Preparation of New Nano-MnO2 and Its Molybdenum Adsorption in Manganese Sulfate Solution

W. Haifeng, Chen Xiaoliang, Zhao Ping-yuan, Gao Zhaowei, You Xiaoyu, Tian Jiayu, Wang Jiawei
{"title":"Preparation of New Nano-MnO2 and Its Molybdenum Adsorption in Manganese Sulfate Solution","authors":"W. Haifeng, Chen Xiaoliang, Zhao Ping-yuan, Gao Zhaowei, You Xiaoyu, Tian Jiayu, Wang Jiawei","doi":"10.1166/NNL.2020.3210","DOIUrl":null,"url":null,"abstract":"Manganese sulfate solution was in this study oxidized, using H2O2 as oxidant, to obtain new Nano-MnO2 in situ. The characterization of new MnO2 was carried out by XRD, SEM, FT-IR and BET. The effect of new manganese dioxide adsorpting\n molybdenum ion in manganese sulfate solution was also studied. Results showed that the main crystal form of the new MnO2 was γ type, and there was agglomeration of nanospheres with 200∼300 nm diameter from the microscopic morphology, which had abundant surface\n hydroxyl groups, and its specific surface area was as high as 146 m2/g. MnO2 addition was 1.0 g under optimal adsorption conditions when the pH was 2, and the reaction time was 30 min, with removal rate of 99.2% molybdenum and 0.26 ppm residual amount of molybdenum in\n manganese sulfate solution, which met the quality standard for high purity manganese sulfate (HG/T4823-2015) with ≤5 ppm molybdenum content. Moreover, the thermodynamics and kinetics of molybdenum adsorption by new manganese dioxide were also studied. The experiments showed that the adsorption\n process was in accordance with the Freundlich adsorption equation. The adsorption process of molybdenum on manganese dioxide could be described with pseudo second order kinetic model, and the internal diffusion was a controlling link of adsorption rate.","PeriodicalId":18871,"journal":{"name":"Nanoscience and Nanotechnology Letters","volume":"12 1","pages":"1070-1078"},"PeriodicalIF":0.0000,"publicationDate":"2020-09-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"3","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Nanoscience and Nanotechnology Letters","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1166/NNL.2020.3210","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 3

Abstract

Manganese sulfate solution was in this study oxidized, using H2O2 as oxidant, to obtain new Nano-MnO2 in situ. The characterization of new MnO2 was carried out by XRD, SEM, FT-IR and BET. The effect of new manganese dioxide adsorpting molybdenum ion in manganese sulfate solution was also studied. Results showed that the main crystal form of the new MnO2 was γ type, and there was agglomeration of nanospheres with 200∼300 nm diameter from the microscopic morphology, which had abundant surface hydroxyl groups, and its specific surface area was as high as 146 m2/g. MnO2 addition was 1.0 g under optimal adsorption conditions when the pH was 2, and the reaction time was 30 min, with removal rate of 99.2% molybdenum and 0.26 ppm residual amount of molybdenum in manganese sulfate solution, which met the quality standard for high purity manganese sulfate (HG/T4823-2015) with ≤5 ppm molybdenum content. Moreover, the thermodynamics and kinetics of molybdenum adsorption by new manganese dioxide were also studied. The experiments showed that the adsorption process was in accordance with the Freundlich adsorption equation. The adsorption process of molybdenum on manganese dioxide could be described with pseudo second order kinetic model, and the internal diffusion was a controlling link of adsorption rate.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
新型纳米MnO2的制备及其在硫酸锰溶液中对钼的吸附
以H2O2为氧化剂,对硫酸锰溶液进行氧化,原位合成新的纳米MnO2。用XRD、SEM、FT-IR和BET对新型二氧化锰进行了表征,并研究了新型二氧化锰对硫酸锰溶液中钼离子的吸附作用。结果表明,新型MnO2的主要晶型为γ型,从微观形貌上看,存在直径为200~300nm的纳米球团聚现象,具有丰富的表面羟基,其比表面积高达146m2/g。在最佳吸附条件下,当pH为2,反应时间为30min时,MnO2的加入量为1.0g,对硫酸锰溶液中钼的去除率为99.2%,钼残留量为0.26ppm,符合HG/T4823-2015高纯硫酸锰质量标准,钼含量≤5ppm。此外,还研究了新型二氧化锰吸附钼的热力学和动力学。实验表明,吸附过程符合Freundlich吸附方程。钼在二氧化锰上的吸附过程可以用拟二阶动力学模型描述,内扩散是吸附速率的控制环节。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
Nanoscience and Nanotechnology Letters
Nanoscience and Nanotechnology Letters Physical, Chemical & Earth Sciences-MATERIALS SCIENCE, MULTIDISCIPLINARY
自引率
0.00%
发文量
0
审稿时长
2.6 months
期刊最新文献
Identification of Immune-Related Prognostic Biomarkers in Pancreatic Cancer Nanocomposite Detection of Elemental Impurities and Process Correlation Analysis of Ceftriaxone Sodium for Injection Astragalus Polysaccharide Nano-Liposomes Modulate the Inflammatory Response and Oxidative Stress in Stroke-Associated Pneumonia by Increasing OIP5-AS1 to Regulate the miR-128-3p/SIRT1 Pathway miR-199a-3p Inhibitor Delivered Through Nano-Drug Delivery Systems Suppresses Tumor Cell Survival and Metastasis Construction of Functional Renal Targeting Nano Drug Liposome and Its Effect on Lupus Nephritis
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1