{"title":"Second-Harmonic Generation in HgGa2S4","authors":"E. Takaoka, K. Kato","doi":"10.1364/cleo_europe.1998.cfh7","DOIUrl":null,"url":null,"abstract":"This paper reports what is believed to be the first attainment of tunable SHG in HgGa2S41,2. The HgGa2S4 crystal used in this experiment was 8 × 8 × 8 mm3 and fabricated at θ = 67.5° (θ = 22.5°) and ϕ = 0° with polished four side surfaces. The transmission range is 0.55 – 12.4 μm.","PeriodicalId":10610,"journal":{"name":"Conference on Lasers and Electro-Optics Europe","volume":"24 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"1998-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Conference on Lasers and Electro-Optics Europe","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1364/cleo_europe.1998.cfh7","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
This paper reports what is believed to be the first attainment of tunable SHG in HgGa2S41,2. The HgGa2S4 crystal used in this experiment was 8 × 8 × 8 mm3 and fabricated at θ = 67.5° (θ = 22.5°) and ϕ = 0° with polished four side surfaces. The transmission range is 0.55 – 12.4 μm.