Валерий Петрович Дорожкин, Е. Мохнаткина, Дмитрий Николаевич Земский, Ансар Хаматович Валиев
{"title":"MECHANODESTRUCTION OF ISOPRENE RUBBER. PART 3. KINETICS OF OXIDATIVE DESTRUCTION","authors":"Валерий Петрович Дорожкин, Е. Мохнаткина, Дмитрий Николаевич Земский, Ансар Хаматович Валиев","doi":"10.47664/0022-9466-2021-80-5-230-234","DOIUrl":null,"url":null,"abstract":"Continuation of studies of changes in molecular parameters, in particular, the molecular weight (MM) during the plasticization (P) of SKI-3 isoprene rubber. The kinetics of oxidative destruction (OD) in the temperature range (T) 30-130 °C and time (t) 30–600 s were studied in detail. Plasticization of rubber, as before, was carried out in a laboratory rubber mixer of the company «NFM», and gel chromatographic studies were carried out on a gel chromatograph of the company «Waters». The speed constant OD K0 decreases in absolute value with a decrease in T and an increase in t. The calculated effective activation energy of OD Eeff decreases from 24,4 to 13 kJ/mol in the studied t range. The influence of the oxygen diffusion process on the kinetic features of the OD of SKI-3 at Р is pointed out.","PeriodicalId":17907,"journal":{"name":"Kauchuk i Rezina","volume":"45 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2021-10-20","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Kauchuk i Rezina","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.47664/0022-9466-2021-80-5-230-234","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
Continuation of studies of changes in molecular parameters, in particular, the molecular weight (MM) during the plasticization (P) of SKI-3 isoprene rubber. The kinetics of oxidative destruction (OD) in the temperature range (T) 30-130 °C and time (t) 30–600 s were studied in detail. Plasticization of rubber, as before, was carried out in a laboratory rubber mixer of the company «NFM», and gel chromatographic studies were carried out on a gel chromatograph of the company «Waters». The speed constant OD K0 decreases in absolute value with a decrease in T and an increase in t. The calculated effective activation energy of OD Eeff decreases from 24,4 to 13 kJ/mol in the studied t range. The influence of the oxygen diffusion process on the kinetic features of the OD of SKI-3 at Р is pointed out.