Surface Treatment of Cardboard with Plant and Bacterial Derived Nanocellulose Suspensions

Еvgeniy А. Toptunov, Yuliya V. Sevastyanova, Ksenia Vashukova
{"title":"Surface Treatment of Cardboard with Plant and Bacterial Derived Nanocellulose Suspensions","authors":"Еvgeniy А. Toptunov, Yuliya V. Sevastyanova, Ksenia Vashukova","doi":"10.37482/0536-1036-2023-3-162-172","DOIUrl":null,"url":null,"abstract":"This study investigates powdered cellulose materials, particularly nanocellulose derived from plant and bacterial sources. The nanocellulose was generated by hydrolyzing bleached sulphate softwood and hardwood pulp samples with strong acids. The original materials are present in the product lines of leading Russian pulp and paper companies. The bacterial cellulose was produced under laboratory conditions from Medusomyces gisevii. The dimensional parameters of the nanocellulose samples were evaluated using electron microscopy, and the degree of polymerization was measured by determining the viscosity of the cellulose solutions in cadoxene. The bleached softwood pulp had a nanocellulose particle length of 80–200 nm, a particle diameter of 80–100 nm, and a degree of polymerization of 60. The bleached hardwood pulp had a particle length of 80–150 nm, a particle diameter of 70–100 nm, and a degree of polymerization of 50. The bacterial nanocellulose had a particle length of 120–250 nm, a particle diameter of 70–120 nm, and a degree of polymerization of 110. Suspensions of various concentrations (from 1 to 10 %) were prepared from nanocellulose samples, which were subsequently used as reinforcing additives in cardboard samples. The additive was applied to the surface in one or two layers. Additives of nanocellulose preparations reduced the breaking length (from 9.6 to 40.4 %) along with an increase in cardboard density (from 6.3 to 23.8 %), tensile rigidity (from 14.0 to 25.0 %) and bursting strength (up to 31.9 %). The best results were obtained by applying a nanocellulose suspension of bleached softwood pulp to the board surface in two layers: a 9.6 % decrease in breaking length was observed with an increase in density of 23.8 %, tensile rigidity of 25.0 %, and bursting resistance of 31.9 % relative to the control sample. Therefore, the study showed the possibility of using nanocellulose suspensions derived from plants and bacterial sources by acid hydrolysis for the surface treatment of cardboard. For citation: Toptunov Е.А., Sevastyanova Yu.V., Vashukova K.S. Surface Treatment of Cardboard with Plant and Bacterial Derived Nanocellulose Suspensions. Lesnoy Zhurnal = Russian Forestry Journal, 2023, no. 3, pp. 162–172. (In Russ.). https://doi.org/10.37482/0536-1036-2023-3-162-172","PeriodicalId":44136,"journal":{"name":"Lesnoy Zhurnal-Forestry Journal","volume":"67 1","pages":""},"PeriodicalIF":0.2000,"publicationDate":"2023-06-10","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Lesnoy Zhurnal-Forestry Journal","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.37482/0536-1036-2023-3-162-172","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"FORESTRY","Score":null,"Total":0}
引用次数: 0

