{"title":"Study of one-step and two-step quench and partition heat treatments on a medium carbon high silicon alloy using dilatometry","authors":"V. Kurup, CW Siyayisa, R. Mostert, J. Moema","doi":"10.36303/satnt.2021cosaami.20","DOIUrl":null,"url":null,"abstract":"This study evaluated the microstructural evolution in a medium carbon high silicon steel during one-step, and two-step quench and partition (Q&P) processes using dilatometry experiments. The two-step Q&P process was carried out using different quench temperatures ranging from 180 to 260 °C. In the one-step process, Q&P heat treatment samples were held isothermally for ten minutes after quenching at specified temperatures ranging between 200 and 4°50 C. The two-step Q&P process yielded a higher fraction of retained austenite than a one-step Q&P process. During the isothermal hold step, the volume expansion due to carbon partitioning and austenite decomposition behavior was interpreted by experimentally determined strain values. For the one-step Q&P process, the austenite decomposition kinetics above and below the Ms temperature differed, as evidenced by the JMAK parameters. The TTT diagram generated for the one-step Q & P process showed a “swing back” at a temperature of around 355 °C.","PeriodicalId":22035,"journal":{"name":"Suid-Afrikaanse Tydskrif vir Natuurwetenskap en Tegnologie","volume":"72 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2022-01-24","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Suid-Afrikaanse Tydskrif vir Natuurwetenskap en Tegnologie","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.36303/satnt.2021cosaami.20","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
This study evaluated the microstructural evolution in a medium carbon high silicon steel during one-step, and two-step quench and partition (Q&P) processes using dilatometry experiments. The two-step Q&P process was carried out using different quench temperatures ranging from 180 to 260 °C. In the one-step process, Q&P heat treatment samples were held isothermally for ten minutes after quenching at specified temperatures ranging between 200 and 4°50 C. The two-step Q&P process yielded a higher fraction of retained austenite than a one-step Q&P process. During the isothermal hold step, the volume expansion due to carbon partitioning and austenite decomposition behavior was interpreted by experimentally determined strain values. For the one-step Q&P process, the austenite decomposition kinetics above and below the Ms temperature differed, as evidenced by the JMAK parameters. The TTT diagram generated for the one-step Q & P process showed a “swing back” at a temperature of around 355 °C.