{"title":"Comparative study of iodine-doped and undoped pyrrole grafting with plasma on poly (glycerol sebacate) scaffolds and its human dental pulp stem cells compatibility.","authors":"Fernando Hernández-Sánchez, Nayeli Rodríguez-Fuentes, Julio César Sánchez-Pech, Alejandro Ávila-Ortega, Hugo Joel Carrillo-Escalante, William Alejandro Talavera-Pech, Gaspar Eduardo Martín-Pat","doi":"10.1177/08853282241258304","DOIUrl":null,"url":null,"abstract":"<p><p>This study addresses the morphological and chemical characterization of PGS scaffolds after (6, 12, 18, 24, and 30 min) residence in undoped pyrrole plasma (PGS-PPy) and the evaluation of cell viability with human dental pulp stem cells (hDPSCs). The results were compared with a previous study that used iodine-doped pyrrole (PGS-PPy/I). Analyses through SEM and AFM revealed alterations in the topography and quantity of deposited PPy particles. FTIR spectra of PGS-PPy scaffolds confirmed the presence of characteristic absorption peaks of PPy, with higher intensities observed in the nitrile and -C≡C- groups compared to PGS-PPy/I scaffolds, while raman spectra indicated a lower presence of polaron N<sup>+</sup> groups. On the other hand, PGS scaffolds modified with PPy exhibited lower cytotoxicity compared to PGS-PPy/I scaffolds, as evidenced by the Live/Dead assay. Furthermore, the PGS-PPy scaffolds at 6 and 12 min, and particularly the PGS-PPy/I scaffold at 6 min, showed the best results in terms of cell viability by the fifth day of culture. The findings of this study suggest that undoped pyrrole plasma modification for short durations could also be a viable option to enhance the interaction with hDPSCs, especially when the treatment times range between 6 min and 12 min.</p>","PeriodicalId":15138,"journal":{"name":"Journal of Biomaterials Applications","volume":" ","pages":"207-220"},"PeriodicalIF":2.3000,"publicationDate":"2024-09-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Biomaterials Applications","FirstCategoryId":"5","ListUrlMain":"https://doi.org/10.1177/08853282241258304","RegionNum":4,"RegionCategory":"医学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"2024/5/31 0:00:00","PubModel":"Epub","JCR":"Q3","JCRName":"ENGINEERING, BIOMEDICAL","Score":null,"Total":0}
引用次数: 0
Abstract
This study addresses the morphological and chemical characterization of PGS scaffolds after (6, 12, 18, 24, and 30 min) residence in undoped pyrrole plasma (PGS-PPy) and the evaluation of cell viability with human dental pulp stem cells (hDPSCs). The results were compared with a previous study that used iodine-doped pyrrole (PGS-PPy/I). Analyses through SEM and AFM revealed alterations in the topography and quantity of deposited PPy particles. FTIR spectra of PGS-PPy scaffolds confirmed the presence of characteristic absorption peaks of PPy, with higher intensities observed in the nitrile and -C≡C- groups compared to PGS-PPy/I scaffolds, while raman spectra indicated a lower presence of polaron N+ groups. On the other hand, PGS scaffolds modified with PPy exhibited lower cytotoxicity compared to PGS-PPy/I scaffolds, as evidenced by the Live/Dead assay. Furthermore, the PGS-PPy scaffolds at 6 and 12 min, and particularly the PGS-PPy/I scaffold at 6 min, showed the best results in terms of cell viability by the fifth day of culture. The findings of this study suggest that undoped pyrrole plasma modification for short durations could also be a viable option to enhance the interaction with hDPSCs, especially when the treatment times range between 6 min and 12 min.
期刊介绍:
The Journal of Biomaterials Applications is a fully peer reviewed international journal that publishes original research and review articles that emphasize the development, manufacture and clinical applications of biomaterials.
Peer-reviewed articles by biomedical specialists from around the world cover:
New developments in biomaterials, R&D, properties and performance, evaluation and applications
Applications in biomedical materials and devices - from sutures and wound dressings to biosensors and cardiovascular devices
Current findings in biological compatibility/incompatibility of biomaterials
The Journal of Biomaterials Applications publishes original articles that emphasize the development, manufacture and clinical applications of biomaterials. Biomaterials continue to be one of the most rapidly growing areas of research in plastics today and certainly one of the biggest technical challenges, since biomaterial performance is dependent on polymer compatibility with the aggressive biological environment. The Journal cuts across disciplines and focuses on medical research and topics that present the broadest view of practical applications of biomaterials in actual clinical use.
The Journal of Biomaterial Applications is devoted to new and emerging biomaterials technologies, particularly focusing on the many applications which are under development at industrial biomedical and polymer research facilities, as well as the ongoing activities in academic, medical and applied clinical uses of devices.