M. Kerbstadt, K. Ma, E. M. H. White, A. J. Knowles, M. C. Galetz
{"title":"Novel Chromium–Silicon Slurry Coatings for Hot Corrosion Environments","authors":"M. Kerbstadt, K. Ma, E. M. H. White, A. J. Knowles, M. C. Galetz","doi":"10.1007/s11085-024-10257-8","DOIUrl":null,"url":null,"abstract":"<div><p>Ni-based superalloys are commonly used in gas turbines because of their exceptional high-temperature mechanical properties. To secure a long service life, the materials must also have sufficient corrosion resistance. Therefore, diffusion coatings are widely used to enrich the surface in protective oxide scale-forming elements. For temperatures between 650 and 950 °C, where hot corrosion occurs, Cr-based coatings are advantageous. These are commonly applied via the laborious pack cementation process. Recently, a novel cost-effective Cr/Si slurry coating process has been developed which demonstrated resistance to oxidative high-temperature environments. Here, the protection of the slurry coatings against hot corrosion type I at 900 °C on the Ni-based superalloy Rene 80 is investigated and compared to coatings produced by pack cementation. Prior to the 300-h exposures in air containing 0.1% SO<sub>2</sub> at 900 °C, 4 mg/cm<sup>2</sup> of Na<sub>2</sub>SO<sub>4</sub> was deposited on the material surfaces. The uncoated Rene 80 exhibited rapid dissolution of the initial oxide scale followed by catastrophic break away oxidation. In comparison, the slurry coatings showed significantly improved hot corrosion resistance compared to the uncoated alloy and a better protection than a Cr pack cementation coating. The Cr pack cemented Rene 80 showed improved hot corrosion resistance, but Cr depletion in the subsurface zone occurred with increasing exposure time, associated with the propagation of Al internal oxidation and increasing sulfidation. In contrast, the slurry coatings formed an external Cr<sub>2</sub>O<sub>3</sub> scale coupled with an agglomeration of SiO<sub>2</sub> underneath and a continuous Al<sub>2</sub>O<sub>3</sub> subscale which offered a better diffusion barrier and leading to superior long-term protection against hot corrosion.</p></div>","PeriodicalId":724,"journal":{"name":"Oxidation of Metals","volume":"101 5","pages":"1077 - 1089"},"PeriodicalIF":2.1000,"publicationDate":"2024-07-24","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://link.springer.com/content/pdf/10.1007/s11085-024-10257-8.pdf","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Oxidation of Metals","FirstCategoryId":"88","ListUrlMain":"https://link.springer.com/article/10.1007/s11085-024-10257-8","RegionNum":3,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"METALLURGY & METALLURGICAL ENGINEERING","Score":null,"Total":0}
引用次数: 0
Abstract
Ni-based superalloys are commonly used in gas turbines because of their exceptional high-temperature mechanical properties. To secure a long service life, the materials must also have sufficient corrosion resistance. Therefore, diffusion coatings are widely used to enrich the surface in protective oxide scale-forming elements. For temperatures between 650 and 950 °C, where hot corrosion occurs, Cr-based coatings are advantageous. These are commonly applied via the laborious pack cementation process. Recently, a novel cost-effective Cr/Si slurry coating process has been developed which demonstrated resistance to oxidative high-temperature environments. Here, the protection of the slurry coatings against hot corrosion type I at 900 °C on the Ni-based superalloy Rene 80 is investigated and compared to coatings produced by pack cementation. Prior to the 300-h exposures in air containing 0.1% SO2 at 900 °C, 4 mg/cm2 of Na2SO4 was deposited on the material surfaces. The uncoated Rene 80 exhibited rapid dissolution of the initial oxide scale followed by catastrophic break away oxidation. In comparison, the slurry coatings showed significantly improved hot corrosion resistance compared to the uncoated alloy and a better protection than a Cr pack cementation coating. The Cr pack cemented Rene 80 showed improved hot corrosion resistance, but Cr depletion in the subsurface zone occurred with increasing exposure time, associated with the propagation of Al internal oxidation and increasing sulfidation. In contrast, the slurry coatings formed an external Cr2O3 scale coupled with an agglomeration of SiO2 underneath and a continuous Al2O3 subscale which offered a better diffusion barrier and leading to superior long-term protection against hot corrosion.
期刊介绍:
Oxidation of Metals is the premier source for the rapid dissemination of current research on all aspects of the science of gas-solid reactions at temperatures greater than about 400˚C, with primary focus on the high-temperature corrosion of bulk and coated systems. This authoritative bi-monthly publishes original scientific papers on kinetics, mechanisms, studies of scales from structural and morphological viewpoints, transport properties in scales, phase-boundary reactions, and much more. Articles may discuss both theoretical and experimental work related to gas-solid reactions at the surface or near-surface of a material exposed to elevated temperatures, including reactions with oxygen, nitrogen, sulfur, carbon and halogens. In addition, Oxidation of Metals publishes the results of frontier research concerned with deposit-induced attack. Review papers and short technical notes are encouraged.