Characteristics of 2-chloropyridine and thiourea condensation. Structure of the as-formed products and their effect on coating properties during electrochemical nickel plating

V. A. Grabelnykh, I. N. Bogdanova, N. Sosnovskaya, N. V. Istomina, N. V. Russavskaya, E. Kondrashov, R. Butrik, N. A. Korchevin, I. B. Rozentsveig
{"title":"Characteristics of 2-chloropyridine and thiourea condensation. Structure of the as-formed products and their effect on coating properties during electrochemical nickel plating","authors":"V. A. Grabelnykh, I. N. Bogdanova, N. Sosnovskaya, N. V. Istomina, N. V. Russavskaya, E. Kondrashov, R. Butrik, N. A. Korchevin, I. B. Rozentsveig","doi":"10.21285/2227-2925-2022-12-4-498-505","DOIUrl":null,"url":null,"abstract":"The synthesis and spectral characterisation of 2-pyridylisothiuronium chloride were performed by regulating the rate of feeding 2-chloropyridine into a thiourea solution in ethyl alcohol for ensuring its low concentration in the reaction zone. According to the data of NMR spectroscopy (1H,13С,15N), the obtained compound represents an approximately equimolar mixture of two tautomers: the expected isothiuronium salt and pyridinium chloride with an isothiocarbamide substituting group in the 2nd position. The ability of isothiuronium salt to transit tautomerically to pyridinium salt is determined by the presence of two main centres, including nitrogen atoms of the isothiourea unit and a nitrogen atom of the pyridine ring. A quantum chemical analysis performed using the DFT method showed that the free energy values of the tautomers were similar, with the tautomer protonated on the nitrogen imido-atom being 2.9 (in the gas phase) and 4.7 kcal/mole (taking into account the dimethyl sulphoxide solvent DMSO at the PCM level) more advantageous as compared to the pyridinium salt. A small difference in the tautomer energies determines their formation in an approximately equimolar quantity. A rapid addition (5–10 mL/min) of 2-chloropyridine to the thiourea solution in the reaction zone creates the surplus of the reagent, acting as a base and causing splitting of the isotiuronium salt. This leads to an additional formation of bis(2-pyridyl)sulphide in the reaction medium, representing a valuable ligand for obtaining coordination compounds. The synthesised mixture of tautomers was examined as an additive to the standard nickel-plating electrolyte. In the concentration of 0.3–0.5 g/L, this additive ensured the production of bright low-porous nickel coatings at a sufficiently high current density of 5–10 A/dm2 and a current yield of 98–99 %.","PeriodicalId":20601,"journal":{"name":"PROCEEDINGS OF UNIVERSITIES APPLIED CHEMISTRY AND BIOTECHNOLOGY","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2023-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"PROCEEDINGS OF UNIVERSITIES APPLIED CHEMISTRY AND BIOTECHNOLOGY","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.21285/2227-2925-2022-12-4-498-505","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

The synthesis and spectral characterisation of 2-pyridylisothiuronium chloride were performed by regulating the rate of feeding 2-chloropyridine into a thiourea solution in ethyl alcohol for ensuring its low concentration in the reaction zone. According to the data of NMR spectroscopy (1H,13С,15N), the obtained compound represents an approximately equimolar mixture of two tautomers: the expected isothiuronium salt and pyridinium chloride with an isothiocarbamide substituting group in the 2nd position. The ability of isothiuronium salt to transit tautomerically to pyridinium salt is determined by the presence of two main centres, including nitrogen atoms of the isothiourea unit and a nitrogen atom of the pyridine ring. A quantum chemical analysis performed using the DFT method showed that the free energy values of the tautomers were similar, with the tautomer protonated on the nitrogen imido-atom being 2.9 (in the gas phase) and 4.7 kcal/mole (taking into account the dimethyl sulphoxide solvent DMSO at the PCM level) more advantageous as compared to the pyridinium salt. A small difference in the tautomer energies determines their formation in an approximately equimolar quantity. A rapid addition (5–10 mL/min) of 2-chloropyridine to the thiourea solution in the reaction zone creates the surplus of the reagent, acting as a base and causing splitting of the isotiuronium salt. This leads to an additional formation of bis(2-pyridyl)sulphide in the reaction medium, representing a valuable ligand for obtaining coordination compounds. The synthesised mixture of tautomers was examined as an additive to the standard nickel-plating electrolyte. In the concentration of 0.3–0.5 g/L, this additive ensured the production of bright low-porous nickel coatings at a sufficiently high current density of 5–10 A/dm2 and a current yield of 98–99 %.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
2-氯吡啶与硫脲缩合反应的特性。电化学镀镍过程中形成产物的结构及其对镀层性能的影响
通过调节2-氯吡啶在巯基脲溶液中的进料速率,保证其在反应区内的低浓度,合成了2-吡啶基异硫脲氯铵并进行了光谱表征。根据核磁共振波谱(1H,13С,15N)的数据,得到的化合物是两个互变异构体的近似等摩尔混合物:预期的异硫脲盐和氯化吡啶,在第2位有异硫脲取代基。异硫脲盐向吡啶盐互变异构过渡的能力是由两个主要中心的存在决定的,包括异硫脲单元的氮原子和吡啶环的氮原子。使用DFT方法进行的量子化学分析表明,互变异构体的自由能值相似,与吡啶盐相比,在氮亚胺原子上质子化的互变异构体为2.9(气相)和4.7千卡/摩尔(考虑到PCM水平的二甲基亚砜溶剂DMSO)更有利。互变异构体能量的微小差异决定了它们以近似等摩尔的量形成。在反应区迅速向硫脲溶液中加入2-氯吡啶(5-10 mL/min)会产生多余的试剂,充当碱并引起异硫脲盐的分裂。这导致在反应介质中额外形成双(2-吡啶基)硫化物,代表获得配位化合物的有价值的配体。合成的互变异构体混合物作为标准镀镍电解质的添加剂进行了测试。在0.3 ~ 0.5 g/L的浓度下,该添加剂可保证在5 ~ 10 a /dm2的电流密度和98 ~ 99%的电流收率下获得光亮的低孔镍镀层。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Biochemical composition of zoned apple varieties growing in different agrocenoses Novel proton-conducting materials based on a polyethylene terephthalate track-etched membrane modified with an N, P-containing ionic liquid Selection of herbaceous cellulose-containing raw materials for biotechnological processing Biochemical composition of ciders from various raw materials Growth characteristics of lactic acid-producing strains using glucose syrup as a carbon source
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1