POLYMERIC COMPOSITION FOR PURIFICATION OF WASTEWATER FROM VARIOUS IMPURITIES IN TEXTILE INDUSTRY

M. Amonova, K. A. Ravshanov
{"title":"POLYMERIC COMPOSITION FOR PURIFICATION OF WASTEWATER FROM VARIOUS IMPURITIES IN TEXTILE INDUSTRY","authors":"M. Amonova, K. A. Ravshanov","doi":"10.6060/ivkkt.20196210.5963","DOIUrl":null,"url":null,"abstract":"This article deals with the development of new and improvement of traditional methods of wastewater treatment of dyening and finishing industries. The composition was developed on the basis of local natural minerals (bentonite Navahermosa origin, sodium bisulfite, polyacrylamide and aluminium sulphate) for the treatment of wastewater of the textile industry. The influence of bentonite particle size on the degree of wastewater discoloration at different flow rates was studied. With a range of wastewater supply flow rates from 0.5 to 2.0 m/s with a particle size of bentonite adsorbent in the range of 0.25-1.0 nm, the maximum degree of wastewater bleaching is achieved and it is in the range of 84-87%. For microporous adsorbents (CAD-100 and CAD-200) the effectiveness of the discoloration also does not depend on the particle size and ranges from 85 to 87 %.  It was found that, for fine-pored adsorbents (BKA-100 and BKA-200), the efficiency of discoloration also practically does not depend on the particle size and ranges from 85 to 87 %. The highest degree of wastewater treatment according to the proposed composition, apparently due to the fact that in the adsorption process, in addition to the sorption of sewage impurities on the surface of adsorbents, there is a sorption of ions and molecules of dissolved substances on the surfaces of air bubbles and their removal in the foam layer. The wastewater treatment parameters of the dyeing and finishing shop using the bentonite composite adsorbent show that the degree of removal of contaminants by the method developed by us is much higher compared to the sedimentation of aluminum or iron oxyhydrates with adsorbed contaminants. Moreover, the effects of reducing the value of COD and concentration of the surfactant in the wastewater was, on average, 65 % and 82 %, and compared to the effects of reducing the same parameters at defending precipitation of oxyhydrates at 48-54 % and 54-61 %, respectively.","PeriodicalId":14640,"journal":{"name":"IZVESTIYA VYSSHIKH UCHEBNYKH ZAVEDENII KHIMIYA KHIMICHESKAYA TEKHNOLOGIYA","volume":"24 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2019-10-29","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"5","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"IZVESTIYA VYSSHIKH UCHEBNYKH ZAVEDENII KHIMIYA KHIMICHESKAYA TEKHNOLOGIYA","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.6060/ivkkt.20196210.5963","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 5

Abstract

This article deals with the development of new and improvement of traditional methods of wastewater treatment of dyening and finishing industries. The composition was developed on the basis of local natural minerals (bentonite Navahermosa origin, sodium bisulfite, polyacrylamide and aluminium sulphate) for the treatment of wastewater of the textile industry. The influence of bentonite particle size on the degree of wastewater discoloration at different flow rates was studied. With a range of wastewater supply flow rates from 0.5 to 2.0 m/s with a particle size of bentonite adsorbent in the range of 0.25-1.0 nm, the maximum degree of wastewater bleaching is achieved and it is in the range of 84-87%. For microporous adsorbents (CAD-100 and CAD-200) the effectiveness of the discoloration also does not depend on the particle size and ranges from 85 to 87 %.  It was found that, for fine-pored adsorbents (BKA-100 and BKA-200), the efficiency of discoloration also practically does not depend on the particle size and ranges from 85 to 87 %. The highest degree of wastewater treatment according to the proposed composition, apparently due to the fact that in the adsorption process, in addition to the sorption of sewage impurities on the surface of adsorbents, there is a sorption of ions and molecules of dissolved substances on the surfaces of air bubbles and their removal in the foam layer. The wastewater treatment parameters of the dyeing and finishing shop using the bentonite composite adsorbent show that the degree of removal of contaminants by the method developed by us is much higher compared to the sedimentation of aluminum or iron oxyhydrates with adsorbed contaminants. Moreover, the effects of reducing the value of COD and concentration of the surfactant in the wastewater was, on average, 65 % and 82 %, and compared to the effects of reducing the same parameters at defending precipitation of oxyhydrates at 48-54 % and 54-61 %, respectively.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
用于纺织工业废水中各种杂质净化的聚合物组合物
本文介绍了染整工业废水处理新方法的发展和对传统方法的改进。该成分是在当地天然矿物(膨润土Navahermosa原产地,亚硫酸氢钠,聚丙烯酰胺和硫酸铝)的基础上开发的,用于处理纺织工业废水。研究了膨润土粒径对不同流量下废水变色程度的影响。在给水流速为0.5 ~ 2.0 m/s,膨润土吸附剂粒径为0.25 ~ 1.0 nm的条件下,废水漂白程度最大,达到84 ~ 87%。对于微孔吸附剂(CAD-100和CAD-200),脱色效果也不取决于颗粒大小,范围为85%至87%。研究发现,对于细孔吸附剂(BKA-100和BKA-200),脱色效率实际上也不依赖于颗粒大小,其范围在85%至87%之间。根据所提出的成分,废水处理的最高程度,显然是由于在吸附过程中,除了吸附吸附剂表面的污水杂质外,还有吸附气泡表面的溶解物质的离子和分子,并在泡沫层中去除。利用膨润土复合吸附剂处理染整车间废水的实验结果表明,与吸附污染物的铝氧合物或铁氧合物沉淀法相比,该方法对污染物的去除率要高得多。此外,降低废水中COD值和表面活性剂浓度的效果平均为65%和82%,而降低相同参数对氧水合物沉淀的效果分别为48- 54%和54- 61%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
DEPENDENCE OF THE ANTIOXIDANT PROPERTIES OF SOME SPATIALLY SUBSTITUTED PHENOLS ON THE CALCULATED PARAMETERS OF THE STRUCTURE OF ANTIOXIDANT MOLECULES THERMOGRAVIMETRIC AND KINETIC STUDY OF FUEL PELLETS FROM BIOMASS OF HERACLEUM SOSNOWSKYI MANDEN SYNTHESIS AND PROPERTIES OF NANOCELLULOSE-DYE CONJUGATES MODEL OF THE INTERMEDIATE CARBON PHASE BASED ON INTERSTITIAL DEFECTS IN GRAPHITE THEORETICAL AND EXPERIMENTAL STUDY OF THE ADSORPTION CAPACITY OF TRANSITION METAL ACETATES IN THE PROCESS OF DESULFURIZATION OF A MODEL HYDROCARBON FUEL
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1