Abstract

This study investigates powdered cellulose materials, particularly nanocellulose derived from plant and bacterial sources. The nanocellulose was generated by hydrolyzing bleached sulphate softwood and hardwood pulp samples with strong acids. The original materials are present in the product lines of leading Russian pulp and paper companies. The bacterial cellulose was produced under laboratory conditions from Medusomyces gisevii. The dimensional parameters of the nanocellulose samples were evaluated using electron microscopy, and the degree of polymerization was measured by determining the viscosity of the cellulose solutions in cadoxene. The bleached softwood pulp had a nanocellulose particle length of 80–200 nm, a particle diameter of 80–100 nm, and a degree of polymerization of 60. The bleached hardwood pulp had a particle length of 80–150 nm, a particle diameter of 70–100 nm, and a degree of polymerization of 50. The bacterial nanocellulose had a particle length of 120–250 nm, a particle diameter of 70–120 nm, and a degree of polymerization of 110. Suspensions of various concentrations (from 1 to 10 %) were prepared from nanocellulose samples, which were subsequently used as reinforcing additives in cardboard samples. The additive was applied to the surface in one or two layers. Additives of nanocellulose preparations reduced the breaking length (from 9.6 to 40.4 %) along with an increase in cardboard density (from 6.3 to 23.8 %), tensile rigidity (from 14.0 to 25.0 %) and bursting strength (up to 31.9 %). The best results were obtained by applying a nanocellulose suspension of bleached softwood pulp to the board surface in two layers: a 9.6 % decrease in breaking length was observed with an increase in density of 23.8 %, tensile rigidity of 25.0 %, and bursting resistance of 31.9 % relative to the control sample. Therefore, the study showed the possibility of using nanocellulose suspensions derived from plants and bacterial sources by acid hydrolysis for the surface treatment of cardboard. For citation: Toptunov Е.А., Sevastyanova Yu.V., Vashukova K.S. Surface Treatment of Cardboard with Plant and Bacterial Derived Nanocellulose Suspensions. Lesnoy Zhurnal = Russian Forestry Journal, 2023, no. 3, pp. 162–172. (In Russ.). https://doi.org/10.37482/0536-1036-2023-3-162-172
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
植物和细菌来源的纳米纤维素悬浮液对纸板表面的处理
本研究研究了粉末状纤维素材料,特别是来源于植物和细菌的纳米纤维素。采用强酸水解漂白过的硫酸盐软木浆和硬木纸浆制备纳米纤维素。原始材料存在于俄罗斯领先的纸浆和造纸公司的产品线中。在实验室条件下,以吉色美杜氏菌为原料制备细菌纤维素。利用电子显微镜对纳米纤维素样品的尺寸参数进行了评价,并通过测定纤维素溶液在卡多辛中的粘度来测定聚合度。漂白后的针叶木浆纳米纤维素颗粒长度为80 ~ 200 nm,粒径为80 ~ 100 nm,聚合度为60。漂白后的硬木纸浆颗粒长度为80 ~ 150 nm,粒径为70 ~ 100 nm,聚合度为50。细菌纳米纤维素的颗粒长度为120 ~ 250 nm,粒径为70 ~ 120 nm,聚合度为110。从纳米纤维素样品中制备不同浓度的悬浮液(从1%到10%),随后将其用作纸板样品中的增强添加剂。添加剂分一层或两层涂在表面。纳米纤维素制剂的添加剂减少了断裂长度(从9.6%到40.4%),同时增加了纸板密度(从6.3%到23.8%),拉伸刚度(从14.0%到25.0%)和破裂强度(高达31.9%)。将漂白后的软木纸浆纳米纤维素悬浮液分两层涂在纸板表面,效果最佳:与对照样品相比,断裂长度减少9.6%,密度增加23.8%,拉伸刚度提高25.0%,抗破裂能力提高31.9%。因此,该研究表明,通过酸水解从植物和细菌来源提取的纳米纤维素悬浮液用于纸板表面处理的可能性。引用:Toptunov Е.А。, Sevastyanova Yu.V。,陈国华。植物和细菌源纳米纤维素悬浮液对纸板表面处理的研究。俄罗斯林业杂志,2023年第1期。3,第162-172页。(俄国人)。https://doi.org/10.37482/0536-1036-2023-3-162-172
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
50.00%
发文量
80
期刊最新文献
Status and prospects for the development of mobile power sources Fundamentally new approaches to solving thermophysical problems in the field of nanoelectronics Comparison between optical and electrophysical data on hole concentration in zinc doped p-GaAs Determination of the polarization plane specific rotation in gyrotropic crystals of the middle category by the spectrophotometric method Changes in the Morphological Characteristics of Secondary Fiber Obtained from Wet-Strength Paper During Gentle Refining of the Recycled Pulp. Part 2. Fines Characteristics
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1