R. França, A. Muench, Paulo Eduardo dos Reis Cardoso
{"title":"Resistência de união entre liga de níquel-cromo e cimentos resinosos","authors":"R. França, A. Muench, Paulo Eduardo dos Reis Cardoso","doi":"10.1590/S0103-06631998000300013","DOIUrl":null,"url":null,"abstract":"The purpose of the investigation was to test tensile strength between Ni-Cr alloy and adhesive cements. Variables were: three cements (Comspan, Panavia Ex and All-Bond CB four surface treatments (smooth, sandblasted, electrolytic etching and silicoater); two types of storage (3 and 30 days in NaCl 0.9% solution at 37° C, performing in the latter 600 thermocycles at 5 and 55° C). Specimens were discs obtained through conventional casting procedures and cemented together two by two. Opposite sides of cementing discs were provided with a loop for fixing to the testing equipment. Conclusions were that: smooth surfaces presented very low retentivity and those with silicoater a very high one; Panavia Ex with sandblasting also led to very high retention; highest retention was obtained with the combination silicoater/All-Bond C&B.","PeriodicalId":77611,"journal":{"name":"Revista de odontologia da Universidade de Sao Paulo","volume":"12 1","pages":"267-270"},"PeriodicalIF":0.0000,"publicationDate":"1998-07-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"6","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Revista de odontologia da Universidade de Sao Paulo","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1590/S0103-06631998000300013","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 6
Abstract
The purpose of the investigation was to test tensile strength between Ni-Cr alloy and adhesive cements. Variables were: three cements (Comspan, Panavia Ex and All-Bond CB four surface treatments (smooth, sandblasted, electrolytic etching and silicoater); two types of storage (3 and 30 days in NaCl 0.9% solution at 37° C, performing in the latter 600 thermocycles at 5 and 55° C). Specimens were discs obtained through conventional casting procedures and cemented together two by two. Opposite sides of cementing discs were provided with a loop for fixing to the testing equipment. Conclusions were that: smooth surfaces presented very low retentivity and those with silicoater a very high one; Panavia Ex with sandblasting also led to very high retention; highest retention was obtained with the combination silicoater/All-Bond C&B.