Injectable macroporous naturally-derived apatite bone cement as a potential trabecular bone substitute

IF 3.2 4区 医学 Q2 ENGINEERING, BIOMEDICAL Journal of biomedical materials research. Part B, Applied biomaterials Pub Date : 2024-03-08 DOI:10.1002/jbm.b.35397
Vimal Kumar Dewangan, T. S. Sampath Kumar, Mukesh Doble, Viju Daniel Varghese
{"title":"Injectable macroporous naturally-derived apatite bone cement as a potential trabecular bone substitute","authors":"Vimal Kumar Dewangan,&nbsp;T. S. Sampath Kumar,&nbsp;Mukesh Doble,&nbsp;Viju Daniel Varghese","doi":"10.1002/jbm.b.35397","DOIUrl":null,"url":null,"abstract":"<p>In this study, we have formulated a novel apatite bone cements derived from natural sources (i.e. eggshell and fishbone) with improved qualities that is, porosity, resorbability, biological activity, and so forth. The naturally-derived apatite bone cement (i.e. FBDEAp) was prepared by mixing hydroxyapatite (synthesized from fishbone) and tricalcium phosphate (synthesized from eggshell) as a solid phase with a liquid phase (a dilute acidic blend of cement binding accelerator and biopolymers like gelatin and chitosan) with polysorbate (as liquid porogen) to get a desired bone cement paste. The prepared cement paste sets within the clinically acceptable setting time (≤20 min), easily injectable (&gt;85%) through hands and exhibits physiological pH stability (7.3–7.4). The pure apatite phased bone cement was confirmed by x-ray diffraction and Fourier transform infrared spectroscopy analyses. The FBDEAp bone cement possesses acceptable compressive strength (i.e. 5–7 MPa) within trabecular bone range and is resorbable up to 28% in simulated body fluid solution within 12 weeks of incubation at physiological conditions. The FBDEAp is macroporous in nature (average pore size ~50–400 μm) with interconnected pores verified by SEM and micro-CT analyses. The FBDEAp showed significantly increased MG63 cell viability (&gt;125% after 72 h), cell adhesion, proliferation, and key osteogenic genes expression levels (up to 5–13 folds) compared to the synthetically derived, synthetic and eggshell derived as well as synthetic and fishbone derived bone cements. Thus, we strongly believe that our prepared FBDEAp bone cement can be used as potential trabecular bone substitute in orthopedics.</p>","PeriodicalId":15269,"journal":{"name":"Journal of biomedical materials research. Part B, Applied biomaterials","volume":"112 3","pages":""},"PeriodicalIF":3.2000,"publicationDate":"2024-03-08","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of biomedical materials research. Part B, Applied biomaterials","FirstCategoryId":"5","ListUrlMain":"https://onlinelibrary.wiley.com/doi/10.1002/jbm.b.35397","RegionNum":4,"RegionCategory":"医学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"ENGINEERING, BIOMEDICAL","Score":null,"Total":0}
引用次数: 0

Abstract

In this study, we have formulated a novel apatite bone cements derived from natural sources (i.e. eggshell and fishbone) with improved qualities that is, porosity, resorbability, biological activity, and so forth. The naturally-derived apatite bone cement (i.e. FBDEAp) was prepared by mixing hydroxyapatite (synthesized from fishbone) and tricalcium phosphate (synthesized from eggshell) as a solid phase with a liquid phase (a dilute acidic blend of cement binding accelerator and biopolymers like gelatin and chitosan) with polysorbate (as liquid porogen) to get a desired bone cement paste. The prepared cement paste sets within the clinically acceptable setting time (≤20 min), easily injectable (>85%) through hands and exhibits physiological pH stability (7.3–7.4). The pure apatite phased bone cement was confirmed by x-ray diffraction and Fourier transform infrared spectroscopy analyses. The FBDEAp bone cement possesses acceptable compressive strength (i.e. 5–7 MPa) within trabecular bone range and is resorbable up to 28% in simulated body fluid solution within 12 weeks of incubation at physiological conditions. The FBDEAp is macroporous in nature (average pore size ~50–400 μm) with interconnected pores verified by SEM and micro-CT analyses. The FBDEAp showed significantly increased MG63 cell viability (>125% after 72 h), cell adhesion, proliferation, and key osteogenic genes expression levels (up to 5–13 folds) compared to the synthetically derived, synthetic and eggshell derived as well as synthetic and fishbone derived bone cements. Thus, we strongly believe that our prepared FBDEAp bone cement can be used as potential trabecular bone substitute in orthopedics.

