A chemical modification-free strategy for fabricating tough and tear-resistant natural rubber/polysaccharide material

IF 4.1 2区 化学 Q2 POLYMER SCIENCE Polymer Pub Date : 2024-11-26 DOI:10.1016/j.polymer.2024.127880
Shaoqi Huang, Junqi Zhang, Lingmin Kong, Zheng-Tian Xie, Jinrong Wu
{"title":"A chemical modification-free strategy for fabricating tough and tear-resistant natural rubber/polysaccharide material","authors":"Shaoqi Huang,&nbsp;Junqi Zhang,&nbsp;Lingmin Kong,&nbsp;Zheng-Tian Xie,&nbsp;Jinrong Wu","doi":"10.1016/j.polymer.2024.127880","DOIUrl":null,"url":null,"abstract":"<div><div>Natural rubber latex (NRL) is widely used in a variety of products, including gloves, balloons, condoms, and foamed items like pillows and footwear components. However, the limitations of traditional NRL materials in terms of tear resistance and toughness restrict their use in high-end applications. Hence, developing tough and tear-resistant NRL materials using eco-friendly and user-friendly methods remains highly desirable. In this work, a chemical modification-free method is reported for the fabrication of tough and tear-resistant vulcanized natural rubber/carrageenan material (SNR/KC). KC is introduced into NRL via a modified latex mixing strategy, which can form hydrogen bonds with the non-rubber components (NRC) such as proteins on the surface of natural rubber latex particles. As a result, KC can be well dispersed and form a segregated network structure within the rubber matrix. The rigid filler network created by KC effectively impedes crack propagation and enhances energy dissipation during deformation. Furthermore, the presence of KC in the NR matrix fosters the strain-induced crystallization (SIC) of NR. All these contribute to the superior tear resistance and toughness of composite materials. With only 0.1 phr of KC, the composite exhibits a fracture toughness of 208.4 kJ/m<sup>2</sup> and a tear strength of 50 kN/m. This work demonstrated that the interaction between polysaccharide and NRC of NRL can be leveraged to fabricate tough and tear-resistant NR composites without any chemical modification and tedious process, favoring a green development and high-quality pursuit of NRL materials.</div></div>","PeriodicalId":405,"journal":{"name":"Polymer","volume":"316 ","pages":"Article 127880"},"PeriodicalIF":4.1000,"publicationDate":"2024-11-26","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Polymer","FirstCategoryId":"92","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S0032386124012163","RegionNum":2,"RegionCategory":"化学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"POLYMER SCIENCE","Score":null,"Total":0}
引用次数: 0

Abstract

Natural rubber latex (NRL) is widely used in a variety of products, including gloves, balloons, condoms, and foamed items like pillows and footwear components. However, the limitations of traditional NRL materials in terms of tear resistance and toughness restrict their use in high-end applications. Hence, developing tough and tear-resistant NRL materials using eco-friendly and user-friendly methods remains highly desirable. In this work, a chemical modification-free method is reported for the fabrication of tough and tear-resistant vulcanized natural rubber/carrageenan material (SNR/KC). KC is introduced into NRL via a modified latex mixing strategy, which can form hydrogen bonds with the non-rubber components (NRC) such as proteins on the surface of natural rubber latex particles. As a result, KC can be well dispersed and form a segregated network structure within the rubber matrix. The rigid filler network created by KC effectively impedes crack propagation and enhances energy dissipation during deformation. Furthermore, the presence of KC in the NR matrix fosters the strain-induced crystallization (SIC) of NR. All these contribute to the superior tear resistance and toughness of composite materials. With only 0.1 phr of KC, the composite exhibits a fracture toughness of 208.4 kJ/m2 and a tear strength of 50 kN/m. This work demonstrated that the interaction between polysaccharide and NRC of NRL can be leveraged to fabricate tough and tear-resistant NR composites without any chemical modification and tedious process, favoring a green development and high-quality pursuit of NRL materials.

Abstract Image

Abstract Image

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
制造坚韧抗撕裂天然橡胶/多糖材料的无化学改性策略
天然橡胶乳胶(NRL)广泛应用于各种产品,包括手套、气球、避孕套以及枕头和鞋类部件等发泡产品。然而,传统 NRL 材料在抗撕裂性和韧性方面的局限性限制了其在高端应用中的使用。因此,采用环保和用户友好的方法开发坚韧且抗撕裂的 NRL 材料仍然是非常理想的选择。在这项工作中,报告了一种无化学改性的方法,用于制造坚韧且抗撕裂的硫化天然橡胶/卡拉胶材料(SNR/KC)。通过改性胶乳混合策略将 KC 引入 NRL,KC 可与天然胶乳颗粒表面的蛋白质等非橡胶成分(NRC)形成氢键。因此,KC 可以很好地分散,并在橡胶基质中形成隔离的网络结构。KC 形成的刚性填充网络可有效阻碍裂纹扩展,并增强变形过程中的能量消耗。此外,KC 在 NR 基体中的存在还能促进 NR 的应变诱导结晶(SIC)。所有这些都有助于提高复合材料的抗撕裂性和韧性。只需 0.1 phr 的 KC,复合材料就能表现出 208.4 kJ/m2 的断裂韧性和 50 kN/m 的撕裂强度。这项研究表明,利用多糖与 NRL 的 NRC 之间的相互作用,无需任何化学改性和繁琐的工艺,就能制造出坚韧且抗撕裂的 NR 复合材料,有利于 NRL 材料的绿色开发和高品质追求。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
Polymer
Polymer 化学-高分子科学
CiteScore
7.90
自引率
8.70%
发文量
959
审稿时长
32 days
期刊介绍: Polymer is an interdisciplinary journal dedicated to publishing innovative and significant advances in Polymer Physics, Chemistry and Technology. We welcome submissions on polymer hybrids, nanocomposites, characterisation and self-assembly. Polymer also publishes work on the technological application of polymers in energy and optoelectronics. The main scope is covered but not limited to the following core areas: Polymer Materials Nanocomposites and hybrid nanomaterials Polymer blends, films, fibres, networks and porous materials Physical Characterization Characterisation, modelling and simulation* of molecular and materials properties in bulk, solution, and thin films Polymer Engineering Advanced multiscale processing methods Polymer Synthesis, Modification and Self-assembly Including designer polymer architectures, mechanisms and kinetics, and supramolecular polymerization Technological Applications Polymers for energy generation and storage Polymer membranes for separation technology Polymers for opto- and microelectronics.
期刊最新文献
Molecular Orientation and Solvent Affinity in Electrospun Fibers of Miscible Blends Eco-friendly fabrication and luminescent properties of flexible Ag-In-Zn-S/ZnS QD-WPU composite film Superparamagnetic Iron Oxide Nanoparticle – Vitrimer Nanocomposites: Reprocessable and Multi-Responsive Materials Self-healing, high mechanical strength and adhesive supramolecular hydrogel based on triblock copolymer for flexible electronics Emulsion-templated macroporous polycaprolactone: Synthesis, degradation, additive manufacturing, and cell-growth
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1