{"title":"The difference of corrosion resistance between NiTi archwires and NiTi with additional cooper archwires in artificial saliva","authors":"E. H. Habar, Fransiske Tatengkeng","doi":"10.15562/JDMFS.V5I2.1089","DOIUrl":null,"url":null,"abstract":"Objective: The aim of this experiment showed the difference of corrosion resistance between Nickel-Titanium (NiTi) archwire and NiTi archwire with additional cooper (NiTi-Cu) in artificial saliva. Material and Methods: This research was conducted in these laboratory experiments, immersed the NiTi archwires and NiTi-Cu archwires on artificial saliva at pH= 7 and incubated on 37°C, with the ratio of the archwire and the saliva was 0.02 gr: 1 ml during 1 day, 33 days and 66 days. Results: Corrosion resistances reviewed by average saliva artificial contained ion Ni after immersed 1 day of NiTi archwires and NiTi-Cu were 0.033 ± 0.000, and after immersed 33 days were 0.053 ± 0.022 and 0.101 ± 0.050, and after 66 days immersed were 0.101 ± 0.050","PeriodicalId":31119,"journal":{"name":"Journal of Dentomaxillofacial Science","volume":"9 1","pages":"120"},"PeriodicalIF":0.0000,"publicationDate":"2020-08-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"5","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Dentomaxillofacial Science","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.15562/JDMFS.V5I2.1089","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 5
Abstract
Objective: The aim of this experiment showed the difference of corrosion resistance between Nickel-Titanium (NiTi) archwire and NiTi archwire with additional cooper (NiTi-Cu) in artificial saliva. Material and Methods: This research was conducted in these laboratory experiments, immersed the NiTi archwires and NiTi-Cu archwires on artificial saliva at pH= 7 and incubated on 37°C, with the ratio of the archwire and the saliva was 0.02 gr: 1 ml during 1 day, 33 days and 66 days. Results: Corrosion resistances reviewed by average saliva artificial contained ion Ni after immersed 1 day of NiTi archwires and NiTi-Cu were 0.033 ± 0.000, and after immersed 33 days were 0.053 ± 0.022 and 0.101 ± 0.050, and after 66 days immersed were 0.101 ± 0.050