is carried out using A356 aluminium material and the addition of 3% titanium carbide (TiC). The casting results are poured into a permanent mould through a cooling slope with a pouring angle of 45°. And finally carried out by heat treatment on the test object with temperature variations of 350°C, 450°C, 550°C with oil cooling media SAE 40. The highest hardness was obtained at a heat treatment temperature of 550°C with a value of 64.25 BHN, at a temperature of 450°C with a value of 60.02 BHN, and 350°C with a value of 56.59 BHN. The highest tensile strength was obtained at a heat treatment temperature of 550°C of 219,862 MPa, a temperature of 450°C of 183,273 MPa, and 350°C of 164,328 MPa. The obtained microstructure shows hypo-eutectic silicon dispersed among the aluminium. The microstructure shows that the homogenization of silicon and TiC at a heat treatment temperature of 550°C is very good, as evidenced by the uniformly dispersed density of the alloy filling the aluminium matrix.