{"title":"mold metal reactions of magnesium alloy az91E using sf6 and 3m novec 612 as protective gasses in investment casting technology","authors":"M. Dyčka, M. Juliš, L. Klakurková, L. Dyčková, P. Gejdoš","doi":"10.37904/metal.2020.3584","DOIUrl":null,"url":null,"abstract":"In this article, the intensity of mold metal reactions between ceramic shell and magnesium alloy AZ91E is studied. The two possible protective gasses used for melt protection are studied SF6 (sulphur hexafluoride) and 3M NOVEC 612. The scanning electron microscopy (SEM) with X-ray spectroscopy (EDS) were used for the analyses of the mold-metal reaction products on the interface between the magnesium alloy and the ceramic shell. Penetration of AZ91E into the ceramic shell was observed, thickness of mold-metal reaction products layer ranged from 0 μm to 80 μm. The intensity of mold metal reaction is much higher on the outer surface than on the inner surface of the casting. The thicker layer of the fine zircon particles as the first layer of ceramic shell seems to lower the mold metal reactions intensity to minimum. While using SF6, the penetration of AZ91E into ceramic shell was observed, the corroded layer consists of Al-enriched phase with higher content of oxygen. The use of 3M NOVEC 612 as the protective gas led to formation of continuous MgO layer between the ceramic shell and the magnesium alloy, thickness of this layer was up to 60 μm depending on the ceramic shell composition in the close surrounding area.","PeriodicalId":21337,"journal":{"name":"Revue De Metallurgie-cahiers D Informations Techniques","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2020-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Revue De Metallurgie-cahiers D Informations Techniques","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.37904/metal.2020.3584","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

In this article, the intensity of mold metal reactions between ceramic shell and magnesium alloy AZ91E is studied. The two possible protective gasses used for melt protection are studied SF6 (sulphur hexafluoride) and 3M NOVEC 612. The scanning electron microscopy (SEM) with X-ray spectroscopy (EDS) were used for the analyses of the mold-metal reaction products on the interface between the magnesium alloy and the ceramic shell. Penetration of AZ91E into the ceramic shell was observed, thickness of mold-metal reaction products layer ranged from 0 μm to 80 μm. The intensity of mold metal reaction is much higher on the outer surface than on the inner surface of the casting. The thicker layer of the fine zircon particles as the first layer of ceramic shell seems to lower the mold metal reactions intensity to minimum. While using SF6, the penetration of AZ91E into ceramic shell was observed, the corroded layer consists of Al-enriched phase with higher content of oxygen. The use of 3M NOVEC 612 as the protective gas led to formation of continuous MgO layer between the ceramic shell and the magnesium alloy, thickness of this layer was up to 60 μm depending on the ceramic shell composition in the close surrounding area.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
熔模铸造工艺中采用sf6和3m novec 612作为保护气体,研究了az91E镁合金的结晶金属反应
本文研究了陶瓷壳与镁合金AZ91E之间的模具金属反应强度。研究了SF6(六氟化硫)和3M NOVEC 612两种可能用于熔体保护的保护气体。采用扫描电子显微镜(SEM)和x射线能谱仪(EDS)对镁合金与陶瓷壳界面上的模-金属反应产物进行了分析。观察到AZ91E对陶瓷壳的渗透,模-金属反应产物层厚度为0 ~ 80 μm。铸件外表面的金属反应强度远高于内表面。较厚的细锆石颗粒层作为第一层陶瓷壳层似乎将模具金属反应强度降低到最低。当使用SF6时,观察到AZ91E对陶瓷壳的渗透,腐蚀层由富al相组成,氧含量较高。使用3M NOVEC 612作为保护气体,在陶瓷壳和镁合金之间形成了连续的MgO层,该层的厚度可达60 μm,具体厚度取决于陶瓷壳的成分。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
审稿时长
24 months
期刊最新文献
Preparation and performance analysis of gas-quenched steel slag beads Abnormal toughness characteristics and fracture model in simulated welding HAZ of 5%Ni Steel Measurement of the steady state tearing in thin sheets using the contactless system Evaluation of carbothermic processing for mixed discarded lithium-ion batteries Influence of Nb2O5 and basicity on the viscosity and structure of CaO-SiO2-Nb2O5-CeO2-CaF2 slag system
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1