{"title":"Utilizing Crushed Clinker Brick Waste as Coarse Aggregate to Produce Concrete With Compressive Strengths Up to 40 Mpa by Adjusting The Gradation Curve","authors":"Y. R. Alkhaly, K. Khairullah, Zulfhazli Zulfhazli, Ainun Mardiah, Deddy Ariska","doi":"10.52088/ijesty.v3i1.437","DOIUrl":null,"url":null,"abstract":"Aggregate gradation is measured by determining the percentage of various particle sizes in an aggregate sample using a standard sieve arrangement. Gradation is usually expressed as a curve showing the percentage of each particle size on a logarithmic scale. This curve can then be used to determine the optimum mix design for a given concrete grade. The purpose of this research is to determine the effect of adjusting the gradation of the coarse aggregate of crushed clinker bricks on the strength of concrete. Clinkers bricks are bricks that have been burned at temperatures that are excessively high. The coarse aggregate grading is adjusted according to aggregate grading limits based on SNI 7656-2012, which are divided into three types of grading limits, namely upper, middle, and lower limits. A total of 60 cylindrical 150mm x 300mm concrete specimens were used for the compressive strength tests. The findings showed that adjusting the lower limit gradation produced optimum compressive strengths of 29.09 MPa, 35.08 MPa, 39.96 MPa, and 38.82 MPa, respectively, for the specified target concrete strengths of 20 MPa, 25 MPa, 30 MPa, and 35 MPa, which were higher than those of the middle and upper limit gradations. The compressive strength and density of the concrete can be significantly improved by modification of the coarse aggregate grading of the clinker bricks","PeriodicalId":14149,"journal":{"name":"International Journal of Engineering, Science and Information Technology","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2023-01-28","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"International Journal of Engineering, Science and Information Technology","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.52088/ijesty.v3i1.437","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Aggregate gradation is measured by determining the percentage of various particle sizes in an aggregate sample using a standard sieve arrangement. Gradation is usually expressed as a curve showing the percentage of each particle size on a logarithmic scale. This curve can then be used to determine the optimum mix design for a given concrete grade. The purpose of this research is to determine the effect of adjusting the gradation of the coarse aggregate of crushed clinker bricks on the strength of concrete. Clinkers bricks are bricks that have been burned at temperatures that are excessively high. The coarse aggregate grading is adjusted according to aggregate grading limits based on SNI 7656-2012, which are divided into three types of grading limits, namely upper, middle, and lower limits. A total of 60 cylindrical 150mm x 300mm concrete specimens were used for the compressive strength tests. The findings showed that adjusting the lower limit gradation produced optimum compressive strengths of 29.09 MPa, 35.08 MPa, 39.96 MPa, and 38.82 MPa, respectively, for the specified target concrete strengths of 20 MPa, 25 MPa, 30 MPa, and 35 MPa, which were higher than those of the middle and upper limit gradations. The compressive strength and density of the concrete can be significantly improved by modification of the coarse aggregate grading of the clinker bricks
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
利用破碎的熟料废砖作为粗骨料,通过调整级配曲线生产抗压强度达40 Mpa的混凝土
骨料级配是通过使用标准筛子排列确定骨料样品中各种粒径的百分比来测量的。级配通常用曲线表示,在对数尺度上表示每种粒度的百分比。该曲线可用于确定给定混凝土等级的最佳配合比设计。本研究的目的是确定调整熟料砖粗集料级配对混凝土强度的影响。熟料砖是在过高温度下燃烧的砖。粗骨料级配根据SNI 7656-2012骨料级配限值进行调整。SNI 7656-2012骨料级配限值分为上、中、下限三种级配限值。共使用60个150mm × 300mm圆柱形混凝土试件进行抗压强度试验。结果表明:当混凝土强度为20 MPa、25 MPa、30 MPa、35 MPa时,调整下限级配可产生的最佳抗压强度分别为29.09 MPa、35.08 MPa、39.96 MPa、38.82 MPa,均高于中、上限级配;通过对熟料砖的粗骨料级配进行改性,可以显著提高混凝土的抗压强度和密度
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Compatibility Analysis of Metolachlor and Pendimethalin for Weed Control in Arabica Coffee Plants Web-Based Math Braille Translator Using Indonesian Braille Symbols Comparison of the Results of the Edas and Vikor Methods in the Decision Support System for KIP Scholarship Recipients at Malikussaleh University Android-Based Drug Information Application Using Augmented Reality Technology Cosmetic Shop Sentiment Analysis on TikTok Shop Using the Support Vector Machine Method
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1