Zhao Changfang, Ren Rui, Wei Yi, Yang Guang, He Bin, Zhang Kebin, Zhong Jianlin
{"title":"Crack Propagation for Glass Fiber Reinforced Laminates Containing Flame Retardant: Based on Single-Edge Tensile Loading","authors":"Zhao Changfang, Ren Rui, Wei Yi, Yang Guang, He Bin, Zhang Kebin, Zhong Jianlin","doi":"10.37358/mp.22.2.5588","DOIUrl":null,"url":null,"abstract":"\nResearch on crack propagation for fiber reinforced composites containing flame retardant is rare. The micro-cracks propagation is a reason for delamination and debonding failure of fiber reinforced composites. To study the crack propagation of continuous glass fiber reinforced epoxy resin laminates that contained ammonium polyphosphate flame retardant (GFRP-APP), the quasi-static single-edge tensile loading (SETL) experiments for the end-notched GFRP-APP specimens were carried out by MTS universal electronic testing machine. The crack propagation of the end-notched 90� GFRP-APP specimen includes two types, both of which belong to opening type (mode I). Namely, one type is mode I multi-cracks propagation without preexisting crack, and the other is mode I fiber bridge propagation with preexisting crack. The intralaminar fracture toughness along fiber direction of GFRP-APP is approximately 8.4 N/mm, which is calculated by area method. The opening displacement-tensile force curves can be divided into three stages for 90� GFRP-APP specimen without crack, i.e., crack gestation, crack birth and crack propagation. However, the 90� GFRP-APP specimen with crack not contains the crack birth stage. Additionally, the microscopic morphology for the fracture face of pure epoxy resin and GFRP-APP, and the phase analysis for GFRP-APP were performed by scanning electron microscope (SEM), X-ray diffraction (XRD) and energy dispersive spectrometer (EDS). As a conclusion, the pores and interfaces in materials were the guiding factors of micro-crack propagation, and the ammonium polyphosphate flame retardant particle contributed extra interfaces.\n","PeriodicalId":18360,"journal":{"name":"Materiale Plastice","volume":" ","pages":""},"PeriodicalIF":0.6000,"publicationDate":"2022-07-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Materiale Plastice","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.37358/mp.22.2.5588","RegionNum":4,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"MATERIALS SCIENCE, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 2
Abstract
Research on crack propagation for fiber reinforced composites containing flame retardant is rare. The micro-cracks propagation is a reason for delamination and debonding failure of fiber reinforced composites. To study the crack propagation of continuous glass fiber reinforced epoxy resin laminates that contained ammonium polyphosphate flame retardant (GFRP-APP), the quasi-static single-edge tensile loading (SETL) experiments for the end-notched GFRP-APP specimens were carried out by MTS universal electronic testing machine. The crack propagation of the end-notched 90� GFRP-APP specimen includes two types, both of which belong to opening type (mode I). Namely, one type is mode I multi-cracks propagation without preexisting crack, and the other is mode I fiber bridge propagation with preexisting crack. The intralaminar fracture toughness along fiber direction of GFRP-APP is approximately 8.4 N/mm, which is calculated by area method. The opening displacement-tensile force curves can be divided into three stages for 90� GFRP-APP specimen without crack, i.e., crack gestation, crack birth and crack propagation. However, the 90� GFRP-APP specimen with crack not contains the crack birth stage. Additionally, the microscopic morphology for the fracture face of pure epoxy resin and GFRP-APP, and the phase analysis for GFRP-APP were performed by scanning electron microscope (SEM), X-ray diffraction (XRD) and energy dispersive spectrometer (EDS). As a conclusion, the pores and interfaces in materials were the guiding factors of micro-crack propagation, and the ammonium polyphosphate flame retardant particle contributed extra interfaces.
期刊介绍:
Materiale Plastice, abbreviated as Mater. Plast., publishes original scientific papers or guest reviews on topics of great interest.
The Journal does not publish memos, technical reports or non-original papers (that are a compiling of literature data) or papers that have been already published in other national or foreign Journal.