An Easy Way for Ceramic Bricks Elaboration to Carry out Basic Technical Measurements

Hicham Elidrissi, Wafaa Borja, L. Daoudi, N. Fagel, R. Hakkou, Y. Taha, Y. Tamraoui
{"title":"An Easy Way for Ceramic Bricks Elaboration to Carry out Basic Technical Measurements","authors":"Hicham Elidrissi, Wafaa Borja, L. Daoudi, N. Fagel, R. Hakkou, Y. Taha, Y. Tamraoui","doi":"10.4028/p-e218c0","DOIUrl":null,"url":null,"abstract":"Fired bricks have shown tremendous potential as a construction material due to their properties. However, their use required some specifications in terms of quality, resistance, and durability. In developing countries, the lack of tools to make test specimens leads to many defects in these brick specimens responsible for low durability and weak precision during mechanical tests and shrinkage. In this study, a simple and traditional method of making test bricks is presented. This simple method allows the production of bricks with the required properties. This method is especially efficient for semi-soft consistency pastes. The elaborated handmade pastes present a very different particle-size distribution < 2 mm (clay: 18-66%; silt: 12-53%; sand: 5-65%). The pastes do not stick to the walls of the mould like in the case of steel moulds, and it gives specimens with standard shape, smooth surface, and sharp edges. The resulting fired bricks exhibit high mechanical strength (up to 102 MPa for the compressive strength, and up to 28 MPa for the flexural strength) comparable to and even better than those of conventional methods. The elaborated bricks allowed also the measurement of very important parameters such as drying and firing shrinkage, drying, and firing weight loss, and porosity.","PeriodicalId":7271,"journal":{"name":"Advanced Materials Research","volume":"101 1","pages":"3 - 14"},"PeriodicalIF":0.0000,"publicationDate":"2022-09-26","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Advanced Materials Research","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4028/p-e218c0","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Fired bricks have shown tremendous potential as a construction material due to their properties. However, their use required some specifications in terms of quality, resistance, and durability. In developing countries, the lack of tools to make test specimens leads to many defects in these brick specimens responsible for low durability and weak precision during mechanical tests and shrinkage. In this study, a simple and traditional method of making test bricks is presented. This simple method allows the production of bricks with the required properties. This method is especially efficient for semi-soft consistency pastes. The elaborated handmade pastes present a very different particle-size distribution < 2 mm (clay: 18-66%; silt: 12-53%; sand: 5-65%). The pastes do not stick to the walls of the mould like in the case of steel moulds, and it gives specimens with standard shape, smooth surface, and sharp edges. The resulting fired bricks exhibit high mechanical strength (up to 102 MPa for the compressive strength, and up to 28 MPa for the flexural strength) comparable to and even better than those of conventional methods. The elaborated bricks allowed also the measurement of very important parameters such as drying and firing shrinkage, drying, and firing weight loss, and porosity.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
一种简便易行的砖坯精加工基础技术测量方法
由于其特性,烧结砖作为一种建筑材料显示出巨大的潜力。然而,它们的使用在质量、阻力和耐用性方面需要一些规范。在发展中国家,由于缺乏制作试件的工具,导致这些砖试件存在许多缺陷,导致其在机械试验和收缩过程中耐久性低,精度弱。在本研究中,提出了一种简单而传统的制作试砖的方法。这种简单的方法可以生产出具有所需性能的砖。这种方法对半软的稠度膏体特别有效。精心制作的手工膏体呈现出非常不同的粒径分布< 2 mm(粘土:18-66%;淤泥:12 - 53%;沙:5 - 65%)。这种糊状物不会像钢模具那样粘在模具壁上,使样品具有标准的形状、光滑的表面和锋利的边缘。所得到的烧结砖具有高的机械强度(抗压强度高达102兆帕,抗折强度高达28兆帕),与传统方法相当,甚至更好。精心制作的砖块也允许测量非常重要的参数,如干燥和烧制收缩率,干燥和烧制重量损失,以及孔隙率。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
The Effect of Molar Ratio and Precipitation Time of Mg/Al Hydrotalcite Synthesis on the Isomerization of Glucose into Fructose Biomaterials and Structural Materials Solid Propellant Aging Detection Method Based on Impedance Spectroscopy Exploring the Potential of α-MnO2/ Carbon Nanotubes for Improved Oxygen Reduction Reaction Performance at the Cathode of Alkaline Fuel Cells Effect of Flame Remelting on the Microstructure, Wear and Corrosion Resistance of HVOF Sprayed NiCrBSi Coatings
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1