{"title":"Study of High Purity Cobalt Carbonate Nanocrystals Production by Microemulsion as Batteries Precursors","authors":"Mulaja Tshakatumba Constantin, Tshipeshi Makina Héritier, Ngoy Moïse Raphael Moramess, Mwema Mutamba Edouard","doi":"10.4236/JMMCE.2021.93022","DOIUrl":null,"url":null,"abstract":"The precipitation of cobalt carbonate nanocrystals was achieved through the reaction of a pure and rich solution of cobalt sulphate (Co2+: 16.80 g/l) with a solution of carbonate solution (200 g/l). A surfactant was added to the reacting mixture in order to control the shape and size of generated crystallites. Two parameters were then varied i.e., the weight of surfactant agent and the precipitation time in accordance with Taguchi’s L4 full experimental procedure (22). Chemical and structural characterizations tests of the obtained precipitates were done through X-Rays Fluorescence (XRF), Scanning Electron Microscopy (SEM) and X-Rays Diffractometer (XRD); whereas the size of crystallites was assessed according to the Laue-Scherrer formula. The results obtained from the variance analysis (ANOVA) indicated an optimal size of cobalt carbonate’s crystallites of 13 nm with a cobalt content of 44.35% (equivalent to 89.45% of CoCO3) at ambient temperature under the following conditions: pH = 7; Mixing speed: 800 tr/min; Surfactant weight: 8 g; and a mixing time: 10 minutes. SEM images revealed an agglomeration of the obtained nanocrystals due to suspected drying conditions i.e., drying temperature and drying atmosphere. It is suggested that the experiment should be conducted under neutral conditions at a temperature below that of cobalt carbonate’s decomposition (181.41℃).","PeriodicalId":16488,"journal":{"name":"Journal of Minerals and Materials Characterization and Engineering","volume":"1 1","pages":"316-326"},"PeriodicalIF":0.0000,"publicationDate":"2021-05-12","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Minerals and Materials Characterization and Engineering","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4236/JMMCE.2021.93022","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

The precipitation of cobalt carbonate nanocrystals was achieved through the reaction of a pure and rich solution of cobalt sulphate (Co2+: 16.80 g/l) with a solution of carbonate solution (200 g/l). A surfactant was added to the reacting mixture in order to control the shape and size of generated crystallites. Two parameters were then varied i.e., the weight of surfactant agent and the precipitation time in accordance with Taguchi’s L4 full experimental procedure (22). Chemical and structural characterizations tests of the obtained precipitates were done through X-Rays Fluorescence (XRF), Scanning Electron Microscopy (SEM) and X-Rays Diffractometer (XRD); whereas the size of crystallites was assessed according to the Laue-Scherrer formula. The results obtained from the variance analysis (ANOVA) indicated an optimal size of cobalt carbonate’s crystallites of 13 nm with a cobalt content of 44.35% (equivalent to 89.45% of CoCO3) at ambient temperature under the following conditions: pH = 7; Mixing speed: 800 tr/min; Surfactant weight: 8 g; and a mixing time: 10 minutes. SEM images revealed an agglomeration of the obtained nanocrystals due to suspected drying conditions i.e., drying temperature and drying atmosphere. It is suggested that the experiment should be conducted under neutral conditions at a temperature below that of cobalt carbonate’s decomposition (181.41℃).
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
微乳法制备高纯碳酸钴纳米晶电池前驱体的研究
碳酸钴纳米晶的析出是通过纯富硫酸钴溶液(Co2+: 16.80 g/l)与碳酸钴溶液(200 g/l)的反应实现的。在反应混合物中加入表面活性剂以控制生成晶体的形状和大小。然后改变两个参数,即表面活性剂的重量和沉淀时间,按照田口的L4全实验程序(22)。通过x射线荧光(XRF)、扫描电子显微镜(SEM)和x射线衍射仪(XRD)对所得沉淀物进行了化学和结构表征;而晶体的大小则根据劳-谢勒公式进行评估。方差分析(ANOVA)结果表明,在环境温度下,当钴含量为44.35%(相当于CoCO3的89.45%)时,碳酸钴晶的最佳尺寸为13 nm: pH = 7;搅拌速度:800 tr/min;表面活性剂重量:8g;混合时间:10分钟。扫描电镜图像显示,由于干燥条件,即干燥温度和干燥气氛,所获得的纳米晶体出现团聚。建议在低于碳酸钴分解温度(181.41℃)的中性条件下进行实验。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Synthesis and Characterization of Gadolinium Oxide-Hematite Magnetic Ceramic Nanostructures Physic, Chemical and Mineralogical Characterizations of Clays Used in the Making of Traditional Ceramics in the City of Katiola, C ôte d’Ivoire Appraisal of Engineering Phases of a Mineral Asset: From Exploration to Mine Approval Study on the Attack of Molten Silicates on Plasma-Sprayed Thermal Barrier Coatings Experimental and Numerical Study of Mechanical Behaviour of Fired Clay Bricks after Exposure to High Temperatures
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1