{"title":"Crystallography of the litharge to massicot phase transformation from neutron powder diffraction data.","authors":"Roderick J Hill, Lachlan M D Cranswick","doi":"10.1107/S205252062401254X","DOIUrl":null,"url":null,"abstract":"<p><p>The crystallographic phase change from tetragonal litharge (α-PbO; P4/nmm) to orthorhombic massicot (β-PbO; Pbcm) has been studied by full-matrix Rietveld analysis of high-temperature neutron powder diffraction data collected in equal steps from ambient temperature up to 925 K and back down to 350 K. The phase transformation takes place between 850 and 925 K, with the coexisting phases having equal abundance by weight at 885 K. The product massicot remains metastable on cooling to near ambient temperature. Both structures are layered networks of OPb<sub>4</sub> tetrahedra and PbO<sub>4</sub> square pyramids, with the space between alternate layers of Pb atoms (in approximate cubic close packing) occupied either by O atom layers or Pb atom lone pairs. In massicot, the symmetric Pb and O layers of litharge become deeply corrugated parallel to [001], with the O-atom layers splitting into two layers, although these are still sandwiched between the approximately cubic close-packed Pb atom layers. The crystallite size of the initial litharge component decreases from around 3500 Å to around 1100 Å at the midpoint of the phase change at 885 K, whereupon the size of the massicot crystallites increases from a similar value to around 2500 Å at 350 K during the cool-down stage. The unit-cell dimensions and atomic coordinates of litharge change smoothly throughout the phase change, but there is a rapid expansion of the c-axis immediately prior to the recrystallization to massicot, and the one free coordinate (Pb z) decreases significantly to producer a thinning of the layers. Increases in the O displacment parameters suggest that this atom is `on the move' as the transformation approaches. Changes in the massicot parameters as its crystallites emerge from the transformation are largely unremarkable. The formation of the heavily corrugated layers in massicot requires significant movements of the O atoms (∼1.2 Å) from their positions in litharge and thus for Pb-O bonds to be broken during the phase change. The requirement for these bonds to be re-broken in a conversion back to litharge is likely to be the reason why massicot is metastable at ambient temperature. Evidence of a temporary intermediate `amorphous' phase in the phase transformation from which the massicot grows is provided in the form of broad, very low amplitude `peaks' in the high-temperature diffraction patterns.</p>","PeriodicalId":7320,"journal":{"name":"Acta crystallographica Section B, Structural science, crystal engineering and materials","volume":" ","pages":""},"PeriodicalIF":1.3000,"publicationDate":"2025-02-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Acta crystallographica Section B, Structural science, crystal engineering and materials","FirstCategoryId":"92","ListUrlMain":"https://doi.org/10.1107/S205252062401254X","RegionNum":3,"RegionCategory":"化学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"CHEMISTRY, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0

Abstract

The crystallographic phase change from tetragonal litharge (α-PbO; P4/nmm) to orthorhombic massicot (β-PbO; Pbcm) has been studied by full-matrix Rietveld analysis of high-temperature neutron powder diffraction data collected in equal steps from ambient temperature up to 925 K and back down to 350 K. The phase transformation takes place between 850 and 925 K, with the coexisting phases having equal abundance by weight at 885 K. The product massicot remains metastable on cooling to near ambient temperature. Both structures are layered networks of OPb4 tetrahedra and PbO4 square pyramids, with the space between alternate layers of Pb atoms (in approximate cubic close packing) occupied either by O atom layers or Pb atom lone pairs. In massicot, the symmetric Pb and O layers of litharge become deeply corrugated parallel to [001], with the O-atom layers splitting into two layers, although these are still sandwiched between the approximately cubic close-packed Pb atom layers. The crystallite size of the initial litharge component decreases from around 3500 Å to around 1100 Å at the midpoint of the phase change at 885 K, whereupon the size of the massicot crystallites increases from a similar value to around 2500 Å at 350 K during the cool-down stage. The unit-cell dimensions and atomic coordinates of litharge change smoothly throughout the phase change, but there is a rapid expansion of the c-axis immediately prior to the recrystallization to massicot, and the one free coordinate (Pb z) decreases significantly to producer a thinning of the layers. Increases in the O displacment parameters suggest that this atom is `on the move' as the transformation approaches. Changes in the massicot parameters as its crystallites emerge from the transformation are largely unremarkable. The formation of the heavily corrugated layers in massicot requires significant movements of the O atoms (∼1.2 Å) from their positions in litharge and thus for Pb-O bonds to be broken during the phase change. The requirement for these bonds to be re-broken in a conversion back to litharge is likely to be the reason why massicot is metastable at ambient temperature. Evidence of a temporary intermediate `amorphous' phase in the phase transformation from which the massicot grows is provided in the form of broad, very low amplitude `peaks' in the high-temperature diffraction patterns.

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
求助全文
约1分钟内获得全文 去求助
来源期刊
Acta crystallographica Section B, Structural science, crystal engineering and materials
Acta crystallographica Section B, Structural science, crystal engineering and materials CHEMISTRY, MULTIDISCIPLINARYCRYSTALLOGRAPH-CRYSTALLOGRAPHY
CiteScore
3.60
自引率
5.30%
发文量
0
期刊介绍: Acta Crystallographica Section B: Structural Science, Crystal Engineering and Materials publishes scientific articles related to the structural science of compounds and materials in the widest sense. Knowledge of the arrangements of atoms, including their temporal variations and dependencies on temperature and pressure, is often the key to understanding physical and chemical phenomena and is crucial for the design of new materials and supramolecular devices. Acta Crystallographica B is the forum for the publication of such contributions. Scientific developments based on experimental studies as well as those based on theoretical approaches, including crystal-structure prediction, structure-property relations and the use of databases of crystal structures, are published.
期刊最新文献
A rare case of Na/Zn isomorphism in the crystal structure of acentric zincophosphate Na5Zn[Zn(PO4)3]. Selective acceleration and inhibition of crystal growth of glass carbamazepine by low-concentration poly(ethylene oxide):effects of drug polymorph. Structural and magnetic phase transitions in Eu1-xLaxFe3(BO3)4 (x = 0, 0.18). Crystallization induced by fungi and bacteria. Photoelasticity of crystals with the scheelite structure: quantum mechanical calculations.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1