Optimisation of synthesis parameters for Co-Mo/MgO catalyst yield in MWCNTs production

A. S. Buhari, A. S. Abdulrahman, S. A. Lawal, A. S. Abdulkareem, R. A. Muriana, O. T. Jimoh, H. K. Ibrahim
{"title":"Optimisation of synthesis parameters for Co-Mo/MgO catalyst yield in MWCNTs production","authors":"A. S. Buhari, A. S. Abdulrahman, S. A. Lawal, A. S. Abdulkareem, R. A. Muriana, O. T. Jimoh, H. K. Ibrahim","doi":"10.4314/njtd.v20i2.1409","DOIUrl":null,"url":null,"abstract":"This study examined the impact of synthesis parameter on Cobalt-Molybdenum supported with magnesium oxide (Co-Mo/MgO) catalyst yield in production of multiwall carbon nanotube (MWCNT). Wet impregnation was used to synthesis the Co-Mo/MgO bimetallic catalyst, while a catalytic chemical vapour deposition reactor (CCVD) was used for the synthesis of carbon nanotubes (CNTs). Factorial and central composite design techniques were used to optimise the catalyst and multi-wall carbon nanotubes (MWCNTs). Thermogravimetric analysis/ Differential thermal analysis (TGA/DTA), selected area (electron) diffraction (SAED), X-Ray diffraction analysis (XRD), and Brunauer–Emmett–Teller (BET) were used to characterise the catalyst and MWCNTs that were produced. The Co-Mo/MgO catalyst had an optimal yield of 93.22%, 247.30 m2/g of specific surface area at 120 °C drying temperature, 16 g of mass support, and a 10-hour drying time. The maximum catalyst yield of 40.62% was obtained at calcination temperature of 500 °C and a holding period of 2 hours. The catalyst with the highest degradation temperature of 398.21 °C was observed at 600 °C, when calcined for 4 hours. It was discovered that the surface area of Co-Mo/MgO catalyst from the BET analysis under ideal conditions varied depending on the holding time. The XRD and SAED revealed the growth of CNTs of concentric graphene pattern with the Co-Mo/MgO catalyst.","PeriodicalId":31273,"journal":{"name":"Nigerian Journal of Technological Development","volume":"90 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2023-10-10","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Nigerian Journal of Technological Development","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4314/njtd.v20i2.1409","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"Engineering","Score":null,"Total":0}
引用次数: 0

Abstract

This study examined the impact of synthesis parameter on Cobalt-Molybdenum supported with magnesium oxide (Co-Mo/MgO) catalyst yield in production of multiwall carbon nanotube (MWCNT). Wet impregnation was used to synthesis the Co-Mo/MgO bimetallic catalyst, while a catalytic chemical vapour deposition reactor (CCVD) was used for the synthesis of carbon nanotubes (CNTs). Factorial and central composite design techniques were used to optimise the catalyst and multi-wall carbon nanotubes (MWCNTs). Thermogravimetric analysis/ Differential thermal analysis (TGA/DTA), selected area (electron) diffraction (SAED), X-Ray diffraction analysis (XRD), and Brunauer–Emmett–Teller (BET) were used to characterise the catalyst and MWCNTs that were produced. The Co-Mo/MgO catalyst had an optimal yield of 93.22%, 247.30 m2/g of specific surface area at 120 °C drying temperature, 16 g of mass support, and a 10-hour drying time. The maximum catalyst yield of 40.62% was obtained at calcination temperature of 500 °C and a holding period of 2 hours. The catalyst with the highest degradation temperature of 398.21 °C was observed at 600 °C, when calcined for 4 hours. It was discovered that the surface area of Co-Mo/MgO catalyst from the BET analysis under ideal conditions varied depending on the holding time. The XRD and SAED revealed the growth of CNTs of concentric graphene pattern with the Co-Mo/MgO catalyst.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
MWCNTs生产中Co-Mo/MgO催化剂产率的合成参数优化
研究了多壁碳纳米管(MWCNT)合成工艺参数对Co-Mo/MgO催化剂产率的影响。采用湿浸渍法制备Co-Mo/MgO双金属催化剂,采用催化化学气相沉积反应器(CCVD)法制备碳纳米管。采用因子设计和中心复合设计技术对催化剂和多壁碳纳米管(MWCNTs)进行优化。采用热重分析/差热分析(TGA/DTA)、选择面积(电子)衍射(SAED)、x射线衍射分析(XRD)和brunauer - emmet - teller (BET)对催化剂和制备的MWCNTs进行表征。Co-Mo/MgO催化剂的最佳产率为93.22%,比表面积为247.30 m2/g,干燥温度为120℃,质量载体为16 g,干燥时间为10 h。焙烧温度为500℃,保温时间为2小时,催化剂收率为40.62%。催化剂在600℃下煅烧4小时,最高降解温度为398.21℃。BET分析发现,在理想条件下,Co-Mo/MgO催化剂的表面积随保温时间的变化而变化。XRD和SAED分析结果表明,在Co-Mo/MgO催化剂的作用下,纳米碳管的生长呈同心石墨烯状。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
Nigerian Journal of Technological Development
Nigerian Journal of Technological Development Engineering-Engineering (miscellaneous)
CiteScore
1.00
自引率
0.00%
发文量
40
审稿时长
24 weeks
期刊最新文献
Evaluation of MgO-ZnO-Crab Shell Biofillers as Reinforcement for Biodegradable Polylactic Acid (PLA) Composite Impact of Rice Husk Ash Based-Geopolymer on Some Geotechnical Properties of Selected Residual Tropical Soils ANFIS-based Indoor localization and Tracking in Wireless Sensor Networking Characterization And Impact Of Cutting Parameters On Face-Milled Surfaces Of Pearlitic Ductile Iron Detection and confirmation of electricity thefts in Advanced Metering Infrastructure by Long Short-Term Memory and fuzzy inference system models
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1