{"title":"Corrosion resistance of iron‐containing experimental titanium alloys exposed to simulated body fluids","authors":"Mogomotsi Leshetla, D. Klenam, J. Merwe, Herman Potgieter, D. Whitefield, M. Bodunrin","doi":"10.1002/maco.202213076","DOIUrl":null,"url":null,"abstract":"In this study, experimental Ti–6Al–1V–3Fe, Ti–4.5Al–1V–3Fe, and Ti–3Fe alloys, as well as commercial Ti–6Al–4V alloy that were scaled up utilizing vacuum induction melting technology, were assessed for corrosion performance in simulated body fluids. The selected simulated body fluids were 0.9 wt% NaCl solution and Hanks balanced salt solution (HBSS). Open circuit potential and linear polarization scans were performed to understand the corrosion performance of the alloys. The surface of the alloys was examined before and after exposure to corrosive solutions using scanning electron microscopy. The results show that all the alloys exhibit good corrosion performance in simulated body fluids. The corrosion rates were less than 0.5 mm/year. Owing to higher corrosion potential and lower corrosion rate, Ti–6Al–1V–3Fe and Ti–4.5Al–1V–3Fe had the best resistance to corrosion in 0.9 wt% NaCl and HBSS, respectively. All the alloys consist of a fully lamellar structure with α and β phases. There was no evidence of severe deterioration on the exposed surface of alloys in the simulated body fluids.","PeriodicalId":18223,"journal":{"name":"Materials and Corrosion","volume":"35 1","pages":"1298 - 1307"},"PeriodicalIF":0.0000,"publicationDate":"2022-02-26","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Materials and Corrosion","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1002/maco.202213076","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2

Abstract

In this study, experimental Ti–6Al–1V–3Fe, Ti–4.5Al–1V–3Fe, and Ti–3Fe alloys, as well as commercial Ti–6Al–4V alloy that were scaled up utilizing vacuum induction melting technology, were assessed for corrosion performance in simulated body fluids. The selected simulated body fluids were 0.9 wt% NaCl solution and Hanks balanced salt solution (HBSS). Open circuit potential and linear polarization scans were performed to understand the corrosion performance of the alloys. The surface of the alloys was examined before and after exposure to corrosive solutions using scanning electron microscopy. The results show that all the alloys exhibit good corrosion performance in simulated body fluids. The corrosion rates were less than 0.5 mm/year. Owing to higher corrosion potential and lower corrosion rate, Ti–6Al–1V–3Fe and Ti–4.5Al–1V–3Fe had the best resistance to corrosion in 0.9 wt% NaCl and HBSS, respectively. All the alloys consist of a fully lamellar structure with α and β phases. There was no evidence of severe deterioration on the exposed surface of alloys in the simulated body fluids.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
含铁实验钛合金暴露于模拟体液中的耐蚀性
在这项研究中,实验Ti-6Al-1V-3Fe、Ti-4.5Al-1V-3Fe和Ti-3Fe合金,以及利用真空感应熔化技术放大的商用Ti-6Al-4V合金,在模拟体液中的腐蚀性能进行了评估。所选模拟体液为0.9 wt% NaCl溶液和Hanks平衡盐溶液(HBSS)。通过开路电位和线性极化扫描来了解合金的腐蚀性能。用扫描电子显微镜对合金暴露于腐蚀溶液前后的表面进行了检测。结果表明,所有合金在模拟体液中均表现出良好的腐蚀性能。腐蚀速率小于0.5 mm/年。Ti-6Al-1V-3Fe和Ti-4.5Al-1V-3Fe分别在0.9 wt% NaCl和HBSS中具有较高的腐蚀电位和较低的腐蚀速率。所有合金均由具有α和β相的全片层结构组成。在模拟体液中,合金暴露的表面没有严重变质的证据。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Research on Pulse Current Cathodic Protection Technology for Long‐Distance Pipeline: A Review On the Impact of Cathodic Polarization on the Chloride Threshold of Carbon Steel in Alkaline Solutions Corrosion Behavior and Evaluation Method of Pipeline Steel Under Dynamic AC Interference: A Study Effect of Corrosion Wastage on the Limit States of Monopile‐Type Offshore Wind Turbines Under Combined Wind and Rotor Blade Rotation Corrosion Behavior of Heat‐Treated Fe‐Based Shape Memory Alloys
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1