George H. Keller , Adrian F. Richards , John H. Recknagel
{"title":"Prevention of water loss through CAB plastic sediment core liners","authors":"George H. Keller , Adrian F. Richards , John H. Recknagel","doi":"10.1016/0146-6313(61)90007-7","DOIUrl":null,"url":null,"abstract":"<div><p>Cellulose acetate butyrate (CAB) core liners lose water through pores in the plastic. A wax bath has been developed to coat liners with a microcrystalline wax to retard water loss. Sealing properties of this wax are compared with those of paraffin and a combination of aluminum foil and microcrystalline wax. Over a 50-day period uncoated liners lost water at an average rate of 21·1 × 10<sup>−4</sup> g/day/cm<sup>2</sup> of surface area, while liners coated with microcrystalline wax or with paraffin lost less than 3·3 × 10<sup>−4</sup> g/day/cm<sup>2</sup>. Liners coated with foil and wax did not lose water during the test.</p></div>","PeriodicalId":100361,"journal":{"name":"Deep Sea Research (1953)","volume":"8 2","pages":"Pages 148, IN3, 149-151"},"PeriodicalIF":0.0000,"publicationDate":"1961-09-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.1016/0146-6313(61)90007-7","citationCount":"4","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Deep Sea Research (1953)","FirstCategoryId":"1085","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/0146631361900077","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 4
Abstract
Cellulose acetate butyrate (CAB) core liners lose water through pores in the plastic. A wax bath has been developed to coat liners with a microcrystalline wax to retard water loss. Sealing properties of this wax are compared with those of paraffin and a combination of aluminum foil and microcrystalline wax. Over a 50-day period uncoated liners lost water at an average rate of 21·1 × 10−4 g/day/cm2 of surface area, while liners coated with microcrystalline wax or with paraffin lost less than 3·3 × 10−4 g/day/cm2. Liners coated with foil and wax did not lose water during the test.