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
可注射的大孔天然磷灰石骨水泥作为一种潜在的骨小梁替代物。
在这项研究中,我们配制了一种新型的天然来源(即蛋壳和鱼骨)磷灰石骨水泥,其孔隙率、可吸收性、生物活性等质量均有所提高。天然磷灰石骨水泥(即 FBDEAp)的制备方法是将羟基磷灰石(从鱼骨中合成)和磷酸三钙(从蛋壳中合成)作为固相与液相(骨水泥结合促进剂以及明胶和壳聚糖等生物聚合物的稀酸性混合物)和聚山梨醇酯(作为液体致孔剂)混合,得到所需的骨水泥浆。制备的骨水泥浆在临床可接受的凝固时间(≤20 分钟)内凝固,易于用手注射(>85%),并具有生理 pH 值稳定性(7.3-7.4)。X 射线衍射和傅立叶变换红外光谱分析证实了这种纯磷灰石相骨水泥。FBDEAp 骨水泥在骨小梁范围内具有可接受的抗压强度(即 5-7 兆帕),在生理条件下培养 12 周后,在模拟体液溶液中的吸收率可达 28%。经扫描电子显微镜(SEM)和显微计算机断层扫描(Micro-CT)分析验证,FBDEAp 具有大孔性质(平均孔径约为 50-400 μm),孔与孔之间相互连接。与合成衍生骨水泥、合成和蛋壳衍生骨水泥以及合成和鱼骨衍生骨水泥相比,FBDEAp 在 MG63 细胞存活率(72 小时后大于 125%)、细胞粘附性、增殖性和关键成骨基因表达水平(高达 5-13 倍)方面均有显著提高。因此,我们坚信我们制备的 FBDEAp 骨水泥可作为骨科中潜在的骨小梁替代物。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
CiteScore
7.50
自引率
2.90%
发文量
199
审稿时长
12 months
期刊介绍: Journal of Biomedical Materials Research – Part B: Applied Biomaterials is a highly interdisciplinary peer-reviewed journal serving the needs of biomaterials professionals who design, develop, produce and apply biomaterials and medical devices. It has the common focus of biomaterials applied to the human body and covers all disciplines where medical devices are used. Papers are published on biomaterials related to medical device development and manufacture, degradation in the body, nano- and biomimetic- biomaterials interactions, mechanics of biomaterials, implant retrieval and analysis, tissue-biomaterial surface interactions, wound healing, infection, drug delivery, standards and regulation of devices, animal and pre-clinical studies of biomaterials and medical devices, and tissue-biopolymer-material combination products. Manuscripts are published in one of six formats: • original research reports • short research and development reports • scientific reviews • current concepts articles • special reports • editorials Journal of Biomedical Materials Research – Part B: Applied Biomaterials is an official journal of the Society for Biomaterials, Japanese Society for Biomaterials, the Australasian Society for Biomaterials, and the Korean Society for Biomaterials. Manuscripts from all countries are invited but must be in English. Authors are not required to be members of the affiliated Societies, but members of these societies are encouraged to submit their work to the journal for consideration.
期刊最新文献
An In Vivo Assessment of Different Mesenchymal Stromal Cell Tissue Types and Their Differentiation State on a Shape Memory Polymer Scaffold for Bone Regeneration Degradation and Fatigue Behavior of 3D-Printed Bioresorbable Tracheal Splints Shape Memory Polymer Scaffolds—Utility for In Vitro Osteogenesis of Canine Multipotent Stromal Cells Alternative Anticoagulant Strategy to Improve the Test Sensitivity of ASTM F2888-19 Standard for Platelet and Leukocyte Count Assay Atomic Interaction S. aureus/Machined and Additive Manufacturing Ti-6Al-4V and Ti-35Nb-7Zr-5Ta Disks for Dental Implants
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1