The essential work of fracture in peridynamics

IF 2.2 3区 工程技术 Q3 MATERIALS SCIENCE, MULTIDISCIPLINARY International Journal of Fracture Pub Date : 2023-07-10 DOI:10.1007/s10704-023-00705-y
Christer Stenström, Kjell Eriksson, Florin Bobaru, Stefan Golling, Pär Jonsén
{"title":"The essential work of fracture in peridynamics","authors":"Christer Stenström,&nbsp;Kjell Eriksson,&nbsp;Florin Bobaru,&nbsp;Stefan Golling,&nbsp;Pär Jonsén","doi":"10.1007/s10704-023-00705-y","DOIUrl":null,"url":null,"abstract":"<div><p>In this work, the essential work of fracture (EWF) method is introduced for a peridynamic (PD) material model to characterize fracture toughness of ductile materials. First, an analytical derivation for the path-independence of the PD <i>J</i>-integral is provided. Thereafter, the classical <i>J</i>-integral and PD <i>J</i>-integral are computed on a number of analytical crack problems, for subsequent investigation on how it performs under large scale yielding of thin sheets. To represent a highly nonlinear elastic behavior, a new adaptive bond stiffness calibration and a modified bond-damage model with gradual softening are proposed. The model is employed for two different materials: a lower-ductility bainitic-martensitic steel and a higher-ductility bainitic steel. Up to the start of the softening phase, the PD model recovers the experimentally obtained stress–strain response of both materials. Due to the high failure sensitivity on the presence of defects for the lower-ductility material, the PD model could not recover the experimentally obtained EWF values. For the higher-ductility bainitic material, the PD model was able to match very well the experimentally obtained EWF values. Moreover, the <i>J</i>-integral value obtained from the PD model, at the absolute maximum specimen load, matched the corresponding EWF value.</p></div>","PeriodicalId":590,"journal":{"name":"International Journal of Fracture","volume":"242 2","pages":"129 - 152"},"PeriodicalIF":2.2000,"publicationDate":"2023-07-10","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://link.springer.com/content/pdf/10.1007/s10704-023-00705-y.pdf","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"International Journal of Fracture","FirstCategoryId":"5","ListUrlMain":"https://link.springer.com/article/10.1007/s10704-023-00705-y","RegionNum":3,"RegionCategory":"工程技术","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"MATERIALS SCIENCE, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0

Abstract

In this work, the essential work of fracture (EWF) method is introduced for a peridynamic (PD) material model to characterize fracture toughness of ductile materials. First, an analytical derivation for the path-independence of the PD J-integral is provided. Thereafter, the classical J-integral and PD J-integral are computed on a number of analytical crack problems, for subsequent investigation on how it performs under large scale yielding of thin sheets. To represent a highly nonlinear elastic behavior, a new adaptive bond stiffness calibration and a modified bond-damage model with gradual softening are proposed. The model is employed for two different materials: a lower-ductility bainitic-martensitic steel and a higher-ductility bainitic steel. Up to the start of the softening phase, the PD model recovers the experimentally obtained stress–strain response of both materials. Due to the high failure sensitivity on the presence of defects for the lower-ductility material, the PD model could not recover the experimentally obtained EWF values. For the higher-ductility bainitic material, the PD model was able to match very well the experimentally obtained EWF values. Moreover, the J-integral value obtained from the PD model, at the absolute maximum specimen load, matched the corresponding EWF value.

Abstract Image

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
周动力学中断裂的基本工作
本文介绍了一种用于表征延性材料断裂韧性的周动力(PD)材料模型的断裂基本工作(EWF)方法。首先,给出了PD - j积分路径无关性的解析推导。在此基础上,计算了若干解析裂纹问题的经典j积分和PD j积分,研究了其在薄板大规模屈服条件下的表现。为了表示高度非线性的弹性行为,提出了一种新的自适应粘结刚度标定方法和一种改进的逐渐软化粘结损伤模型。该模型适用于两种不同的材料:低延展性贝氏体-马氏体钢和高延展性贝氏体钢。直到软化阶段开始,PD模型恢复了实验得到的两种材料的应力应变响应。由于低延性材料对缺陷存在的破坏敏感性高,PD模型无法恢复实验得到的EWF值。对于高延展性贝氏体材料,PD模型能很好地匹配实验得到的EWF值。PD模型得到的j积分值在绝对最大试件荷载下与相应的EWF值相匹配。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
International Journal of Fracture
International Journal of Fracture 物理-材料科学:综合
CiteScore
4.80
自引率
8.00%
发文量
74
审稿时长
13.5 months
期刊介绍: The International Journal of Fracture is an outlet for original analytical, numerical and experimental contributions which provide improved understanding of the mechanisms of micro and macro fracture in all materials, and their engineering implications. The Journal is pleased to receive papers from engineers and scientists working in various aspects of fracture. Contributions emphasizing empirical correlations, unanalyzed experimental results or routine numerical computations, while representing important necessary aspects of certain fatigue, strength, and fracture analyses, will normally be discouraged; occasional review papers in these as well as other areas are welcomed. Innovative and in-depth engineering applications of fracture theory are also encouraged. In addition, the Journal welcomes, for rapid publication, Brief Notes in Fracture and Micromechanics which serve the Journal''s Objective. Brief Notes include: Brief presentation of a new idea, concept or method; new experimental observations or methods of significance; short notes of quality that do not amount to full length papers; discussion of previously published work in the Journal, and Brief Notes Errata.
期刊最新文献
Wave interactions and fracture evolution in a thin glass plate under impact: a combined experimental and peridynamic analysis Size-dependency and lattice-discreetness effect on fracture toughness in 2D crystals under antiplanar loading Crack propagation behavior in the stacked \({{\varvec{TaC}}}\)–\({{\varvec{Gr}}}\) core–shell composites The study on the high cycle fatigue performance and life prediction of Ti–6Al–4V alloy fabricated by laser engineered net shaping 3D characterization of kinematic fields and poroelastic swelling near the tip of a propagating crack in a hydrogel
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1