Fatigue behavior of sintered, glazed and glass-infiltrated surfaces of 5Y-PSZ bonded plates.

IF 1.5 4区 医学 Q3 DENTISTRY, ORAL SURGERY & MEDICINE Brazilian oral research Pub Date : 2024-12-09 eCollection Date: 2024-01-01 DOI:10.1590/1807-3107bor-2024.vol38.0027
Ana Carolina da Silva, Laura Patrícia Nadal Ortiz, Larissa Márcia Martins Alves, Kiara Serafini Dapieve, Tiago Moreira Bastos Campos, Marco Antonio Bottino, Gilmar Patrocínio Thim, Luiz Felipe Valandro, Renata Marques de Melo Marinho
{"title":"Fatigue behavior of sintered, glazed and glass-infiltrated surfaces of 5Y-PSZ bonded plates.","authors":"Ana Carolina da Silva, Laura Patrícia Nadal Ortiz, Larissa Márcia Martins Alves, Kiara Serafini Dapieve, Tiago Moreira Bastos Campos, Marco Antonio Bottino, Gilmar Patrocínio Thim, Luiz Felipe Valandro, Renata Marques de Melo Marinho","doi":"10.1590/1807-3107bor-2024.vol38.0027","DOIUrl":null,"url":null,"abstract":"<p><p>This study evaluated the effect of different occlusal surface finishes (glaze and silica glass infiltration) on surface characteristics and fatigue behavior of partially stabilized zirconia (PSZ) plates adhesively bonded onto epoxy resin discs. PSZ disc specimens (n = 15; Katana blocks STML, Kuraray Noritake Dental) were produced (Ø = 10 mm; thickness = 1.2 mm) and allocated into 3 groups: As sintered (S), silica glass infiltration (SGI), and glaze application (G). The PSZ intaglio surface was air-abraded with 50-µm alumina powder followed by bonding agent application. All produced PSZ were adhesively cemented onto dentin analogue discs made of epoxy resin material (Ø = 10 mm; thickness = 2 mm). Step stress fatigue test was performed (load ranging from 200 to 1800 N; step size 100 N and 10,000 cycles; 20 Hz). The topographic, microstructural, and fractographic analyses were performed by scanning electron microscopy. Results: No statistically significant difference in fatigue behavior was detected among the groups. All failures started at the bonding surface. Silica glass-infiltration and glaze layer application provided a smoothing effect, while the sintered group had a surface with grooves. The occlusal surface finishing method (silica glass infiltration or glazing) had no deleterious effect on fatigue behavior of adhesively bonded PSZ plates.</p>","PeriodicalId":9240,"journal":{"name":"Brazilian oral research","volume":"38 ","pages":"e027"},"PeriodicalIF":1.5000,"publicationDate":"2024-12-09","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://www.ncbi.nlm.nih.gov/pmc/articles/PMC11654874/pdf/","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Brazilian oral research","FirstCategoryId":"3","ListUrlMain":"https://doi.org/10.1590/1807-3107bor-2024.vol38.0027","RegionNum":4,"RegionCategory":"医学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"2024/1/1 0:00:00","PubModel":"eCollection","JCR":"Q3","JCRName":"DENTISTRY, ORAL SURGERY & MEDICINE","Score":null,"Total":0}
引用次数: 0

Abstract

This study evaluated the effect of different occlusal surface finishes (glaze and silica glass infiltration) on surface characteristics and fatigue behavior of partially stabilized zirconia (PSZ) plates adhesively bonded onto epoxy resin discs. PSZ disc specimens (n = 15; Katana blocks STML, Kuraray Noritake Dental) were produced (Ø = 10 mm; thickness = 1.2 mm) and allocated into 3 groups: As sintered (S), silica glass infiltration (SGI), and glaze application (G). The PSZ intaglio surface was air-abraded with 50-µm alumina powder followed by bonding agent application. All produced PSZ were adhesively cemented onto dentin analogue discs made of epoxy resin material (Ø = 10 mm; thickness = 2 mm). Step stress fatigue test was performed (load ranging from 200 to 1800 N; step size 100 N and 10,000 cycles; 20 Hz). The topographic, microstructural, and fractographic analyses were performed by scanning electron microscopy. Results: No statistically significant difference in fatigue behavior was detected among the groups. All failures started at the bonding surface. Silica glass-infiltration and glaze layer application provided a smoothing effect, while the sintered group had a surface with grooves. The occlusal surface finishing method (silica glass infiltration or glazing) had no deleterious effect on fatigue behavior of adhesively bonded PSZ plates.

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
5Y-PSZ粘结板烧结面、釉面和玻璃浸润面疲劳行为
本研究评估了不同的表面处理(釉和硅玻璃渗透)对部分稳定氧化锆(PSZ)板粘接在环氧树脂盘上的表面特性和疲劳行为的影响。PSZ椎间盘标本(n = 15;制作武士刀块STML, Kuraray Noritake Dental) (Ø = 10 mm;厚度= 1.2 mm),分为烧结组(S)、硅玻璃浸润组(SGI)和上釉组(G)。用50µm氧化铝粉对PSZ凹版表面进行空气研磨,然后涂上粘结剂。所有生产的PSZ都粘接在由环氧树脂材料制成的牙本质模拟盘上(Ø = 10 mm;厚度= 2mm)。进行阶梯应力疲劳试验(载荷范围200 ~ 1800 N;步长100n,周期10000次;20 Hz)。通过扫描电子显微镜进行了形貌、显微组织和断口分析。结果:各组疲劳行为差异无统计学意义。所有的故障都是从粘接表面开始的。硅玻璃渗透和釉层的应用提供了平滑效果,而烧结组的表面有凹槽。咬合表面处理方法(硅玻璃浸润或上釉)对粘接PSZ板的疲劳性能无不良影响。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
CiteScore
3.70
自引率
4.00%
发文量
107
审稿时长
12 weeks
期刊最新文献
Principles of radiological protection and application of ALARA, ALADA, and ALADAIP: a critical review. Carbon fiber-reinforced PEEK as a framework material for single implant-retained mandibular overdentures. Aging and post-polymerization effects on conversion degree and properties of additive splint materials. Impact of polyethylene fiber-reinforced composite resin and thermomechanical cycling on dentin bond strength. Occlusion, acid resistance, and elemental characterization of dentin treated with desensitizing agents.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1