Evaluation of the optical and surface properties of monolithic CAD-CAM ceramics after simulated tooth-brushing.

Esra Kaynak Öztürk,Seçil Karakoca Nemli,Bilge Turhan Bal,Merve Bankoğlu Güngör
{"title":"Evaluation of the optical and surface properties of monolithic CAD-CAM ceramics after simulated tooth-brushing.","authors":"Esra Kaynak Öztürk,Seçil Karakoca Nemli,Bilge Turhan Bal,Merve Bankoğlu Güngör","doi":"10.1016/j.prosdent.2024.08.010","DOIUrl":null,"url":null,"abstract":"STATEMENT OF PROBLEM\r\nMonolithic computer-aided design and computer-aided manufacturing (CAD-CAM) ceramics have various microstructures, but studies on their optical and surface properties after tooth-brushing are lacking.\r\n\r\nPURPOSE\r\nThe purpose of this in vitro study was to evaluate the changes in the color, gloss, surface roughness, and surface topography of different monolithic CAD-CAM ceramics after simulated tooth-brushing and compare the tested parameters of the different ceramics.\r\n\r\nMATERIAL AND METHODS\r\nNinety specimens were prepared with a 1.5-mm thickness from 9 different materials: monolithic zirconia (ZR), lithium disilicate ceramics (precrystallized and crystallized), zirconia reinforced lithium silicate ceramics (precrystallized and crystallized), interpenetrating network ceramic, leucite reinforced ceramic, feldspathic ceramic, and interpenetrating network nanoceramics (n=10). After mechanical polishing, the color parameters, gloss, and surface roughness values of each specimen were measured. Then, the specimens were subjected to 50 000 tooth-brushing cycles. After the brushing simulation, the color change (ΔE00) values were calculated, and the gloss and surface roughness values of the specimens were measured. Data were statistically analyzed with 2-way repeated measures of ANOVA and Bonferroni multiple comparison tests (α=.05).\r\n\r\nRESULTS\r\nThe brushing simulation and ceramic type affected the gloss and surface roughness values of the tested ceramics (P<.001). The surface roughness values of the ceramics increased after 50 000 cycles of simulated brushing. The surface gloss of the ZR group significantly increased after 50 000 cycles of simulated brushing (P<.001). Only the ceramic type affected the color change values (P<.001). The color change value (ΔE00) of ZR was the highest among the tested materials, exceeding the perceptibility threshold after 50 000 cycles, while the ΔE00 of the other materials was lower.\r\n\r\nCONCLUSIONS\r\nSimulated tooth-brushing affected the surface gloss and surface roughness of the tested materials. The ceramic type affected the surface gloss, surface roughness, and color change values. Except for the monolithic zirconia, the color change values were below the perceptibility threshold (0.8) in the experimental groups.","PeriodicalId":501672,"journal":{"name":"The Journal of Prosthetic Dentistry","volume":"29 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2024-09-12","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"The Journal of Prosthetic Dentistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1016/j.prosdent.2024.08.010","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

STATEMENT OF PROBLEM Monolithic computer-aided design and computer-aided manufacturing (CAD-CAM) ceramics have various microstructures, but studies on their optical and surface properties after tooth-brushing are lacking. PURPOSE The purpose of this in vitro study was to evaluate the changes in the color, gloss, surface roughness, and surface topography of different monolithic CAD-CAM ceramics after simulated tooth-brushing and compare the tested parameters of the different ceramics. MATERIAL AND METHODS Ninety specimens were prepared with a 1.5-mm thickness from 9 different materials: monolithic zirconia (ZR), lithium disilicate ceramics (precrystallized and crystallized), zirconia reinforced lithium silicate ceramics (precrystallized and crystallized), interpenetrating network ceramic, leucite reinforced ceramic, feldspathic ceramic, and interpenetrating network nanoceramics (n=10). After mechanical polishing, the color parameters, gloss, and surface roughness values of each specimen were measured. Then, the specimens were subjected to 50 000 tooth-brushing cycles. After the brushing simulation, the color change (ΔE00) values were calculated, and the gloss and surface roughness values of the specimens were measured. Data were statistically analyzed with 2-way repeated measures of ANOVA and Bonferroni multiple comparison tests (α=.05). RESULTS The brushing simulation and ceramic type affected the gloss and surface roughness values of the tested ceramics (P<.001). The surface roughness values of the ceramics increased after 50 000 cycles of simulated brushing. The surface gloss of the ZR group significantly increased after 50 000 cycles of simulated brushing (P<.001). Only the ceramic type affected the color change values (P<.001). The color change value (ΔE00) of ZR was the highest among the tested materials, exceeding the perceptibility threshold after 50 000 cycles, while the ΔE00 of the other materials was lower. CONCLUSIONS Simulated tooth-brushing affected the surface gloss and surface roughness of the tested materials. The ceramic type affected the surface gloss, surface roughness, and color change values. Except for the monolithic zirconia, the color change values were below the perceptibility threshold (0.8) in the experimental groups.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
评估模拟刷牙后整体 CAD-CAM 陶瓷的光学和表面特性。
本体外研究的目的是评估不同的整体计算机辅助设计和计算机辅助制造(CAD-CAM)陶瓷在模拟刷牙后颜色、光泽、表面粗糙度和表面形貌的变化,并比较不同陶瓷的测试参数。材料和方法用 9 种不同的材料制备了 90 个厚度为 1.5 毫米的试样:整体氧化锆(ZR)、二硅酸锂陶瓷(预结晶和结晶)、氧化锆增强硅酸锂陶瓷(预结晶和结晶)、互穿网络陶瓷、白榴石增强陶瓷、长石陶瓷和互穿网络纳米陶瓷(n=10)。机械抛光后,测量每个试样的颜色参数、光泽度和表面粗糙度值。然后,对试样进行 50 000 次刷牙循环。模拟刷牙后,计算颜色变化(ΔE00)值,并测量试样的光泽度和表面粗糙度值。结果刷牙模拟和陶瓷类型影响了受测陶瓷的光泽度和表面粗糙度值(P<.001)。陶瓷的表面粗糙度值在模拟刷洗 50 000 次后有所增加。模拟刷洗 50 000 次后,ZR 组的表面光泽度明显增加(P<.001)。只有陶瓷类型会影响颜色变化值(P<.001)。ZR 的变色值(ΔE00)是所有测试材料中最高的,在 50 000 次循环后超过了可感知阈值,而其他材料的ΔE00 则较低。陶瓷类型会影响表面光泽度、表面粗糙度和颜色变化值。除整体氧化锆外,实验组的颜色变化值均低于可感知阈值(0.8)。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Impact of altering the dispensing methods of resin-based cements on their physical and bonding qualities. Factors affecting accuracy in the additive manufacturing of interim dental prostheses: A systematic review. Evaluation of the optical and surface properties of monolithic CAD-CAM ceramics after simulated tooth-brushing. Evaluation of axial displacement and torque loss of Morse-type prosthetic abutments of different angular tapers to their respective implants. Prospective clinical-radiological study of the survival and behavior of short implants.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1