{"title":"Friction Stir Welding of Thick Steel Plate Using Silicon Nitride Tool","authors":"Masakazu Mori, Tatsuya Ban, Hiroki Takeuchi, Yoshiaki Morisada, Hidetoshi Fujii","doi":"10.2355/isijinternational.isijint-2024-172","DOIUrl":null,"url":null,"abstract":"</p><p>Friction stir welding (FSW) is expected to be applied as a welding technique of materials with relatively high melting temperature such as steel materials. Silicon nitride is one of the inexpensive and attractive tool materials for FSW of the thick steel plate. Therefore, in this study, the capability of the silicon nitride tool without groove scroll to weld a low carbon steel plate with a thickness of 15 mm was investigated. The suitability of a tool shape was confirmed by FSW of a thick A5052 plate using a SKD61 tool with same shape as the silicon nitride tool. The defect-free welded specimen of the thick steel plate was obtained using the silicon nitride tool under the optimum welding condition. The silicon nitride tool could be used for FSW of the 15 mm thick steel plate until the welding length of 200 mm without breaking the tool. The groove defect area in the stir zone of the thick steel plate was decreased with decreasing of the tool rotation speed and tool tilt angle. Especially, the tool tilt angle was effective to increase the heat input and the material flow velocity. It is considered that the defect-free weld specimen of the thick steel plate was obtained to sufficient material supply to the RS of the stir zone by decreasing tool tilt angle to 1°.</p>\n<p></p>\n<img alt=\"\" src=\"https://www.jstage.jst.go.jp/pub/isijinternational/64/11/64_ISIJINT-2024-172/figure/64_ISIJINT-2024-172.jpg\"/>\n<span style=\"padding-left:5px;\">Fullsize Image</span>","PeriodicalId":14619,"journal":{"name":"Isij International","volume":null,"pages":null},"PeriodicalIF":1.6000,"publicationDate":"2024-09-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Isij International","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.2355/isijinternational.isijint-2024-172","RegionNum":4,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"METALLURGY & METALLURGICAL ENGINEERING","Score":null,"Total":0}
引用次数: 0

Abstract

Friction stir welding (FSW) is expected to be applied as a welding technique of materials with relatively high melting temperature such as steel materials. Silicon nitride is one of the inexpensive and attractive tool materials for FSW of the thick steel plate. Therefore, in this study, the capability of the silicon nitride tool without groove scroll to weld a low carbon steel plate with a thickness of 15 mm was investigated. The suitability of a tool shape was confirmed by FSW of a thick A5052 plate using a SKD61 tool with same shape as the silicon nitride tool. The defect-free welded specimen of the thick steel plate was obtained using the silicon nitride tool under the optimum welding condition. The silicon nitride tool could be used for FSW of the 15 mm thick steel plate until the welding length of 200 mm without breaking the tool. The groove defect area in the stir zone of the thick steel plate was decreased with decreasing of the tool rotation speed and tool tilt angle. Especially, the tool tilt angle was effective to increase the heat input and the material flow velocity. It is considered that the defect-free weld specimen of the thick steel plate was obtained to sufficient material supply to the RS of the stir zone by decreasing tool tilt angle to 1°.

Abstract Image Fullsize Image
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
使用氮化硅工具搅拌摩擦焊接厚钢板
搅拌摩擦焊(FSW)有望成为钢材等熔化温度相对较高材料的焊接技术。氮化硅是用于厚钢板 FSW 的廉价且有吸引力的工具材料之一。因此,在本研究中,研究了无滚槽氮化硅工具焊接厚度为 15 毫米的低碳钢板的能力。通过使用与氮化硅工具形状相同的 SKD61 工具对 A5052 厚钢板进行 FSW,确认了工具形状的适用性。在最佳焊接条件下,使用氮化硅工具获得了无缺陷的厚钢板焊接试样。氮化硅工具可用于 15 毫米厚钢板的 FSW,直到焊接长度达到 200 毫米而不会损坏工具。厚钢板搅拌区的沟槽缺陷面积随着工具转速和工具倾斜角度的降低而减小。尤其是工具倾斜角度对增加热输入和材料流动速度非常有效。我们认为,将工具倾斜角度减小到 1°,可为搅拌区 RS 提供充足的材料,从而获得无缺陷的厚钢板焊接试样。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
Isij International
Isij International 工程技术-冶金工程
CiteScore
3.40
自引率
16.70%
发文量
268
审稿时长
2.6 months
期刊介绍: The journal provides an international medium for the publication of fundamental and technological aspects of the properties, structure, characterization and modeling, processing, fabrication, and environmental issues of iron and steel, along with related engineering materials.
期刊最新文献
Ductility loss of a metastable austenitic stainless steel and its TIG weldment due to hydrogen embrittlement at low temperatures considering the effect of pre-strain at 4K Iterative Convergence for Solving the Exit Plastic Zone and Friction Coefficient Model of Ultra-thin Strip Rolling Force Ductile Fracture Prediction During Metal Forming Using an Ellipsoidal Void Model and Some Other Models Atmospheric Corrosion Behavior of Ni-Advanced Weathering Steels in High-Chloride Environment: Effect of Ni on Corrosion Morphology Arc-plasma-assisted laser-induced breakdown spectroscopy (AP-LIBS): A Study on Signal Enhancement and Spatiotemporal Distribution
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1