{"title":"Use fly ash for the production of lightweight building materials","authors":"Lan Tran Thi, Duong Nguyen Anh, Anh Phan Luu, Man Tran Thi","doi":"10.15625/2615-9783/16204","DOIUrl":null,"url":null,"abstract":"Fly ash is a waste byproduct of thermal power plants or steel plants with a low density. Study on using fly ash to produce lightweight construction materials will is a new application of this material resource. Pha Lai fly ash is a byproduct from Pha Lai Thermal Power Joint Stock Company, in which the main mineral component was mullite (15-20%), quartz (14-16%), carbon (5-7%). The content of the amorphous component was about 67-73%. The chemical composition of Pha Lai mainly was SiO2 (51.73%), Al2O3 (23.22%), Fe2O3 (4.23%). To fabricate the lightweight material from Pha Lai fly ash, the fly ash was mixed with additive materials to create binders following two ways: (1) lime + fly ash and (2) geopolymer technology. For the way of lime + fly ash, with the optimal mixture ratio was fly ash:lime: water = 10:2:1, the lightweight material samples had the bulk density of 1.32g/cm3, the compressive strength of 3.91 MPa, satisfied the Vietnamese standard TCVN 6477-2011 for concrete bricks. Applying the geopolymer technology, with the optimal mixture ratio was fly ash: NaOH/Na2SiO3: Al powder = 100:45:0.15, NaOH/Na2SiO3 ratio = 1:2, the lightweight materials obtained the bulk density of 0,62g/cm3, the compressive strength of 1,54 MPa, satisfied the Vietnamese standard TCVN:9029-2017 for Lightweight concrete - Foam concrete and non-autoclaved concrete products-specification.","PeriodicalId":23639,"journal":{"name":"VIETNAM JOURNAL OF EARTH SCIENCES","volume":null,"pages":null},"PeriodicalIF":2.4000,"publicationDate":"2021-06-25","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"VIETNAM JOURNAL OF EARTH SCIENCES","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.15625/2615-9783/16204","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"GEOSCIENCES, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0

Abstract

Fly ash is a waste byproduct of thermal power plants or steel plants with a low density. Study on using fly ash to produce lightweight construction materials will is a new application of this material resource. Pha Lai fly ash is a byproduct from Pha Lai Thermal Power Joint Stock Company, in which the main mineral component was mullite (15-20%), quartz (14-16%), carbon (5-7%). The content of the amorphous component was about 67-73%. The chemical composition of Pha Lai mainly was SiO2 (51.73%), Al2O3 (23.22%), Fe2O3 (4.23%). To fabricate the lightweight material from Pha Lai fly ash, the fly ash was mixed with additive materials to create binders following two ways: (1) lime + fly ash and (2) geopolymer technology. For the way of lime + fly ash, with the optimal mixture ratio was fly ash:lime: water = 10:2:1, the lightweight material samples had the bulk density of 1.32g/cm3, the compressive strength of 3.91 MPa, satisfied the Vietnamese standard TCVN 6477-2011 for concrete bricks. Applying the geopolymer technology, with the optimal mixture ratio was fly ash: NaOH/Na2SiO3: Al powder = 100:45:0.15, NaOH/Na2SiO3 ratio = 1:2, the lightweight materials obtained the bulk density of 0,62g/cm3, the compressive strength of 1,54 MPa, satisfied the Vietnamese standard TCVN:9029-2017 for Lightweight concrete - Foam concrete and non-autoclaved concrete products-specification.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
利用粉煤灰生产轻质建筑材料
粉煤灰是火电厂或钢铁厂的低密度废弃物副产品。利用粉煤灰生产轻质建筑材料的研究将是粉煤灰资源的一种新应用。Pha Lai粉煤灰是Pha Lai热电股份有限公司的副产品,主要矿物成分为莫来石(15-20%)、石英(14-16%)、碳(5-7%)。非晶态成分含量约为67 ~ 73%。Pha Lai的化学成分主要为SiO2(51.73%)、Al2O3(23.22%)、Fe2O3(4.23%)。为了利用Pha Lai粉煤灰制备轻质材料,采用两种方法(1)石灰+粉煤灰和(2)地聚合物技术将粉煤灰与添加剂混合制成粘结剂。采用石灰+粉煤灰的方式,最佳配比为粉煤灰:石灰:水= 10:2:1,轻质材料试样容重为1.32g/cm3,抗压强度为3.91 MPa,满足越南混凝土砖标准TCVN 6477-2011。采用地聚合物技术,最佳配比为粉煤灰:NaOH/Na2SiO3:铝粉= 100:45:15,NaOH/Na2SiO3比= 1:2,轻质材料的堆积密度为0.62 g/cm3,抗压强度为1.54 MPa,满足越南标准TCVN:9029-2017《轻质混凝土-泡沫混凝土和非蒸压混凝土产品-规范》。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
VIETNAM JOURNAL OF EARTH SCIENCES
VIETNAM JOURNAL OF EARTH SCIENCES GEOSCIENCES, MULTIDISCIPLINARY-
CiteScore
3.60
自引率
20.00%
发文量
0
期刊最新文献
Hybrid approach for permeability prediction in porous media: combining FFT simulations with machine learning Identification of the active faults and seismotectonic zonation of Laos territory Multi-step-ahead prediction of water levels using machine learning: A comparative analysis in the Vietnamese Mekong Delta Temporal and spatial variation in water quality in the Son La hydropower Reservoir, Northwestern Vietnam Application of hybrid modeling to predict California bearing ratio of soil
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1