Low energy synthesis of crystalline mesoporous aluminosilicate consisting of Na-P1 zeolite derived from coal fly ash

Md. Saiful Quddus , Mandira Saha , Md. Hasanuzzaman , Nahid Sharmin , Muhammad Shahriar Bashar
{"title":"Low energy synthesis of crystalline mesoporous aluminosilicate consisting of Na-P1 zeolite derived from coal fly ash","authors":"Md. Saiful Quddus ,&nbsp;Mandira Saha ,&nbsp;Md. Hasanuzzaman ,&nbsp;Nahid Sharmin ,&nbsp;Muhammad Shahriar Bashar","doi":"10.1016/j.clema.2024.100247","DOIUrl":null,"url":null,"abstract":"<div><p>Worldwide every year massive amount of coal fly ash is being generated as by product in the power plants which creates economic, environmental and most importantly health problems. Usually coal fly ash is used in cement production worldwide. At present, in Bangladesh, about 95 % of fly ash remains still unutilized. The alkali activation of fly ash has become a top research topic as it is possible to synthesize low cost and ecologically sound mesoporous zeolite type materials. In the present work, to the best of our knowledge, for the first time in Bangladesh, synthesis and characterization of crystalline mesoporous (H3 type hysteresis) aluminosilicate consisting of Na-P1 zeolite with a high BET specific surface area and a high pore volume from coal fly ash based on hydrothermal alkali activation technique have been successfully done. This product has versatile applications like catalysis, gas separation, water softening, water purification, gas sensing etc. The variable of alkali concentration was studied which has the notable influence on the development of the framework of the pores. The untreated coal fly ash (CFA) and the synthesized modified fly ashes (MFAs) were tested by WDS-XRF, XRD, N<sub>2</sub> physisorption, FE-SEM, FT-IR, XPS, EDAX-mapping, particle size analysis and other technologies. The BET specific surface area, total pore volume and average pore diameter of the CFA were only 3 m<sup>2</sup>/g, 0.01 cc/g and 6.3 nm respectively based on nitrogen gas physisorption technique, whereas, after alkali activation at a specific temperature and time, and then curing, significant and promising increased values of the said parameters of 45 m<sup>2</sup>/g, 0.11 cc/g and 9.8 nm were obtained respectively. In methylene blue dye adsorption experiment, MFA showed higher adsorption capacity (23.87 mg/g).</p></div>","PeriodicalId":100254,"journal":{"name":"Cleaner Materials","volume":"12 ","pages":"Article 100247"},"PeriodicalIF":0.0000,"publicationDate":"2024-04-10","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://www.sciencedirect.com/science/article/pii/S2772397624000315/pdfft?md5=76480ff342e06cc77b3fe29b956c4ef6&pid=1-s2.0-S2772397624000315-main.pdf","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Cleaner Materials","FirstCategoryId":"1085","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S2772397624000315","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Worldwide every year massive amount of coal fly ash is being generated as by product in the power plants which creates economic, environmental and most importantly health problems. Usually coal fly ash is used in cement production worldwide. At present, in Bangladesh, about 95 % of fly ash remains still unutilized. The alkali activation of fly ash has become a top research topic as it is possible to synthesize low cost and ecologically sound mesoporous zeolite type materials. In the present work, to the best of our knowledge, for the first time in Bangladesh, synthesis and characterization of crystalline mesoporous (H3 type hysteresis) aluminosilicate consisting of Na-P1 zeolite with a high BET specific surface area and a high pore volume from coal fly ash based on hydrothermal alkali activation technique have been successfully done. This product has versatile applications like catalysis, gas separation, water softening, water purification, gas sensing etc. The variable of alkali concentration was studied which has the notable influence on the development of the framework of the pores. The untreated coal fly ash (CFA) and the synthesized modified fly ashes (MFAs) were tested by WDS-XRF, XRD, N2 physisorption, FE-SEM, FT-IR, XPS, EDAX-mapping, particle size analysis and other technologies. The BET specific surface area, total pore volume and average pore diameter of the CFA were only 3 m2/g, 0.01 cc/g and 6.3 nm respectively based on nitrogen gas physisorption technique, whereas, after alkali activation at a specific temperature and time, and then curing, significant and promising increased values of the said parameters of 45 m2/g, 0.11 cc/g and 9.8 nm were obtained respectively. In methylene blue dye adsorption experiment, MFA showed higher adsorption capacity (23.87 mg/g).

Abstract Image

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
低能合成由煤粉灰提取的 Na-P1 沸石组成的结晶介孔铝硅酸盐
全世界每年都会产生大量的粉煤灰,这些粉煤灰是发电厂的副产品,造成了经济、环境以及最重要的健康问题。粉煤灰通常用于水泥生产。目前,在孟加拉国,约 95% 的粉煤灰仍未得到利用。粉煤灰的碱活化已成为一个热门研究课题,因为它可以合成低成本、无害生态的介孔沸石型材料。据我们所知,本研究首次在孟加拉国成功地利用水热碱活化技术从粉煤灰中合成了具有高 BET 比表面积和高孔隙率的由 Na-P1 沸石组成的结晶介孔(H3 型滞后)铝硅酸盐,并对其进行了表征。该产品具有催化、气体分离、软化水、水净化、气体传感等多种用途。碱浓度对孔隙框架的形成有显著影响。通过 WDS-XRF、XRD、N2 物理吸附、FE-SEM、FT-IR、XPS、EDAX 图谱、粒度分析等技术对未经处理的粉煤灰(CFA)和合成的改性粉煤灰(MFA)进行了测试。根据氮气物理吸附技术,CFA 的 BET 比表面积、总孔体积和平均孔直径分别仅为 3 m2/g、0.01 cc/g 和 6.3 nm,而在特定温度和时间下进行碱活化,然后固化后,上述参数值分别达到 45 m2/g、0.11 cc/g 和 9.8 nm,并有显著提高。在亚甲基蓝染料吸附实验中,MFA 显示出较高的吸附容量(23.87 mg/g)。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
CiteScore
9.20
自引率
0.00%
发文量
0
期刊最新文献
Investigation of the influence of crushed sand on carbonation of Mortar: Physical and microstructural analysis Biodegradable natural polymers and fibers for 3D printing: A holistic perspective on processing, characterization, and advanced applications Experimental study of phase change material (PCM) biochar composite for net-zero built environment applications Research trends on thermochromic asphalt mixtures functionalization: Bibliometric analysis and review Synergistic impact of geopolymer binder and recycled coarse aggregates on the performance of concrete masonry units
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1