Avaliação da resistência da união metal-resina usando sistemas de retenção mecânico e químico

Luciana Silva Andrade Tarozzo, M. C. T. D. Mattos, Ricardo Faria Ribeiro, Osvaldo Luiz Bezzon, M. Semprini
{"title":"Avaliação da resistência da união metal-resina usando sistemas de retenção mecânico e químico","authors":"Luciana Silva Andrade Tarozzo, M. C. T. D. Mattos, Ricardo Faria Ribeiro, Osvaldo Luiz Bezzon, M. Semprini","doi":"10.1590/S0103-06631999000400006","DOIUrl":null,"url":null,"abstract":"The objective of the present investigation was to evaluate the resistance of metal-resin bonding using the Silicoater® MD system (Kulzer), five types of retention in the metal structure, and three commercial Ni-Cr alloys: Duceranium U, Wiron 99 and Wirocer. A total of 90 samples were submitted to the shearing test. Statistical analysis of the results permitted us to conclude that retention versus alloy interaction was statistically significant at a 1% level of probability, the highest mean value being obtained with the Wirocer alloy with mechanical retention with 0.6 mm spheres. The lowest mean values were observed with the Wiron 99 alloy with chemical retention.","PeriodicalId":77611,"journal":{"name":"Revista de odontologia da Universidade de Sao Paulo","volume":"13 1","pages":"349-355"},"PeriodicalIF":0.0000,"publicationDate":"1999-12-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Revista de odontologia da Universidade de Sao Paulo","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1590/S0103-06631999000400006","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2

Abstract

The objective of the present investigation was to evaluate the resistance of metal-resin bonding using the Silicoater® MD system (Kulzer), five types of retention in the metal structure, and three commercial Ni-Cr alloys: Duceranium U, Wiron 99 and Wirocer. A total of 90 samples were submitted to the shearing test. Statistical analysis of the results permitted us to conclude that retention versus alloy interaction was statistically significant at a 1% level of probability, the highest mean value being obtained with the Wirocer alloy with mechanical retention with 0.6 mm spheres. The lowest mean values were observed with the Wiron 99 alloy with chemical retention.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
使用机械和化学保留系统评估金属树脂结合强度
本研究的目的是利用硅水®MD系统(Kulzer)、金属结构中的五种类型的保留以及三种商用Ni-Cr合金:Duceranium U、Wiron 99和Wirocer来评估金属-树脂结合的阻力。共提交90个试样进行剪切试验。对结果的统计分析使我们得出结论,保留与合金相互作用在1%的概率水平上具有统计显著性,0.6 mm球的wiroser合金的机械保留获得了最高的平均值。具有化学保留的Wiron 99合金的平均值最低。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
"Resisting social identity threat and maintaining resilience": A qualitative study of Chinese parents following the loss of an only child. Study of surface alterations of composite and ionomeric materials submitted to simulation of a high cariogenic challenge Infiltração marginal de agentes cimentantes em coroas metálicas fundidas Efeito da desinfeccao por aerossois sobre a capacidade de umedecimento de moldes de polieter por gesso tipo IV Microinfiltração em dentes decíduos em função de materiais restauradores e condicionamento ácido
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1